1-20 of 371 Search Results for

ceramic properties

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003059
EISBN: 978-1-62708-200-6
... structure, density, mechanical properties, physical properties, electrical properties, thermal properties, and magnetic properties. ceramics crystallographic data diamond electrical properties engineering data graphite magnetic properties mechanical properties physical properties thermal...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003066
EISBN: 978-1-62708-200-6
... Abstract This article describes the chemical composition, physical properties, thermal properties, mechanical properties, electrical properties, optical properties, magnetic properties, and chemical properties of glasses, glass-matrix composites, and glass-ceramics. chemical properties...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001241
EISBN: 978-1-62708-170-2
... as metals, ceramics, and composites, to grinding. ceramics composites ductility electrical properties finishing grindability grinding hardness magnetic properties metals microstructure stiffness thermal properties toughness FINISHING METHODS used to generate surfaces of work...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005675
EISBN: 978-1-62708-198-6
... in physical properties, and relates properties and hard-tissue response to particular clinical applications. The article provides information on glass or glass-ceramic particles for cancer treatments. bioactive glasses biocompatibility calcium phosphate ceramics cancer treatments ceramics...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003063
EISBN: 978-1-62708-200-6
... summarizes the properties of various ceramic reinforcements and industrial applications of these composites. ceramic reinforcements ceramic-matrix composites composite processing composite testing methods continuous-fiber-reinforced composites discontinuously reinforced composites high...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003052
EISBN: 978-1-62708-200-6
... requirements are being applied to the properties of ceramic products and because the best natural deposits are being gradually depleted. A clay-based ceramic body usually consists of one or more clays or clay minerals mixed with nonclay mineral powders such as fluxes (e.g., feldspar) and fillers (e.g...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001320
EISBN: 978-1-62708-170-2
..., aerospace, and other manufacturing industries. Tables 1 , 2 , and 3 list the representative properties of carbide, cermet, and ceramic tool materials, respectively. In the past two decades, surface modification technologies have significantly expanded tool application ranges, particularly for carbides...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001280
EISBN: 978-1-62708-170-2
.... Overfiring causes excessive oxidation of the substrate, resulting in poor adhesion or a decrease in coating properties. Underfired coatings have poor adhesion and strength and do not develop maximum coating protection. Equipment for spraying ceramic coatings is available commercially. The spray gun should...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001299
EISBN: 978-1-62708-170-2
... Abstract This article discusses the various tests applied to a thermal barrier coating system and to the zirconia layer to establish thermomechanical, environmental stability, and thermal design properties such as coefficient of thermal expansion, specific heat, and thermal transport properties...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005240
EISBN: 978-1-62708-187-0
... Abstract There are several main sources of thermophysical property data that provide the most authoritative and comprehensive compilations of critically and systematically evaluated data that are presently available. This article provides thermophysical property data to assist in the materials...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.9781627081627
EISBN: 978-1-62708-162-7
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001297
EISBN: 978-1-62708-170-2
... Abstract This article focuses on the evaluation of mechanical properties of freestanding films and films adherent to their substrates. Common methods of testing freestanding films, including uniaxial tensile testing, uniaxial creep testing, biaxial testing, and beam-bending methods, are...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003086
EISBN: 978-1-62708-199-3
... Abstract Material properties are the link between the basic structure and composition of the material and the service performance of a part or component. This article describes the most significant properties that must be considered when choosing a metal for a given application, namely physical...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001286
EISBN: 978-1-62708-170-2
... postdeposition changes. It also discusses the effects and causes of growth-related properties of films deposited by physical vapor deposition processes, including residual film stress, density, and adhesion. adhesion atomistic film growth atomistically deposited films composite materials condensation...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005329
EISBN: 978-1-62708-187-0
... Abstract This article discusses the mechanical properties of carbon steels, low-alloy steels, wear-resistant steels, corrosion-resistant steels, heat-resistant steels, and common alloys at both room and elevated temperature. It also provides information on the corrosion-resistant and heat...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003049
EISBN: 978-1-62708-200-6
... Abstract This article provides an overview of the types, properties, and applications of traditional and advanced ceramics and glasses. Principal product areas for traditional ceramics include whitewares, glazes, porcelain enamels, structural clay products, cements, and refractories. Advanced...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003056
EISBN: 978-1-62708-200-6
... physical and mechanical properties of the seal interface is essential. In addition to classification by material type, ceramic joining can also be classified by the bonding mechanism or process. Within each material classification introduced above, there exist subclasses based on the type of joint...
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.a0006671
EISBN: 978-1-62708-213-6
... Abstract The characterization, testing, and nondestructive evaluation of ceramics and glasses are vital to manufacturing control, property improvement, failure prevention, and quality assurance. This article provides a broad overview of characterization methods and their relationship to...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003060
EISBN: 978-1-62708-200-6
..., turbine wheels, ceramic valves, and sliding parts. conceptual design detailed design engine component design proof testing properties of structural ceramics structural ceramics THE DESIGN PROCESS for ceramic materials is generally more complex than that for metals because of the ceramic...
Book Chapter

By Peter J. Blau
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003242
EISBN: 978-1-62708-199-3
... understand and model the fundamental nature of a certain type of wear. Surprising to some, the wear resistance of a given material is not a basic material property, like elastic modulus or yield strength. Rather, a material's wear behavior depends on the conditions of its use. Therefore, the first step in...