1-20 of 635 Search Results for

biomedical applications

Sort by
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004207
EISBN: 978-1-62708-184-9
.... Biomedical devices are usually subjected to static or dynamic forces, such as in orthopedic and cardiovascular applications. For example, various artificial joint implants, fracture fixation devices, heart valves, and vascular stents are all subjected to significant repetitive loadings. On the other hand...
Series: ASM Handbook
Volume: 23A
Publisher: ASM International
Published: 12 September 2022
DOI: 10.31399/asm.hb.v23A.9781627083928
EISBN: 978-1-62708-392-8
Image
Published: 01 December 2008
Fig. 6 Biomedical applications for investment castings. (a) Whiteside hip-femoral prosthesis. (b) Whiteside II-C knee-tibial base. (c) London elbow-humeral prosthesis. All cast in ASTM F75 cobalt-chromium-molybdenum alloy; all courtesy of Dow Corning Wright More
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005741
EISBN: 978-1-62708-171-9
... cermet coatings. chromium carbide chromium oxide orthopaedic joints substrate selection thermal spray coating titanium THERMAL SPRAY COATINGS have been used for biomedical devices for decades, primarily in the orthopaedic and dental fields. The purpose of this article is to give readers...
Image
Published: 12 September 2022
Fig. 1 Additive-manufactured biomedical devices for applications from arthroplasty to dental appliance. (a) As-printed directed-energy deposition hip stem. (b) Powder-bed fusion as-printed hip stem with support structures. (c) Hip stem with support structures removed. (d) Acetabular cup. (e More
Series: ASM Handbook
Volume: 23A
Publisher: ASM International
Published: 12 September 2022
DOI: 10.31399/asm.hb.v23A.a0006859
EISBN: 978-1-62708-392-8
... Abstract Powder-bed fusion (PBF) is a group of additive manufacturing (AM) processes that includes selective laser sintering, selective laser melting, and electron beam melting. This article explains the processes and parameters of PBF systems that are used for biomedical applications. It also...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005670
EISBN: 978-1-62708-198-6
... Abstract This article focuses on the use of noble and precious metals for biomedical applications. These include gold, platinum, palladium, ruthenium, rhodium, iridium, and osmium. The physical and mechanical properties of noble and precious metals are presented in tables. A brief discussion...
Series: ASM Handbook
Volume: 23A
Publisher: ASM International
Published: 12 September 2022
DOI: 10.31399/asm.hb.v23A.a0006885
EISBN: 978-1-62708-392-8
... applications of DED for titanium-base biomedical implants. It concludes with a section on the forecast of DED in biomedical applications. bioceramic coatings biomedical alloys biomedical implants cobalt-chromium-molybdenum alloys computational modeling directed-energy deposition magnesium alloys...
Series: ASM Handbook
Volume: 23A
Publisher: ASM International
Published: 12 September 2022
DOI: 10.31399/asm.hb.v23A.a0006888
EISBN: 978-1-62708-392-8
..., and PH stainless steels for biomedical applications. In addition, the challenges and obstacles to the clinical use of AM parts are covered. binder jet biomedical devices directed-energy deposition laser powder-bed fusion stainless steel MEDICAL DEVICES, according to the U.S. Food and Drug...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005654
EISBN: 978-1-62708-198-6
... Abstract This article describes mechanical/electrochemical phenomena related to in vivo degradation of metals used for biomedical applications. It discusses the properties and failure of these materials as they relate to stress-corrosion cracking (SCC) and corrosion fatigue (CF). The article...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004208
EISBN: 978-1-62708-184-9
... cracking (SCC). It discusses some of the mechanical and electrochemical phenomena related to the in vivo degradation of materials used for biomedical applications. These materials include stainless steels, cobalt and titanium-base alloy systems, and dental amalgam. The article addresses key issues related...
Series: ASM Handbook
Volume: 23A
Publisher: ASM International
Published: 12 September 2022
DOI: 10.31399/asm.hb.v23A.a0006882
EISBN: 978-1-62708-392-8
... used for biomedical applications. Due to the complex nature of this printing process, many key print parameters and material properties need to be considered to ensure a successful print. These influential parameters are addressed throughout the article to inform the reader of the considerations...
Series: ASM Handbook
Volume: 23A
Publisher: ASM International
Published: 12 September 2022
DOI: 10.31399/asm.hb.v23A.a0006908
EISBN: 978-1-62708-392-8
... Abstract Additive manufacturing, or three-dimensional printing technologies, for biomedical applications is rather different from other engineering components, particularly for biomedical implants that are intended to be used within the human body. This article contains two sections: "Design...
Series: ASM Handbook
Volume: 23A
Publisher: ASM International
Published: 12 September 2022
DOI: 10.31399/asm.hb.v23A.a0006906
EISBN: 978-1-62708-392-8
...; rather, what occurred is an improvement in their methods of manufacturing. This article discusses the fundamentals, benefits, manufacturing, and other application examples beyond orthopedics of PSIs. In addition, an outlook of AM in biomedical applications is also covered. additive manufacturing...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005669
EISBN: 978-1-62708-198-6
... properties of cast and wrought cobalt alloys. The article contains tables that list the commonly used cobalt alloys and their biomedical applications and chemical compositions. It discusses the mechanical and corrosion properties of cobalt alloys, and provides a description of the microstructure of cobalt...
Series: ASM Handbook
Volume: 23A
Publisher: ASM International
Published: 12 September 2022
DOI: 10.31399/asm.hb.v23A.a0006883
EISBN: 978-1-62708-392-8
..., the flowability of powder feedstock, and polymer part characteristics. The article describes the types of polymers in PBF, the processes involved in powder recycling, and the prospects of PBF in AM. In addition, the biomedical application of polyether ether ketone (PEEK) is also covered. biomedical...
Series: ASM Handbook
Volume: 23A
Publisher: ASM International
Published: 12 September 2022
DOI: 10.31399/asm.hb.v23A.a0006861
EISBN: 978-1-62708-392-8
... the in vitro cytocompatibility and in vivo biocompatibility of both binder-jetted and direct-inkjetted scaffolds for biomedical applications. Finally, it discusses the challenges and troubleshooting methodologies in 3D inkjetting of biomaterials. biomaterials biomedical applications in vitro...
Series: ASM Handbook
Volume: 23A
Publisher: ASM International
Published: 12 September 2022
DOI: 10.31399/asm.hb.v23A.a0006892
EISBN: 978-1-62708-392-8
... for a suitable biomaterial, currently used biomaterials, and cells and cellular structures. Additionally, applications of microvalve jetting in biomedical engineering are presented, which include cellular and RNA analysis, high-throughput drug screening, and tissue engineering. biomaterials cellular...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001080
EISBN: 978-1-62708-162-7
... cycle to maturity in the aircraft industry. The metal is still in the growth stage in applications where corrosion resistance is important, such as the marine and biomedical industries. Other commercial and consumer applications, such as in the automotive industry and in architecture, are only...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005674
EISBN: 978-1-62708-198-6
... cases, heart valve parts, and load-bearing bone or hip joint replacements or bone splints. Hip replacements are a common biomedical application of titanium alloys today (2011), and nearly half of all knee replacements use titanium. Other biomedical applications include: Expandable titanium rib...