Image
Published: 01 January 1993
Fig. 21 Use of composite brazing filler metal (two layers of silver-base filler metal and a copper shim) to join tungsten carbide to steel More
Image
Published: 01 January 1993
Fig. 1 Assembly that was torch brazed with a silver brazing filler metal for use in a high vacuum atmosphere system More
Image
Published: 01 January 1993
Fig. 13 Cryogenic valve that was vacuum brazed with BNi-2 brazing filler metal. All joints on the body, flanges, seat, and bonnets were brazed simultaneously. Courtesy of Wall Colmonoy Corporation More
Image
Published: 01 January 1993
Fig. 2 DFB joint illustrating how the brazing filler metal and nickel plate diffused into the base metal, almost obliterating the joint. Specimen: nickel-plated Nimonic 80A 6.4 mm (0.252 in.) tensile test bar machined from rectangular brazed blocks. Brazing procedure: 30 min at 1175 ┬░C (2150 More
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001458
EISBN: 978-1-62708-173-3
... Abstract Fabrication of high-density heat exchangers, which have a large heat transfer area and a compact size, is best accomplished by brazing where the brazing filler metal is clad to the materials to be brazed. This article focuses on the brazing procedures involved in the fabrication...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006692
EISBN: 978-1-62708-210-5
... Abstract Wrought 4xxx alloys (extrusions and forgings) exhibit high surface hardness, wear resistance, and a low coefficient of thermal expansion. This article provides a summary of brazing filler metals used to join brazeable aluminum-base metals. It contains tables that list the nominal...
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005856
EISBN: 978-1-62708-167-2
... of the right induction heating equipment to carry out the brazing or soldering operation are also provided. The article describes the types of brazing filler metals and joint designs. It also presents the types of inspection methods, namely, mechanical and visual, used to determine the quality of the brazed...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001392
EISBN: 978-1-62708-173-3
... Abstract This article focuses on clad brazing material, which is defined as any base material or alloy that is clad with an appropriate lower-melting-point brazing filler metal. It provides information on typical clad brazing strip products in a tabular form and lists the advantages of using...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001452
EISBN: 978-1-62708-173-3
... Abstract The quality of brazed stainless steel joints depends on the selection of the brazing process, process temperature, filler metal, and the type of protective atmosphere or flux. This article provides a detailed discussion on the applicability and brazeability of stainless steel and lays...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001453
EISBN: 978-1-62708-173-3
... Abstract This article focuses primarily on the various steps involved in the brazing of heat-resistant alloys (nickel- and cobalt-base alloys). The major steps include the selection of brazing filler metals, surface cleaning and preparation, brazing processes and their corresponding atmospheres...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001345
EISBN: 978-1-62708-173-3
... Abstract This article describes the physical principles of brazing with illustrations and details elements of the brazing process. The elements of brazing process include filler-metal flow, base-metal characteristics, filler-metal characteristics, surface preparation, joint design and clearance...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001450
EISBN: 978-1-62708-173-3
... Abstract This article focuses on the various criteria considered in the selection of product forms, joint types, solders, and filler metals for brazing and soldering of base material components. brazing brazing filler metals joints material selection soldering solders...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006828
EISBN: 978-1-62708-329-4
... of the material, joint design, prebraze cleaning, brazing procedures, postbraze cleaning, and quality control. Factors that must be considered include brazeability of the base metals; joint design and fit-up; filler-metal selection; prebraze cleaning; brazing temperature, time, atmosphere, or flux; conditions...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003210
EISBN: 978-1-62708-199-3
... Abstract This article provides information about the selection of brazing processes and filler metals and describes the brazing (heating) methods, including manual torch brazing, furnace brazing, induction brazing, dip brazing, resistance brazing and specialized brazing processes...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001391
EISBN: 978-1-62708-173-3
... Abstract Exothermic brazing is a process that utilizes the heat produced in a solid-state chemical reaction to melt a conventional filler metal or to produce molten filler metal as a product of the reaction. This article provides the pros and cons of exothermic brazing, describes procedure...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001454
EISBN: 978-1-62708-173-3
... Abstract Copper, copper alloys, and precious metals are probably the most easily brazed metals because of their resistance to oxidation at high temperatures. This article provides a brief discussion on the metallurgy of copper, copper alloys, and precious metals and discusses the filler metals...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006302
EISBN: 978-1-62708-179-5
... Abstract Brazing and soldering are done at temperatures below the solidus temperature of the base material but high enough to melt the filler metal and allow the liquid filler metal to wet the surface and spread into the joint gap by capillary action. This article discusses the common...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006529
EISBN: 978-1-62708-207-5
... Abstract Brazing technology is continually advancing for a variety of metals including aluminum and its alloys and nonmetals. This article discusses the key physical phenomena in aluminum brazing and the materials for aluminum brazing, including base metals, filler metals, brazing sheet...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001390
EISBN: 978-1-62708-173-3
... Abstract Diffusion brazing (DFB) is a process that coalesces, or joins, metals by heating them to a suitable brazing temperature at which either a preplaced filler metal will melt and flow by capillary attraction or a liquid phase will form in situ between one faying surface and another...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0009239
EISBN: 978-1-62708-173-3
... to avoid thermal deformation ( Ref 3 ). Selection of Brazing Filler Metals Selection of filler metal depends on cost and technical requirements to brazed joints: metallurgical compatibility to base materials, method of brazing, projected strength, work temperature, corrosion resistance, and design...