Skip Nav Destination
Close Modal
Search Results for
bonded joints
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 168 Search Results for
bonded joints
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Book Chapter
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006457
EISBN: 978-1-62708-190-0
... Abstract Adhesive-bonded joints are extensively used in aircraft components and assemblies where structural integrity is critical. This article addresses the problem of how to inspect bonded assemblies so that all discrepancies are identified. It describes several inspection techniques and...
Abstract
Adhesive-bonded joints are extensively used in aircraft components and assemblies where structural integrity is critical. This article addresses the problem of how to inspect bonded assemblies so that all discrepancies are identified. It describes several inspection techniques and presents drawbacks and limitations of these techniques. Generic flaw types and flaw-producing mechanisms are listed in a table. The article discusses metal-to-metal defects, adherend defects, honeycomb sandwich defects, repair defects, and in-service defects. It reviews the methods applicable to the inspection of bonded structures, including visual inspection, ultrasonic inspection, X-ray radiography, and neutron radiography. The evaluation and correlation of inspection results are also discussed. The article concludes with information on the effects of ultrasonic wave interference in the ultrasonic inspection of adhesive-bonded joints.
Book: Corrosion: Materials
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003831
EISBN: 978-1-62708-183-2
... exceeding those of base materials. Brazing is a high-temperature joining process, usually above 450 °C (840 °F). In addition to the mechanical bonding between the base material and the braze alloy, there is also a metallurgical bonding that occurs, resulting in very high joint strengths. Due to the chemical...
Abstract
Corrosion is often thought of as rusting, the process of deterioration undergone by a metal when it is exposed to air or water. This article provides the fundamentals of joints corrosion and primarily addresses the various forms of corrosion observed in brazed and soldered joints and their causes. It describes the role of proper brazing procedures in controlling corrosion. The article concludes with information on the corrosion resistance of various brazing alloy systems.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003047
EISBN: 978-1-62708-200-6
... in adhesive bonding, including storage and handling of adhesives, bonding preparation, adhesive application, tooling, and curing. adhesive joints adhesive modifiers applications electron beam cured adhesives hot melt adhesives pressure sensitive adhesives primers structural adhesives...
Abstract
This article begins with an overview of the fundamentals of adhesive technology, including functions, limitations, adhesive joint types, and the key factors in the selection of adhesives, including application, type of joint, process limitation, mechanical requirement, and service conditions. It then focuses on the characteristics, types, and properties of the five groups of adhesives, such as structural, hot melt, pressure sensitive, water based, ultraviolet, and electron beam cured adhesives. The article also discusses the functions and applications of adhesive modifiers, including fillers, adhesion promoters, tackifiers, and tougheners. It gives a short note on functions of primers and primerless bonding. Applications of adhesives in automotive, aerospace, electronics, electrical, medical, sports, and construction sectors are also described. Finally, the article describes the steps in adhesive bonding, including storage and handling of adhesives, bonding preparation, adhesive application, tooling, and curing.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003043
EISBN: 978-1-62708-200-6
... Abstract The structural efficiency of a composite structure is established by its joints and assembly. Adhesive bonding, mechanical fastening, and fusion bonding are three types of joining methods for polymer-matrix composites. This article provides information on surface treatment and the...
Abstract
The structural efficiency of a composite structure is established by its joints and assembly. Adhesive bonding, mechanical fastening, and fusion bonding are three types of joining methods for polymer-matrix composites. This article provides information on surface treatment and the applications of adhesive bonding. It discusses the types of adhesives, namely, epoxy adhesives, epoxy-phenolic adhesives, condensation-reaction PI adhesives, addition-reaction PI adhesives, bismaleimide adhesives, and structural adhesives. The article provides information on fastener selection considerations, including corrosion compatibility, fastener materials and strength, head configurations, importance of clamp-up, interference fit fasteners, lightning strike protection, blind fastening, and sensitivity to hole quality. Types of fusion bonding are presented, namely, thermal welding, friction welding, electromagnetic welding, and polymer-coated material welding.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003046
EISBN: 978-1-62708-200-6
... repair have been validated in this article through the required environmental and load condition tests. These include bonded-scarf joint flush repair, double-scarf joint flush repair, blind-side banded-scarf repair, blind-side sandwich repair, and bonded external patch repair. A brief note on...
Abstract
Relatively limited effort has gone into developing repair processes and materials for composites, in contrast to the significant labor and expense that has gone into the development of these materials for numerous critical applications. As composites gain wider acceptance as aerospace materials, there is a need to understand the requirements of the end users regarding repair of these advanced materials. This article focuses on the repair of graphite-epoxy structures designed in a variety of forms for a wide range of load intensities. Five repair concepts developed for generic laminate repair have been validated in this article through the required environmental and load condition tests. These include bonded-scarf joint flush repair, double-scarf joint flush repair, blind-side banded-scarf repair, blind-side sandwich repair, and bonded external patch repair. A brief note on thermoplastic repair concepts is also provided in this article.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003205
EISBN: 978-1-62708-199-3
... for welding, brazing, and soldering. It also describes joint design considerations such as selection of weld joints and welds. adhesive bonding brazing fusion welding joining mechanical fastening soldering solid-state welding weld joint design weld preparation welding JOINING...
Abstract
This article discusses different types of joining processes, including welding, brazing, soldering, mechanical fastening, and adhesive bonding. It examines two broad classes of welding: fusion welding and solid-state welding. The article discusses the process selection considerations for welding, brazing, and soldering. It also describes joint design considerations such as selection of weld joints and welds.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003021
EISBN: 978-1-62708-200-6
..., joining of polyvinyl chloride (PVC) pipe. It is also widely familiar because of its use by hobbyists for building plastic (usually polystyrene) models using solvents such as acetone or toluene. A joint strength of 85 to 100% of that of the parent material can be obtained with solvent bonding ( Ref 9...
Abstract
This article discusses the classification of the attachment and joining methods in plastics, including mechanical fastening, adhesive bonding, solvent bonding, and welding. It describes the mechanical fastening techniques used to join both similar and dissimilar materials with machine screws or bolts, nuts and washers, molded-in threads, self-threading screws, rivets, spring-steel fasteners, press fits, and snap fits. The article explains solvent bonding used for thermoplastic parts, and tabulates the solvent types used with various plastics. It also describes the surface preparation of plastics, chemical treatment for adhesion, and tabulates the adhesive types for bonding plastics to plastics and plastics to nonplastics. The article briefly describes the welding processes of thermoplastics, including fusion welding (hot-tool, hot gas, extrusion, and focused infrared), friction welding (vibration, spin, and ultrasonic), and electromagnetic welding (resistance, induction, dielectric, and microwave). It concludes with the evaluation of welds using destructive and nondestructive testing.
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003172
EISBN: 978-1-62708-199-3
... Abstract This article discusses classification of foundry processes based on the molding medium, such as sand molds, ceramic molds, and metallic molds. Sand molds can be briefly classified into two types: bonded sand molds, and unbonded sand molds. Bonded sand molds include green sand molds...
Abstract
This article discusses classification of foundry processes based on the molding medium, such as sand molds, ceramic molds, and metallic molds. Sand molds can be briefly classified into two types: bonded sand molds, and unbonded sand molds. Bonded sand molds include green sand molds, dry sand molds, resin-bonded sand molds, and sodium silicate bonded sand. The article describes the casting processes that use these molds, including the no-bake process, cold box process, hot box process, the CO2 process, lost foam casting process and vacuum molding process. The casting processes that use ceramic molds include investment casting, and plaster casting. Metallic molds are used in permanent mold casting, die casting, semisolid casting, and centrifugal casting.
Book Chapter
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005251
EISBN: 978-1-62708-187-0
... line. Production: 60 complete molds per hour. Flask size: 1300 × 1100 × 400 mm (50 × 40 × 15 in.). Amount of sand: 120 Mg (130 tons/h). Number of operators: 5 Fig. 2 Cope-and-drag assembly of vacuum-bonded sand mold. The sand in the elevated cope mold is under vacuum and is held in place by...
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003056
EISBN: 978-1-62708-200-6
... physical and mechanical properties of the seal interface is essential. In addition to classification by material type, ceramic joining can also be classified by the bonding mechanism or process. Within each material classification introduced above, there exist subclasses based on the type of joint...
Abstract
Many applications of ceramics and glasses require them to be joined to each other or to other materials such as metals. This article focuses on ceramic joining technologies, including glass-metal sealing, glass-ceramic/metal joining, ceramic-metal joining, ceramic-ceramic joining, and the more advanced joining of nonoxide ceramics. It also discusses metallizing, brazing, diffusion bonding, and chemical bonding.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003048
EISBN: 978-1-62708-200-6
... dopes or cements are used for bonding and sealing plastic plumbing joints. Polypropylenes used as hot melts, particularly mechanically foamed versions, have established a strong position in appliance seal and gasket applications and are used as automotive and roofing weather seals. Several other...
Abstract
This article is an informative primer on sealants and the role they play in engineered assemblies. It discusses the physical, thermal, chemical, and electrical properties of sealant materials and the various forms in which they are applied, including liquids, pastes, and extruded tapes. It also describes classifications and types, comparing and contrasting sealants made from oil-based caulks, asphalts, coal tar resins, latex acrylic sealants, polyvinyl acetate caulks, solvent acrylics, butyl sealants, polysulfides, polyurethanes, modified silicones, anaerobics, vinyl plastisols, and polypropylenes. In addition, the article provides practical design insight, addressing application requirements, seal configurations, and joint stresses. It concludes with a brief discussion on the use of sealants in aerospace, automotive, electrical, and construction applications.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003210
EISBN: 978-1-62708-199-3
... metallurgical bond, using a nonferrous filler metal as the bonding material and a furnace as the heat source. ( Fig. 1 ). Furnace brazing is only practical if the filler metal can be placed on the joint before brazing and retained in position during brazing. Fig. 1 Cross-sectional view of three-part...
Abstract
This article provides information about the selection of brazing processes and filler metals and describes the brazing (heating) methods, including manual torch brazing, furnace brazing, induction brazing, dip brazing, resistance brazing and specialized brazing processes such as diffusion and exothermic brazing. The article explains joint design, filler materials, fuel gases, equipment, and fluxes in the brazing methods. The article also describes the brazing of steels, stainless steels, cast irons, heat-resistant alloys, aluminum alloys, copper and copper alloys, and titanium and titanium alloys.
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005656
EISBN: 978-1-62708-198-6
... Abstract Porous coatings are used in the field of joint replacement, particularly in cementless total hip/knee arthroplasty. This article reviews the offerings and biomaterial properties in orthopedic surgery for the contemporary class of highly porous metals. It describes the traditional...
Abstract
Porous coatings are used in the field of joint replacement, particularly in cementless total hip/knee arthroplasty. This article reviews the offerings and biomaterial properties in orthopedic surgery for the contemporary class of highly porous metals. It describes the traditional porous metal/coating having an open-cell structure, high porosity, and a microsctructure resembling that of cancellous bone. The traditional porous metal/coating includes fiber-metal mesh, cobalt-chromium (CoCr) beads, cancellous-structured titanium, and plasma spray. The article discusses other porous metal/coating due to the limitations of traditional porous metals for numerous open-cell-structured metals, such as titanium-base foams and trabecular metal.
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003060
EISBN: 978-1-62708-200-6
... metallized material. Other systems incorporate a reactive metal in the braze. This reactive metal reacts with the surface layer of the ceramic to wet it, and the remaining braze constituents bond to this reacted layer. When brazed joints are used, high residual stresses may be induced in the components...
Abstract
The design process for ceramic materials is more complex than that of metals because of low-strain tolerance, low fracture toughness and brittleness. The application of structural ceramics to engineering systems hinges on the functional benefits to be derived and is manifested in the conceptual design for acceptable reliability. This article discusses the design considerations for the use of structural ceramics for engineering applications. It describes the conceptual design and deals with fast fracture reliability, lifetime reliability, joints, attachments, interfaces, and thermal shock in detailed design procedure. The article provides information on the proof testing of ceramics, and presents a short note on public domain software that helps determine the reliability of a loaded ceramic component. The article concludes with several design scenarios for gas turbine components, turbine wheels, ceramic valves, and sliding parts.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003130
EISBN: 978-1-62708-199-3
... note on aluminum clad products and corrosion at joints. aluminum aluminum alloys aluminum clad products corrosion resistance protective coatings types of corrosion ALUMINUM and most aluminum alloys have good corrosion resistance in natural atmospheres, fresh waters, seawater, many soils...
Abstract
This article discusses the corrosion resistance of aluminum and aluminum alloys in various environments, such as in natural atmospheres, fresh waters, seawater, and soils, and when exposed to chemicals and their solutions and foods. It describes the forms of corrosion of aluminum and aluminum alloys, including pitting corrosion, intergranular corrosion, exfoliation corrosion, galvanic corrosion, stray-current corrosion, deposition corrosion, crevice corrosion, filiform corrosion, stress-corrosion cracking, corrosion fatigue, and hydrogen embrittlement. The article also presents a short note on aluminum clad products and corrosion at joints.
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005674
EISBN: 978-1-62708-198-6
... Abstract Titanium and its alloys have been used extensively in a wide variety of implant applications, such as artificial heart pumps, pacemaker cases, heart valve parts, and load-bearing bone or hip joint replacements or bone splints. This article discusses the properties of titanium and its...
Abstract
Titanium and its alloys have been used extensively in a wide variety of implant applications, such as artificial heart pumps, pacemaker cases, heart valve parts, and load-bearing bone or hip joint replacements or bone splints. This article discusses the properties of titanium and its alloys and presents titanium-base biomaterials in a table. Titanium components are produced in wrought, cast, and powder metallurgy (PM) form. The article describes forging, casting, and heat treating of titanium alloys for producing titanium components. Typical mechanical properties of titanium biomedical implant alloys are listed in a tabular form. The article presents an overview of surface-modification methods for titanium and its alloys implants. It concludes with a section on biocompatibility and in vivo corrosion of titanium alloys.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003209
EISBN: 978-1-62708-199-3
..., allowing formation of strong metallurgical bonds. If any melting does occur during upset welding, the molten metal is typically extruded out of the weld joint area. DEFORMATION WELDING solid-state processes differ from diffusion welding (bonding) processes in two important ways. First...
Abstract
This article describes the mechanism, advantages and disadvantages, fundamentals, capabilities, variations, equipment used, and weldability of metals in solid-state welding processes, including diffusion bonding, explosion welding, friction welding, ultrasonic welding, upset welding, and deformation welding.
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006037
EISBN: 978-1-62708-172-6
... bonding, cracking, chemical attack, and moisture that affect the polymeric floor coatings on concrete. abrasion resistance chemical resistance coating failures physical properties polymer chemistries thermal properties POLYMERIC FLOOR COATINGS (also called polymeric flooring systems...
Abstract
Polymeric floor coatings refer to flooring materials composed of multicomponent thermoset resins formulated with various fillers and pigments that are installed in situ, usually over concrete substrates. Polymeric flooring systems, specified for all industrial and commercial environments, use a variety of polymer chemistries and are constructed in a variety of methods and designs. This article provides a description of the service conditions for the polymeric flooring systems. It provides information on polymeric flooring systems, including thin-film coatings, self-leveling systems, membrane systems, broadcast systems, troweled systems, and terrazzo. The article also focuses on properties, applications, testing, and factors and requirements to be considered during the installation of polymeric floor coatings. It concludes with a discussion about coating failures, including bonding, cracking, chemical attack, and moisture that affect the polymeric floor coatings on concrete.
Book Chapter
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003064
EISBN: 978-1-62708-200-6
..., Si 3 N 4 , and SiB 4 ) produced no bonding or very weak bonds. Thus, it was determined that only the latter two systems (boron and TiSi 2 ) were suitable for producing joints of sufficient shear strength (γ > 3.4 MPa, or 0.5 ksi). Due to the difficulty of melting the boron interlayers, only solid...
Abstract
Carbon-carbon composites (CCCs) are introduced in fields that require their high specific strength and stiffness, in combination with their thermoshock resistance, chemical resistance, and fracture toughness, especially at high temperatures. The use of CCCs has expanded as the price of carbon fibers has dropped and their mechanical properties have increased. This article begins with an overview of the carbon conversion processes, fiber properties and microstructures, and interfacial bonding and environmental interaction of carbon fibers, followed by a detailed discussion on the various techniques available for processing CCCs for specific applications, including preform fabrication (fiber weaving), densification, application of protective coatings, and joining. The article closes with a description of the mechanical and physical properties and applications of CCCs. The main applications of CCCs, in terms of money and mass, are in the military, space, and aircraft industries.
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006007
EISBN: 978-1-62708-172-6
... Abstract Functional fusion-bonded epoxy (FBE) coatings are used as external pipe coatings, base layer for three-layer pipe-coating systems, internal pipe linings, and corrosion coatings for concrete reinforcing steel (rebar). This article provides information on the chemistries of FBE, and...
Abstract
Functional fusion-bonded epoxy (FBE) coatings are used as external pipe coatings, base layer for three-layer pipe-coating systems, internal pipe linings, and corrosion coatings for concrete reinforcing steel (rebar). This article provides information on the chemistries of FBE, and discusses the application procedures for internal and external FBE pipe coating. The procedures involve pipe inspection, surface preparation, heating, powder application, curing, cooling, coating inspection, and repairing. It describes the problems and solutions for FBE external pipe coatings, girth weld FBE application, FBE custom coatings, internal FBE pipe linings, and FBE rebar coatings.