Published: 12 September 2022
Fig. 20 Elastic modulus values for various biomedical alloys. CP, commercially pure; ST, solution treated. Source: Ref 161 More
Book Chapter

By Steven Lampman
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005674
EISBN: 978-1-62708-198-6
... biomedical implant alloys are listed in a tabular form. The article presents an overview of the surface-modification methods for titanium and its alloys implants. It concludes with a section on biocompatibility and in vivo corrosion of titanium alloys. artificial heart pumps biocompatibility...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003792
EISBN: 978-1-62708-177-1
... Abstract Metallography plays a significant role in the quality control of metals and alloys used in the manufacture of implantable surgical devices. This article provides information and data on metallographic techniques along with images showing the microstructure of biomedical orthopedic...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004207
EISBN: 978-1-62708-184-9
... alloys are given in Tables 1 , 2 , 3 . Typical microstructures for these three major alloy systems are shown in Fig. 1 . Chemical composition of commonly used stainless steels for biomedical applications Table 1 Chemical composition of commonly used stainless steels for biomedical applications...
Series: ASM Handbook
Volume: 23A
Publisher: ASM International
Published: 12 September 2022
DOI: 10.31399/asm.hb.v23A.a0006885
EISBN: 978-1-62708-392-8
... Abstract This article focuses on the directed-energy deposition (DED) additive manufacturing (AM) technique of biomedical alloys. First, it provides an overview of the DED process. This is followed by a section describing the design and development of the multiphysics computational modeling...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005653
EISBN: 978-1-62708-198-6
... Abstract This article reviews the corrosion interactions between biomedical alloys, in particular iron-base, titanium-base, and cobalt-base alloys, in complex geometries and in applications where there are significant cyclic stresses and potential for wear and fretting motion. It discusses...
Series: ASM Handbook
Volume: 23A
Publisher: ASM International
Published: 12 September 2022
DOI: 10.31399/asm.hb.v23A.a0006907
EISBN: 978-1-62708-392-8
... for Biomedical Applications In this section, the development of zirconium alloy powder for L-PBF is introduced as a case study. Zirconium and its alloys are one of the candidates for metals applicable to magnetic resonance imaging environments, because they have lower magnetic susceptibility than titanium...
Series: ASM Handbook
Volume: 23A
Publisher: ASM International
Published: 12 September 2022
DOI: 10.31399/asm.hb.v23A.a0006889
EISBN: 978-1-62708-392-8
... biomedical-based devices: binder jetting, powder-bed fusion, and directed-energy deposition. The article then characterizes the electrochemical properties of additive-manufactured/processed cobalt-chromium alloys. This is followed by sections providing an evaluation of the biological response to CoCr alloys...
Image
Published: 12 September 2022
Fig. 11 Example of laser-patterned hydroxyapatite coating on AZ31B magnesium biomedical alloy. Source: Ref 64 More
Series: ASM Handbook
Volume: 23A
Publisher: ASM International
Published: 12 September 2022
DOI: 10.31399/asm.hb.v23A.a0006857
EISBN: 978-1-62708-392-8
... directly. In this article, the processing of titanium and its alloys by PBF and DED is described, with a specific focus on their use in biomedical devices. The article then covers the density and mechanical properties of both commercially pure titanium and titanium-aluminum-vanadium alloy. Lastly...
Series: ASM Handbook
Volume: 23A
Publisher: ASM International
Published: 12 September 2022
DOI: 10.31399/asm.hb.v23A.a0006888
EISBN: 978-1-62708-392-8
... Abstract Metallic alloys that are typically used for medical purposes include stainless steels, Ti-6Al-4V, and Co-Cr-Mo. This article discusses the relative merits of each of these alloys. The utilization of stainless steels in the biomedical industry, especially in relation to the additive...
Book Chapter

By Leon Pope, Darpan Shidid, Kate Fox
Series: ASM Handbook
Volume: 23A
Publisher: ASM International
Published: 12 September 2022
DOI: 10.31399/asm.hb.v23A.a0006859
EISBN: 978-1-62708-392-8
... residual stresses and increase fatigue strength and tensile properties ( Ref 26 , 27 ). Materials that are commonly used for SLM-fabricated biomedical applications include titanium alloys, cobalt-chromium alloys, and 316L stainless steel. Table 4 includes a list of materials processed by SLM...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005670
EISBN: 978-1-62708-198-6
... on the ancient history of noble and precious metal use in dentistry is provided. The article discusses the use of direct gold dental filling materials, direct silver dental filling materials, traditional amalgam alloys, high-copper amalgam alloys, and gallium alloys in biomedical applications. It also provides...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004208
EISBN: 978-1-62708-184-9
... cracking (SCC). It discusses some of the mechanical and electrochemical phenomena related to the in vivo degradation of materials used for biomedical applications. These materials include stainless steels, cobalt and titanium-base alloy systems, and dental amalgam. The article addresses key issues related...
Series: ASM Handbook
Volume: 23A
Publisher: ASM International
Published: 12 September 2022
DOI: 10.31399/asm.hb.v23A.a0006908
EISBN: 978-1-62708-392-8
.... additive manufacturing biocompatibility orthopedic implants pure titanium titanium alloys ADDITIVE MANUFACTURING (AM)—or three-dimensional (3D) printing technologies—for biomedical applications is rather different from other engineering components, particularly for biomedical implants...
Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006573
EISBN: 978-1-62708-290-7
... main use for Co-Cr alloys is biomedical applications. Traditional processing methods for the part production of these alloys include casting, powder metallurgy, and metal forming ( Ref 9 – 12 ). However, the steps involved during materials processing followed by metal forming and machining are time...
Book Chapter

By Robert Pilliar, Scott D. Ramsay
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005669
EISBN: 978-1-62708-198-6
... properties of cast and wrought cobalt alloys. The article contains tables that list the commonly used cobalt alloys and their biomedical applications and chemical compositions. It discusses the mechanical and corrosion properties of cobalt alloys, and provides a description of the microstructure of cobalt...
Image
Published: 01 December 2008
Fig. 6 Biomedical applications for investment castings. (a) Whiteside hip-femoral prosthesis. (b) Whiteside II-C knee-tibial base. (c) London elbow-humeral prosthesis. All cast in ASTM F75 cobalt-chromium-molybdenum alloy; all courtesy of Dow Corning Wright More
Book Chapter

Series: ASM Handbook
Volume: 24
Publisher: ASM International
Published: 15 June 2020
DOI: 10.31399/asm.hb.v24.a0006581
EISBN: 978-1-62708-290-7
... Abstract Titanium alloys are known for their high-temperature strength, good fracture resistance, low specific gravity, and excellent resistance to corrosion. Ti-6Al-4V is the most commonly used titanium alloy in the aerospace, aircraft, automotive, and biomedical industries. This article...
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 June 2024
DOI: 10.31399/asm.hb.v12.a0007028
EISBN: 978-1-62708-387-4
... Abstract This article focuses on the fractography of Nitinol, a shape memory alloy of nickel and titanium, in superelastic biomedical applications, which primarily comprise drawn and/or laser-cut wire and tube components. Overload fracture, hydrogen embrittlement fracture, and fatigue fracture...