Skip Nav Destination
Close Modal
Search Results for
carburizing modeling
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 275
Search Results for carburizing modeling
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Series: ASM Handbook
Volume: 4F
Publisher: ASM International
Published: 01 February 2024
DOI: 10.31399/asm.hb.v4F.a0007017
EISBN: 978-1-62708-450-5
... and potential methods for determining a solution. Then, quantitative analyses of practical industrial problems are demonstrated. Finally, the potential shift in these approaches with the advent of Industry 4.0 is outlined. carburizing Industry 4.0 modeling quenching QUENCHING and industrial heat...
Abstract
Mathematical models have been used for over five decades in industrial heat-treating operations. Most of these modeling efforts have emanated from academia or research institutes, with the primary approach of mathematically capturing heat-treating processes and validating quality predictions. In this article, a contrarian but more realistic scenario is considered, where two industrial problem descriptions become the starting point. The technical complexity of the industry problem has been elaborated for a deeper understanding of the issue along with elaboration of the approach and potential methods for determining a solution. Then, quantitative analyses of practical industrial problems are demonstrated. Finally, the potential shift in these approaches with the advent of Industry 4.0 is outlined.
Image
Published: 30 September 2015
Fig. 2 Tungsten carburization model. Carburization occurs via a reaction between blended tungsten and carbon powders in a diffusion-controlled process via a shrinking-core mechanism.
More
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005799
EISBN: 978-1-62708-165-8
... information on carburizing modeling, case depth prediction, case depth measurement, and case depth evaluation as well as on carburizing equipment, and also covers the factors affecting distortion after carburizing. austenite carbon content carburizing modeling case depth continuous furnaces...
Abstract
This article describes the thermodynamics and kinetics of gas carburizing reactions, and details the mass transfer mechanism during gas carburizing. It discusses the various considerations involved in carburizing process planning, and reviews successful operation of the gas carburizing process based on the control of three principal variables: temperature, atmosphere composition or carbon potential, and time. The article also describes the selection criteria for alloy, carbon sources, atmosphere types, and carbon monoxide level for endothermic carburizing atmospheres. It provides information on carburizing modeling, case depth prediction, case depth measurement, and case depth evaluation as well as on carburizing equipment, and also covers the factors affecting distortion after carburizing.
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005987
EISBN: 978-1-62708-168-9
..., induction hardening, through hardening, and nitriding. In view of the emerging use of mathematical modeling and optimization, a brief overview of its application for process and design optimization is also provided. carburizing gears heat treatment induction hardening low-pressure carburizing...
Abstract
This article provides an overview of steel gear heat treating processes and brings out the nuances of the various important heat treating considerations for steel gear applications. The heat treatment processes covered are annealing, carburizing, hardening, low-pressure carburizing, induction hardening, through hardening, and nitriding. In view of the emerging use of mathematical modeling and optimization, a brief overview of its application for process and design optimization is also provided.
Image
in Industrial Applications of Analytics and Modeling for Carburizing and Quenching Processes
> Quenchants and Quenching Technology
Published: 01 February 2024
Image
Published: 01 January 1997
Book: Powder Metallurgy
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006052
EISBN: 978-1-62708-175-7
... and chemical composition are influenced by several factors including temperature, carbon content, dopant levels, reaction time ( Ref 4 , 5 ), starting tungsten grain/particle size, impurity type and amounts, powder bed thickness, and carburizing environment. Fig. 2 Tungsten carburization model...
Abstract
This article discusses the methods and procedures used to extract, purify, and synthesize tungsten carbide powder, metal, and other refractory carbide/nitride powders used in hard metal production. Selection of powders, additives, equipment, and processes for making ready-to-press hard metal powders is also discussed. The article also provides information on the emerging technologies for tungsten carbide synthesis and binders in hard metal production, such as cobalt, iron, and nickel.
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005956
EISBN: 978-1-62708-166-5
... for hardening. This article provides a model-based description of the development of residual stresses during case hardening. It also describes the influence and effects of residual stresses and distortion in hardening, carburizing, and nitriding processes of the steel. axial stress carbon content...
Abstract
The process of case hardening of steel includes three consecutive steps of heat treatment: heating; the thermochemical process with the enrichment of the surface area during the carburizing or carbonitriding stage with carbon and nitrogen; and the subsequent quenching process for hardening. This article provides a model-based description of the development of residual stresses during case hardening. It also describes the influence and effects of residual stresses and distortion in hardening, carburizing, and nitriding processes of the steel.
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005982
EISBN: 978-1-62708-168-9
... possible, the effect of microstructure on properties, primarily hardness and fatigue resistance, are incorporated into the discussion of a particular microstructural feature. Much of the published work on carburizing is devoted to processing ( Ref 3 , 4 ), aided by computer modelling and control...
Abstract
This article describes the microstructure, properties, and performance of carburized steels, and elucidates the microstructural gradients associated with carbon and hardness gradients. It provides information on case depth measurement, the factors affecting case depth, and the formation and causes of microcracks. The article discusses the effects of alloying elements on hardenability, the effects of excessive retained austenite and massive carbides on fatigue resistance, the effects of residual stresses and internal oxidation on fatigue performance of carburized steels. In addition, the causes of intergranular fracture at austenite grain boundaries and their prevention methods are explored. The article also describes the major mechanisms of bending fatigue crack initiation in carburized steels.
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005959
EISBN: 978-1-62708-168-9
... , 61 , 62 ). Most investigations relate to plasma-based nitriding/carburizing. Models based on the growth kinetics of the expanded austenite zone should take into consideration that the diffusivity of interstitials in expanded austenite is (strongly) concentration dependent and driven not only...
Abstract
Low-temperature surface hardening is mostly applied to austenitic stainless steels when a combination of excellent corrosion performance and wear performance is required. This article provides a brief history of low-temperature surface hardening of stainless steel, followed by a discussion on physical metallurgy, including crystallographic identity, thermal stability and decomposition, nitrogen and carbon solubility in expanded austenite, and diffusion kinetics of interstitials. It provides a description of low-temperature nitriding and nitrocarburizing processes for primarily austenitic and, to a lesser extent, other types of stainless steels along with practical examples and industrial applications of these steels.
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002489
EISBN: 978-1-62708-194-8
... based on the boundary conditions and material description. A typical process model, such as one for heat treatment, has several major aspects to it. A process model for a carburizing process is shown in Fig. 7 . The flow chart shown in Fig. 7 represents the different pieces of a simulation tool...
Abstract
This article presents an overview of the techniques used in the design for heat treatment and discusses the primary criteria for design: minimization of distortion and undesirable residual stresses. It provides theoretical and empirical guidelines to understand the sources of common heat treat defects. A simple example is presented to demonstrate how thermal and phase-transformation-induced strains cause dimensional changes and residual stresses. The article concludes with a discussion on the heat treatment process modeling technology.
Book: Fatigue and Fracture
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002400
EISBN: 978-1-62708-193-1
... of the steel, the carbon gradient, and the case depth. The residual stresses as a function of case depth are routinely measured by x-ray diffraction ( Ref 71 ), and considerable effort has been applied to modeling residual stress profiles in carburized steels as a function of cooling and hardenability ( Ref 72...
Abstract
Bending fatigue of carburized steel components is a result of cyclic mechanical loading. This article reviews the alloying and processing factors that influence the microstructures and bending fatigue performance of carburized steels. These include austenitic grain size, surface oxidation, retained austenite, subzero cooling, residual stresses, and shot peening. The article describes the analysis of bending fatigue behavior of the steels based on S-N curves that represents a stress-based approach to fatigue. It discusses the types of specimen used to evaluate bending fatigue in carburized steels. The stages of fatigue and fracture of the steels, namely crack initiation, stable crack propagation, and unstable crack propagation, are reviewed. The article analyzes the intergranular fracture at the prior-austenite grain boundaries of high-carbon case microstructures that dominates bending fatigue crack initiation and unstable crack propagation of direct-quenched carburized steels.
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005950
EISBN: 978-1-62708-166-5
... was the implementation of transformation-induced plasticity (TRIP), which is an additional inelastic strain caused by the interaction of stresses with ongoing phase transformations, in the thermomechanical model. Moreover, Inoue et al. ( Ref 28 ) made the first attempt to simulate the carburized quenching process...
Abstract
This article describes the fundamental concepts of heat treatment simulation, including the physical events and their interactions, the heat treatment simulation software, and the commonly used simulation strategies. It summarizes material data needed for heat treatment simulations and discusses reliable data sources as well as experimental and computational methods for material data acquisition. The article provides information on the process data needed for accurate heat treatment simulation and the methods for their determination. Methods for validating heat treatment simulations are also discussed with an emphasis on the underlying philosophy for the selection and design of validation tests. The article also discusses the applications, capabilities, and limitations of heat treatment simulations via selected industrial case studies for a better understanding of the effect of microstructure, distortion, residual stress, and cracking in gears, shafts, and bearing rings.
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005967
EISBN: 978-1-62708-166-5
... observed during and after heat treating of quenched and tempered steels. It describes phase transformations of steels during heating, cooling of steel with and without metallurgical transformation, and the formation of high-temperature transformation products on the surface of a carburized part...
Abstract
Of the various thermal processing methods for steel, heat treating has the greatest overall impact on control of residual stress and on dimensional control. This article provides an overview of the effects of material- and process-related parameters on the various types of failures observed during and after heat treating of quenched and tempered steels. It describes phase transformations of steels during heating, cooling of steel with and without metallurgical transformation, and the formation of high-temperature transformation products on the surface of a carburized part. The article illustrates the use of carbon restoration on decarburized spring steels. Different geometric models for carbide formation are shown schematically. The article also describes the different microstructural features such as grain size, microcracks, microsegregation, and banding.
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005812
EISBN: 978-1-62708-165-8
... 2012 , p 253 – 256 10.1016/j.jallcom.2012.07.069 9. Jiménez H. , Staia M.H. , and Puchi E.S. , Mathematical Modeling of a Carburizing Process of a SAE 8620H Steel , Surf. Coat. Tech. , Vol 120–121 , Nov 1999 , p 358 – 365 10.1016/S0257-8972(99)00464-8 10. Hao...
Abstract
Supercarburizing, also referred to as high-concentration carburizing, carbide-precipitation carburizing, and carbide dispersion, is a carburizing method that results in a large amount of dispersed particulate carbide, with carbon content as high as 2 to 3%, to obtain surfaces with high hardness and good wear resistance. This article briefly reviews the process of supercarburizing using conventional carburizing steel as well as steels developed for supercarburizing, including 20CrMnMo steel, 20Cr2Ni4 steel, 35Cr3SiMnMoV steel, and 20CrMnTi steel. In addition, it discusses supercarburized steel composition, carburizing characteristics, mechanical properties testing, and microstructure analysis of 35Cr3SiMnMoV steel.
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005771
EISBN: 978-1-62708-165-8
... the proportional relation of Eq 1 explicit ( Case depth = K Time ) for gas carburization only ( Ref 2 , 3 ). However, even in gas carburization, the kinetics of carbon diffusion gives an incomplete picture of carburizing. A comprehensive model of gas carburization must include algorithms...
Abstract
Surface hardening improves the wear resistance of steel parts. This article focuses exclusively on the methods that involve surface and subsurface modification without any intentional buildup or increase in part dimensions. These include diffusion methods, such as carburizing, nitriding, carbonitriding, and austenitic and ferritic nitrocarburizing, as well as selective-hardening methods, such as laser transformation hardening, electron beam hardening, ion implantation, selective carburizing, and surface hardening with arc lamps. The article also discusses the factors affecting the choice of these surface-hardening methods.
Series: ASM Handbook
Volume: 22B
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.hb.v22b.a0005536
EISBN: 978-1-62708-197-9
... time-step, and so on. The model has been successfully used to simulate processes such as carburization of nickel-chromium alloys ( Ref 9 ), carbon diffusion in welds between dissimilar steels ( Ref 9 ), and gradient sintering of cemented carbide cutting tools ( Ref 10 ). Several examples where...
Abstract
This article focuses on the modeling and simulation of diffusion-controlled processes related to both materials processing such as heat treatments, and materials degradation from a practical perspective by using the one-dimensional (1-D) sharp interface approach. It describes various diffusion simulation models, such as one-phase simulations, moving phase-boundary simulations, and dispersed system simulations. The article presents case studies that illustrate some examples where diffusion simulations have been applied to industrial-based problems, with an emphasis on the approaches used and the lessons learned from performing such simulations.
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005966
EISBN: 978-1-62708-166-5
... Abstract This article focuses on the mechanisms, models, prevention, correction, and effects associated with decarburization inherited from semi-finished product processing prior to induction heating. It discusses the diffusion of carbon in austenitic iron, which has a face-centered cubic...
Abstract
This article focuses on the mechanisms, models, prevention, correction, and effects associated with decarburization inherited from semi-finished product processing prior to induction heating. It discusses the diffusion of carbon in austenitic iron, which has a face-centered cubic crystal structure that provides an interstitial path for the migration of the relatively small carbon atoms. The article describes the evolution of steel microstructure with progressive decarburization (in air) to a steady-state carbon gradient using an iron-iron carbide phase diagram. It provides useful information on the impact of alloying on vulnerability to decarburization, and the impact of decarburization on the mechanical properties of steels and cast irons. The article also describes the technological operations that potentially cause decarburization and the practical implications for induction hardening.
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005940
EISBN: 978-1-62708-166-5
... the distortion mechanisms by using the concept of distortion potential and its carriers (see the article “Basics of Distortion and Stress Generation during Heat Treatment” in this Volume). Modeling and simulation not only are helpful, but in many cases are necessary tools to fully understand the mechanisms...
Abstract
This article presents the three levels of investigations of distortion engineering. On Level 1, the parameters and variables influencing distortion in every manufacturing step must be identified. More than 200 parameters can affect distortion. The design of experiments approach allows for the investigation of larger numbers of parameters by a limited number of samples, and can be structured into system analysis, test strategy, test procedure, and test evaluation. Level 2 focuses on understanding the distortion mechanisms by using the concept of distortion potential and its carriers. Distortion engineering aims to compensate distortion using the so-called compensation potential (Level 3). Level 3 discusses the measures to improve homogeneity, and respectively the symmetry, of the carriers of the distortion potential. The article also discusses the compensation of the resulting size and shape changes of the existing asymmetries by well-directed insertions of additional inhomogeneity/asymmetries in one or more of the distributions of the carriers.
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005439
EISBN: 978-1-62708-196-2
... Abstract This article presents various equations that are essential for the modeling of both single-phase and multiphase profiles. It includes the fundamental laws of diffusion, along with its equations and solutions. The article provides information on the series of applications...
Abstract
This article presents various equations that are essential for the modeling of both single-phase and multiphase profiles. It includes the fundamental laws of diffusion, along with its equations and solutions. The article provides information on the series of applications that illustrate how various diffusional processes can be modeled.