1-20 of 606 Search Results for

binary alloys

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Image
Published: 15 June 2019
Fig. 17 Effect of magnesium content on mechanical properties of binary alloys More
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005439
EISBN: 978-1-62708-196-2
... that illustrate how various diffusional processes can be modeled. single-phase modeling multiphase modeling diffusion modeling binary alloys multicomponent alloys MODELING DIFFUSION in alloys can be divided into two activities. One activity is to model the changes in composition and phases...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006247
EISBN: 978-1-62708-163-4
... Abstract This article provides a discussion on binary alloy phase diagrams published in this handbook. All diagrams presented are for stable equilibrium conditions, except where metastable conditions are indicated. binary alloy phase diagrams crystal structure The 1083 binary...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006145
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of binary alloy phase diagrams for which arsenic (As) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006171
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of binary alloy phase diagrams for which indium (In) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006149
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of binary alloy phase diagrams for which beryllium (Be) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006219
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of binary alloy phase diagrams for which ytterbium (Yb) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006220
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of binary alloy phase diagrams for which zinc (Zn) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary system...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006209
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of binary alloy phase diagrams for which tantalum (Ta) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006199
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of binary alloy phase diagrams for which rhodium (Rh) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006210
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of binary alloy phase diagrams for which terbium (Tb) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006173
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of binary alloy phase diagrams for which lanthanum (La) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006200
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of binary alloy phase diagrams for which ruthenium (Ru) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006211
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of binary alloy phase diagrams for which tellurium (Te) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006201
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of binary alloy phase diagrams for which sulfur (S) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006212
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of binary alloy phase diagrams for which thorium (Th) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006153
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of binary alloy phase diagrams for which cadmium (Cd) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006189
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of binary alloy phase diagrams for which nickel (Ni) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006174
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of binary alloy phase diagrams for which lithium (Li) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006213
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of binary alloy phase diagrams for which titanium (Ti) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary...