Image
Published: 01 December 2008
Fig. 1 A 17-4 PH stainless steel ceramic mold casting, the wall thickness of which was reduced, from the presumed practicable minimum of 0.150 to 0.080 in., without appreciably affecting the soundness of castings produced More
Image
Published: 01 December 2008
Fig. 9 Details and smoothness are evident in this bulk Unicast ceramic mold of a duck head. Courtesy of Unicast Development Company More
Image
Published: 01 December 2008
Fig. 10 Sequence of operations used in the Shaw all-ceramic mold process More
Image
Published: 30 September 2015
Fig. 1 The sequence of operations to produce a part using the ceramic mold process ( Ref 1 , 2 , 3 ) More
Image
Published: 12 September 2022
Fig. 2 Ceramic injection molding. Source: Ref 35 . Creative Commons License (CC BY 3.0), https://creativecommons.org/licenses/by/3.0/ More
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005249
EISBN: 978-1-62708-187-0
... Abstract This article discusses slurry molding that encompasses two distinct processes: plaster molding and ceramic molding. Plaster mold casting is a specialized casting process used to produce nonferrous castings that have greater dimensional accuracy, smoother surfaces, and more finely...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003172
EISBN: 978-1-62708-199-3
... Abstract This article discusses classification of foundry processes based on the molding medium, such as sand molds, ceramic molds, and metallic molds. Sand molds can be briefly classified into two types: bonded sand molds, and unbonded sand molds. Bonded sand molds include green sand molds...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005241
EISBN: 978-1-62708-187-0
... resins; shell molding of sand with a thin resin-bonded shell; no-bond vacuum molding of sand; plaster-mold casting; ceramic-mold casting; rammed graphite molding; and magnetic (no-bond) molding of ferrous shot. The article tabulates a general comparison of casting methods and discusses the basic...
Image
Published: 01 December 2004
) formed by reaction of melt with ceramic mold, also seen in (a). Source: Ref 66 More
Image
Published: 01 January 1990
Fig. 16 Prealloyed HIP Ti-6Al-4V aerospace parts produced by the Crucible ceramic mold method. (a) F-14 fighter plane fuselage brace. (b) F-18 fighter plane engine mount support fitting. (c) Cruise missile engine impeller. (d) Four-section welded nacelle frame structure. (e) Titanium aluminide More
Image
Published: 30 September 2015
Fig. 2 Components produced from prealloyed titanium powder, using HIP and the ceramic mold process. (a) Nacelle frame for F14A, Ti-6Al-6V-2Sn, (b) radial impeller for F107 cruise missile engine, Ti-6Al-4V, (c) complex airframe component for the stealth bomber, Ti-6Al-4V, and (d) engine mount More
Book Chapter

Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005256
EISBN: 978-1-62708-187-0
... of the investment casting process in terms of molding but with an expendable pattern made from high-quality expanded polystyrene (EPS) as in lost foam (instead of the lost wax pattern of investment casting). The EPS pattern is coated in ceramic slurry and then fired to produce the ceramic mold. The firing process...
Image
Published: 01 December 2008
Fig. 6 In-mold ceramic foam filters More
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006297
EISBN: 978-1-62708-179-5
.... Suppliers constantly come up with new products that are claimed to be suitable for specific purposes. For instance, there has been long-standing interest in molding with hollow ceramic spheres ( Fig. 3f ), which have extremely low thermal diffusivity and are used as insulating material. Their thermal...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006140
EISBN: 978-1-62708-175-7
...) processes involved in the PA powder metallurgy technique. It discusses the technical problems addressed in shape control and their solutions for understanding the advantages of powder metallurgy HIP. ceramic mold process fabrication hot isostatic pressing metal can near-net shaping prealloyed...