1-20 of 367 Search Results for

brittleness

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000630
EISBN: 978-1-62708-181-8
...-brittle fatigue crack propagation, brittle and ductile fracture, crack-growth mechanisms, tearing, fibrillation, and fatigue striations of these surfaces. crack growth fatigue crack propagation fatigue striations fractograph polycarbonate polyethylene polyimide polymers Fig. 1317...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004007
EISBN: 978-1-62708-185-6
... hydrostatic extrusion of structural alloys, composites, brittle materials, and intermetallics or intermetallic compounds, with examples. It concludes with a discussion on the attempts made to extend the hydrostatic extrusion to higher temperatures. brittle materials composites hot hydrostatic...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003225
EISBN: 978-1-62708-199-3
... macroscopic scale as ductile fractures, brittle fractures, fatigue fractures, and fractures resulting from the combined effects of stress and environment. corrosion failures corrosion-fatigue failures distortion failures elevated-temperature failures fatigue failures fracture hydrogen-damage...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005342
EISBN: 978-1-62708-187-0
... Abstract This article discusses the visual and microscopic characteristics of fractures of cast alloys. The fractures include ductile rupture, transgranular brittle fracture, intergranular fracture, fatigue, and environmentally induced fracture. The article describes the factors that affect the...
Book Chapter

By Sam Nasser
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005684
EISBN: 978-1-62708-198-6
... Abstract Physically, tantalum is a dark, blue-gray, lusterless metal that exists in two crystalline forms: an alpha-phase with a body-centered cubic structure, and a brittle beta-phase with a tetragonal orientation. This article tabulates the physical and material properties of tantalum. It...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003060
EISBN: 978-1-62708-200-6
... Abstract The design process for ceramic materials is more complex than that of metals because of low-strain tolerance, low fracture toughness and brittleness. The application of structural ceramics to engineering systems hinges on the functional benefits to be derived and is manifested in the...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000612
EISBN: 978-1-62708-181-8
... fracture, low-cycle and high-cycle fatigue fracture, fracture surface, brittle intergranular fracture, hydrogen embrittlement, and intergranular stress-corrosion cracking of stainless steel components of these steels. The components include high-pressure compressor parts, springs, deflector yokes of...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000620
EISBN: 978-1-62708-181-8
... Abstract This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of cast aluminum alloys and in identifying and interpreting the morphology of fracture surfaces. The fractographs illustrate the brittle fracture, microvoid coalescence, fatigue...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000605
EISBN: 978-1-62708-181-8
... fracture, brittle fracture, tensile-test fracture, transgranular fracture, cleavage fracture, delayed fracture, corrosion fatigue, inclusion morphology, fatigue crack propagation, and in-service fatigue fracture of various automotive components. These components include tie rod adjusting sleeves...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000613
EISBN: 978-1-62708-181-8
...-overload fractures, impact fractures, microstructure, quench cracking, brittle-in-service failure, hydrogen embrittlement, stress-corrosion cracking, and grain-boundary cracking of tool steel components. These components include diesel engine injector plungers, rivet-heading tools, circular saw blades, and...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000626
EISBN: 978-1-62708-181-8
... brittle fracture, transgranular fracture, intergranular fracture, and crack propagation of the tungsten carbide. brittle fracture cemented carbides four-point bending test fractograph intergranular fracture tungsten carbide Fig. 1273 Eta phase on the fracture surface of a 94WC-6Co alloy...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000603
EISBN: 978-1-62708-181-8
... Abstract This article is an atlas of fractographs that covers pearlitic and ferritic ductile irons. The fractographs display the following: brittle cleavage fracture; fatigue crack propagation; fatigue and monotonic fracture surfaces; fracture modes in slow monotonic loading and impact loading...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000606
EISBN: 978-1-62708-181-8
... fracture, brittle fracture, and in-service rotary bending fatigue fracture of fractured roof-truss angles, pressure-vessel shells, automotive axle shafts, broken keyed spindles, crane gears, blooming-mill spindles, automotive bolts, and crane wheels of these steels. axle shafts brittle fracture...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0001835
EISBN: 978-1-62708-181-8
... general features of ductile and brittle fracture modes. fractography fracture modes scanning electron microscopy specimen preparation THE SCANNING ELECTRON MICROSCOPE has unique capabilities for analyzing surfaces. A beam of electrons moves in an x - y pattern across a conductive specimen...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000609
EISBN: 978-1-62708-181-8
... Abstract This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of ASTM/ASME alloy steels and in identifying and interpreting the morphology of fracture surfaces. The fractographs illustrate the solidification cracking, creep failure, brittle...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000608
EISBN: 978-1-62708-181-8
... Abstract This article is an atlas of fractographs that helps in understanding the causes and mechanisms of fracture of AISI/SAE alloy steels (4xxx steels) and in identifying and interpreting the morphology of fracture surfaces. The fractographs illustrate the brittle fracture, ductile fracture...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0001834
EISBN: 978-1-62708-181-8
... illustrations. The article also describes microscopic and macroscopic features of the different fracture mechanisms with illustrations with emphasis on visual and light microscopy examination. The types of fractures considered include ductile fractures, tensile-test fractures, brittle fractures, fatigue...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000610
EISBN: 978-1-62708-181-8
... candy fracture, cleavage fracture, brittle fracture, high-cycle fatigue fracture, fatigue striations, hydrogen-embrittlement failure, creep crack propagation, fatigue crack nucleation, intergranular creep fracture, torsional overload fracture, stress-corrosion cracking, and grain-boundary damage of...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000625
EISBN: 978-1-62708-181-8
... the ductile fracture, interlaminar failure, transgranular cleavage and fracture, tension-overload fracture, longitudinal and transverse cracking, fiber splitting, stress rupture, and low-cycle fatigue of these composites. ductile to brittle transition fractograph metal-matrix composites...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005657
EISBN: 978-1-62708-198-6
... to which the device was subjected. Fatigue is the accumulation of repeated loading-induced damage that results in the initiation and propagation of cracks. Cyclic loading at levels below the yield strength of a metal can and does result in fatigue failures. Fatigue failures appear brittle...