1-20 of 439 Search Results for

bronze plating

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001255
EISBN: 978-1-62708-170-2
...) Current density, A/dm 2 (A/ft 2 ) 1-4 (9-37) 3-16 (28-149) 1-8 (9-74) Composition and operating conditions for a typical bronze plating solution Table 3 Composition and operating conditions for a typical bronze plating solution Composition of plated deposit, 88Cu-12Sn Constituent...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003215
EISBN: 978-1-62708-199-3
... conditions of electrodeposition processes for chromium plating, nickel plating, iron plating, cadmium plating, zinc plating, indium plating, lead plating, tin plating, silver plating, gold plating, brass plating, bronze plating, tin-lead plating, zinc-iron plating, and zinc-nickel plating. The article also...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003215
EISBN: 978-1-62708-199-3
..., and operating conditions of electrodeposition processes for chromium plating, nickel plating, iron plating, cadmium plating, zinc plating, indium plating, lead plating, tin plating, silver plating, gold plating, brass plating, bronze plating, tin-lead plating, zinc-iron plating, and zinc-nickel plating...
Book Chapter

Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005114
EISBN: 978-1-62708-186-3
... at the interface of the two surfaces. Specially processed bronze-plated bushings exemplify this approach and exhibit an extremely low rate of wear. As stated previously, seizure is an extreme form of abrasive wear. It is typified by considerable surface material removal and/or relocation and drastic increases...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004139
EISBN: 978-1-62708-184-9
... Fiber Reinforcements Sandwich Core Construction Steel Hull Aluminum Hulls Ferrocement Hulls Copper Sheathing Stainless Steels Aluminum Galvanized Steel Bronze Brass Zinc Alloy Winches Backing Plates Lifeline Supports Anchor Systems Inboard Engines...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005140
EISBN: 978-1-62708-186-3
...-0.6Mn-0.3Si-1Cr-0.2Mo … 4140 modified Fe-0.4C-1.2Cr-0.2Mo-1Al … Nonferrous alloys Zinc alloy (UNS Z35543) Zn-4Al-3Cu-0.06Mg See text Aluminum bronze (UNS C62500), 270 to 300 HB Cu-13Al-4Fe See text Plastics Polyester-glass and/or powder filled Glass filled: 50% polyester...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006412
EISBN: 978-1-62708-192-4
... C C C F 38 5.5 Connecting-rod and main bearings, camshaft bearings  High-lead bronze D D D C E 45 6.5 Camshaft bearings, turbine bearings, pump bushings, thrust washers  Medium-lead bronze E E E B D 55 8 Piston pin bushings, rocker-arm bushings, wear plates, steering...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003167
EISBN: 978-1-62708-199-3
... from alloys containing from 5.5 to 7% Sn, plus smaller amounts of copper, nickel, silicon, and magnesium. Starting forms for bearing fabrication include cast tubes as well as rolled plate and strip, which can be press formed into half-round shapes. As is the case with solid bronze bearings, relatively...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001066
EISBN: 978-1-62708-162-7
... bronze plate, sheet, strip, and rolled bar B 121 Leaded brass plate, sheet strip, and rolled bar B 122 Copper-nickel-tin alloy, copper-nickel-zinc alloy (nickel silver), and copper-nickel alloy plate, sheet, strip, and rolled bar B 152 and B 152M (metric) Copper sheet, strip, plate...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001065
EISBN: 978-1-62708-162-7
..., primers, plaques, jewelry base for gold plate C22000 (commercial bronze, 90%) Fabrication characteristics same as C21000, plus heading and upsetting, roll threading and knurling, hot forging and pressing. Uses: etching bronze, grillwork, screen cloth, weather stripping, lipstick cases, compacts...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005148
EISBN: 978-1-62708-186-3
...-quality steels W1; O1 O1; A2 A2; D2 300-series stainless steels W1 chromium plated; aluminum bronze Nitrided A2; aluminum bronze Nitrided D2 or D3; cemented carbide Cups 305 mm (12 in.) or more across, drawn from 1.6 mm (0.062 in.) sheet (parts 4 and 5 ) Drawing-quality aluminum and copper...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002185
EISBN: 978-1-62708-188-7
... mm ( 1 4 –6 in.) plate Copper (20–60 HRB) 460–910 (1500–3000) Brasses (60–100 HRB) 150 (500) Bronzes (60–100 HRB) 120 (400) Feed, mm/tooth (in./tooth), for 6.4–150 mm ( 1 4 –6 in.) plate Copper (20–60 HRB) 0.17 (0.0065) Brasses (60–100 HRB) 0.15 (0.006...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001309
EISBN: 978-1-62708-170-2
... wide 850 Black-on-bronze bookends, highlights relieved (b) Black background with colored copper highlights Pumice in water Cloth, sewn sections 180 diam by 13 wide 7 diam by 1 2 wide 850 Silver-plated lipstick cap (c) Satin Greaseless rouge, proprietary Loose cloth wheel...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006429
EISBN: 978-1-62708-192-4
... compressors Bearing and sealing parts Materials Frame Cast iron Bearing Back plate Carbon steel Middle member Bronze Sliding surface White-metal Cylinder Cast iron Spherical graphite cast iron Cast steel Forged steel Valve seat and retainer Cast iron Carbon steel Stainless...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003204
EISBN: 978-1-62708-199-3
... T8 (d) T4 … … … … T451 (e) … … … … 2025 Die forgings 515 960 T4 170 340 10 T6 2219 (f) Flat sheet 535 995 T31 (d) 175 350 18 T81 (d) T37 (d) 165 325 24 T87 (d) T42 190 375 36 T62 Plate 535 995 T31 (d) 175 350 18 T81 (d) T37 (d...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001070
EISBN: 978-1-62708-162-7
... products, including self-lubricating sintered bearings, structural parts, oxide-dispersion-strengthened copper, sintered metal friction materials, and porous filters. copper powder-metallurgy copper-base structural parts oxide-dispersion-strengthened copper porous bronze filters powder production...
Book Chapter

Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0006541
EISBN: 978-1-62708-183-2
... coating M Brass, low copper; bronze, low copper Metallic coating N Brass, high copper; bronze, high copper Metallic coating O Copper, high nickel Metallic coating P Nickel, cobalt Metallic coating Q Titanium Anodized R Silver Plating S Palladium, rhodium, gold, platinum...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003135
EISBN: 978-1-62708-199-3
...Abstract Abstract This article discusses the characteristics, properties, and production methods of copper powders and copper alloy powders. Bulk of the discussion is devoted to production and applications of powder metallurgy (P/M) parts, including pure copper P/M parts, bronze P/M parts...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005143
EISBN: 978-1-62708-186-3
... (0.010 in.) thick, 0.019 mm (0.00075 in.) grain, 491 MPa (71.2 ksi) UTS C19400 HSM copper Annealed, 0.69 mm (0.027 in.) thick, 319 MPa (46.3 ksi) UTS, 29% tensile elongation (d) C22000 Commercial bronze Annealed, 0.69 mm (0.027 in.) thick, 0.017 mm (0.00067 in.) grain, 234 MPa (34 ksi) UTS (d...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005259
EISBN: 978-1-62708-187-0
... produced in this type of mold. Metal Molds Metal Mold Design Mold Wall Thickness End Plate Thicknesses End Plate Recess End Plate Mold Lock Design End Plate Wedge and Pin Design Mold Adapter Tables Pretreatment for Metal Molds Mold Wash for Permanent Molds Water Cooling...