Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006152
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of binary alloy phase diagrams for which calcium (Ca) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary...
Image
Published: 09 June 2014
Fig. 2 Calcium-clogged water paths due to high-conductivity water More
Image
Published: 30 September 2015
Fig. 16 Calcium Chloride Moisture Vapor Emission Test More
Image
Published: 30 September 2015
Fig. 10 Calcium chloride test on concrete floor. Courtesy of KTA-Tator, Inc. More
Image
Published: 01 January 2003
Fig. 3 Corrosion rate versus calcium concentration in three different waters. A, HCO 3 − = 38 mg/L, Cl − = 78 mg/L, SO 4 2 − = 78 mg/L; B, HCO 3 − = 100 mg/L, Cl − = 224 mg/L, SO 4 2 − = 224 mg/L; C, HCO 3 − = 266 mg/L, Cl − = 644 mg/L More
Image
Published: 01 December 2004
Fig. 7 Pb-0.083Ca. A higher calcium content than in Fig. 6 results in smaller grains. Fine Pb 3 Ca precipitate (dark) is recognizable in (b). 15 g citric acid + 9 g ammonium molybdate in 80 mL H 2 O. (a) Original magnification 92×. (b) Original magnification 1825× More
Image
Published: 01 December 2004
Fig. 14 Low-carbon steel showing inclusions of calcium sulfide outer rim (light gray) and calcium aluminate core (dark gray). The matrix is pearlite and ferrite. As-polished. 500×. Courtesy of B.L. Bramfitt and J.R. Kilpatrick More
Image
Published: 01 June 2012
Fig. 1 Scanning electron micrograph of a calcium phosphate coating on the surface of a poly (carbonate urethane) substrate, formed by immersion in a concentrated simulated body-fluid-like solution. Courtesy of D.H. Barnes More
Image
Published: 01 June 2012
Fig. 20 Friction coefficients of a calcium phosphate coating (deposited on a steel substrate) when sliding against an ultrahigh-molecular-weight polyethylene pin at various sliding speeds and in both dry and lubricated conditions More
Image
Published: 01 June 2012
Fig. 21 Wear track of a calcium phosphate coating after 28 min of sliding at a speed of 40 mm/s (1.6 in./s) in dry conditions More
Image
Published: 01 June 2012
Fig. 8 Solubility diagram of some calcium phosphates. DCPA, dicalcium phosphate anhydrous; DCPD, dicalcium phosphate dehydrate; OCP, octacalcium phosphate; α- and β-TCP, tricalciumphosphate; HA, hydroxyapatite; and TTCP, tetracalcium phosphate. Source: Ref 40 More
Image
Published: 01 January 2002
Fig. 15 Comparison of axial fatigue data for untreated and calcium-treated rolled ASTM A516 steel. 51 mm (2 in.) thick plates tested with alternating stress ratio of 0.1. Source: Ref 9