1-20 of 1929 Search Results for

castings design

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006332
EISBN: 978-1-62708-179-5
... composition and initial melt condition. Besides the basic alloy properties, the effective castability of high-alloy irons can be significantly improved through casting and casting system design. The article describes the product design and processing factors of high-alloy graphitic irons and high-alloy white...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0009015
EISBN: 978-1-62708-187-0
... Abstract This article provides a general introduction on casting processes and design techniques. It discusses the process steps and methods of the main categories of shape casting methods, namely, expendable molds with permanent patterns, expendable molds with expendable patterns, and metal...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0009020
EISBN: 978-1-62708-187-0
... Abstract Casting offers a great amount of component design flexibility. This article discusses six casting design parameters that drive the geometry of casting design from a process standpoint. It provides information on the design of junctions and addresses considerations of secondary...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0009014
EISBN: 978-1-62708-187-0
... Abstract This article discusses issues that impact a good casting design. The focus is on the casting design in general, and on sand and permanent mold aluminum casting in particular. The article examines the casting design process from a variety of design and processing perspectives...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003176
EISBN: 978-1-62708-199-3
... Abstract This article provides general guidelines for casting design to provide progressive solidification, minimize heat concentration, eliminate cores, and prevent distortion. Casting design also affects tolerances. Casting tolerances depend on the alloy being poured, the size of the casting...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002484
EISBN: 978-1-62708-194-8
... Abstract Casting offers the cost advantages over other manufacturing methods for most components. This article reviews the aspects of castings with which designers should be familiar, as well as the methods used by foundries to produce high-integrity castings. It discusses the design concepts...
Image
Published: 01 December 2008
Fig. 10 Design parameters to aid stress reduction in magnesium alloy castings More
Image
Published: 01 January 1989
Fig. 5 Tap design for zinc die castings More
Image
Published: 01 December 2008
Fig. 17 The effects of design on distortion of castings. (a) Top view of casting; numbers indicate moduli of the two sections. (b) Distortion caused by solidification stresses More
Image
Published: 01 December 2008
Fig. 35 Use of brackets in steel casting design (top). Lightening of a casting that is too massive by means of ribs and recessing (bottom) More
Image
Published: 01 December 2008
Fig. 25 Good casting design, permitting ideal location of gates, made for efficient production of this aluminum permanent mold casting. Although this casting had a wall thickness of 0.093 in., the recommended minimum for the material and process ( Table 1 ), all surfaces were produced More
Image
Published: 01 December 2008
Fig. 5 Casting design that would require different shrinkage allowances than those normally used. Dimension X can contract freely, while dimension Y is restrained by the core used to make the hole. More
Image
Published: 01 December 2008
Fig. 2 Traditional casting design process More
Image
Published: 01 December 2008
Fig. 4 Structure of guidelines for light metal casting design More
Image
Published: 01 December 2008
Fig. 19 Casting design and solidification of a simple wedge. (a) Riser placed at narrow end of wedge; shrinkage occurs at wide end. The crosshatched region represents the approximate area of the casting where solidification is first complete, thus cutting off the feeding path of the casting More
Image
Published: 30 November 2018
Fig. 33 Good casting design permitting ideal location of gates enabled efficient production of this aluminum permanent-mold casting. Although casting wall thickness is only 2.36 mm (0.093 in.), all surfaces were produced to a finish of at least 125 micro-in. More
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005219
EISBN: 978-1-62708-187-0
.... The article lists information required for the maintenance tooling record and preventive maintenance (PM) items from the North American Die Casting Association's publication E501. It concludes with information on objectives for proper storage of tools and patterns. The objectives are preventing tool...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006326
EISBN: 978-1-62708-179-5
... Abstract This article discusses some of the factors that are linked directly to the casting design of ductile iron castings. It reviews the choice of molding process, application of draft, and patternmaker's allowance that should be taken into consideration in designing castings. The article...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002407
EISBN: 978-1-62708-193-1
... Abstract This article reviews the fatigue and fracture properties of aluminum alloy castings, specifically alloys A356 and A357/D357 (all-T6) and alloy A201-T7, from the perspective of both design and manufacturing considerations. In addition, it provides an overview of the roles played...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005327
EISBN: 978-1-62708-187-0
... Abstract This article presents a discussion on the melting, pouring, and shakeout practices; composition control; molds, patterns, and casting design; heat treatment; and applications of different classes of nickel-chromium white irons and high-chromium white irons. iron castings heat...