Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006496
EISBN: 978-1-62708-207-5
... Abstract Castability is a complex characteristic that depends on both the intrinsic fluid properties of the molten metal and the manner in which the particular alloy solidifies. This article discusses the practical aspects of solidification important to aluminum foundrymen. The primary focus...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006326
EISBN: 978-1-62708-179-5
... describes the solidification shrinkage associated with the volume change that occurs during solidification, as well as strength and stiffness of ductile iron castings. It concludes with a discussion on the thermal deformation and residual stress in ductile iron castings. castability castings design...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006328
EISBN: 978-1-62708-179-5
... Abstract The morphology of the graphite particles in compacted graphite iron (CGI) is intermediate to the graphite particles found in gray iron or ductile iron. This article discusses the castability and product design of compacted graphite iron. The introduction of modern measurement...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006332
EISBN: 978-1-62708-179-5
... Abstract Castability of alloys is a measure of their ability to be cast to a given shape with a given process without the formation of cracks/tears, pores/shrinkage, and/or other significant casting defects. This article discusses the factors which affect the fluidity of an iron melt: alloy...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005223
EISBN: 978-1-62708-187-0
... Abstract Castability of alloys is a measure of their ability to be cast to a given shape with a given process without the formation of casting defects. This article describes the factors that limit fluidity as well as experimental methods for measuring fluidity of various alloys. Various tests...
Image
Published: 01 January 1993
Fig. 2 Pumphrey-Moore cracking index based on castability data obtained from aluminum-copper-magnesium alloys. Source: Ref 25 More
Image
Published: 30 November 2018
Fig. 19 Pumphrey-Moore cracking index based on castability data obtained from Al-Cu-Mg alloys. Source: Ref 19 More
Image
Published: 09 June 2014
Fig. 20 General dry-out/heat-up schedule for conventional castable linings in induction heating applications. Courtesy of Allied Mineral Products More
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006578
EISBN: 978-1-62708-210-5
... Abstract The 391-type hypereutectic aluminum-silicon alloys are hypereutectic alloys designed for applications where excellent wear resistance is needed. They are similar to the 390 family of alloys, except for a low copper content to improve castability and corrosion resistance. This datasheet...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006524
EISBN: 978-1-62708-207-5
... Abstract Aluminum casting alloys are among the most versatile of all common foundry alloys and generally have high castability ratings. This article provides an overview of the common methods of aluminum shape casting. It discusses the designations of aluminum casting alloys categorized...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006329
EISBN: 978-1-62708-179-5
... casting, with particular emphasis on the melting practices, molten metal treatment, and feeding of molten metal into sand molds. It discusses the castability factors, such as fluidity, shrinkage, and resistance, of gray iron. Typical cupola charge compositions and the final analyses for class 30 and class...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003134
EISBN: 978-1-62708-199-3
... describes the major factors considered in alloy selection for casting, including raw material cost, castability, machinability, and the bearing and wear properties. It also provides information on the cost of the final product. alloy selection bearing properties castability conductivity copper...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005840
EISBN: 978-1-62708-167-2
... the cracking that is associated with thermal cycling. Most fused silica castables have a nominal use temperature of approximately 1200 °C (2200 °F). At temperatures above 1200 °C (2200 °F), the fused silica converts to quartzite and will not withstand thermal cycling without cracking. This results in a maximum...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006571
EISBN: 978-1-62708-210-5
...-magnesium die-casting alloys mechanical properties; physical properties Alloys 360.0 and A360.0 are hypoeutectic Al-Si-Mg die-casting alloys with restricted copper content ( Table 1 ). They have very good castability and good corrosion resistance, but fair machinability, less generous limitations...
Book Chapter

Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005323
EISBN: 978-1-62708-187-0
... Abstract This article begins with an overview of classes and applications of gray iron. It discusses the castability of gray iron in terms of section sensitivity and fluidity. The article provides information on the dimensions of prevailing sections recommended for gray irons and reviews...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005325
EISBN: 978-1-62708-187-0
... Abstract This article reviews the graphite morphology, chemical composition requirements, castability, mechanical properties, and corrosion resistance of compacted graphite (CG) irons. It describes the factors affecting the mechanical properties of CG irons. The article also presents...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005335
EISBN: 978-1-62708-187-0
... and continuous casting process. It provides information on castability and quality of the casted alloys. The article details the postcasting treatment, including heat treatment, hot isostatic pressing, and coatings. It summarizes the applications of cast cobalt alloys. cast cobalt alloys castability...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006563
EISBN: 978-1-62708-210-5
... 9.0 34 5.0 17 10 4 52 7.5 34 5.0 25 Source data are in English units; metric values are converted and rounded Alloy 332.0 has many characteristics like 336.0, while offering improved castability and machinability ( Ref 1 ). This alloy retains strength at elevated temperatures...
Image
Published: 01 December 2004
Fig. 20 Six low-carbon steel sheet specimens, separated by steel spacers, showing (a) damage from mounting in a thermosetting phenolic resin and (b) lack of damage when mounted in a castable epoxy More
Image
Published: 01 December 2004
Fig. 19 A low-carbon steel sheet plated with electroless nickel showing (a) damage to the coating from mounting in a thermosetting phenolic resin and (b) the lack of damage when mounted in a castable epoxy. As-polished. 100× More