... Abstract This article discusses the stable and metastable three-phase fields in the binary Fe-C phase diagram. It schematically illustrates that austenite decomposition requires accounting for nucleation and growth of ferrite and then nucleation and growth of pearlite in the remaining...
Image
Published: 31 August 2017
Fig. 2 Phase diagram of the binary Fe-C system: The stable system (Fe-graphite) is shown with full lines; the metastable system (Fe-Fe 3 C) is shown with dotted lines. Source: Ref 2 More
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006162
EISBN: 978-1-62708-163-4
... “Be (Beryllium) Binary Alloy Phase Diagrams.” “C-Fe (Carbon - Iron)” in the article “C (Carbon) Binary Alloy Phase Diagrams.” “Ce-Fe (Cerium - Iron)” in the article “Ce (Cerium) Binary Alloy Phase Diagrams.” “Co-Fe (Cobalt - Iron)” in the article “Co (Cobalt) Binary Alloy Phase Diagrams...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006217
EISBN: 978-1-62708-163-4
... Diagrams.” “Be-W (Beryllium - Tungsten)” in the article “Be (Beryllium) Binary Alloy Phase Diagrams.” “C-W (Carbon - Tungsten)” in the article “C (Carbon) Binary Alloy Phase Diagrams.” “Co-W (Cobalt - Tungsten)” in the article “Co (Cobalt) Binary Alloy Phase Diagrams.” “Cr-W...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006203
EISBN: 978-1-62708-163-4
... Diagrams .” “C-Sc (Carbon - Scandium)” in the article “C (Carbon) Binary Alloy Phase Diagrams .” “Cr-Sc (Chromium - Scandium)” in the article “Cr (Chromium) Binary Alloy Phase Diagrams .” “Fe-Sc (Iron - Scandium)” in the article “Fe (Iron) Binary Alloy Phase Diagrams .” “Ga-Sc...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006212
EISBN: 978-1-62708-163-4
... (Beryllium - Thorium)” in the article “Be (Beryllium) Binary Phase Diagrams.” “C-Th (Carbon - Thorium)” in the article “C (Carbon) Binary Phase Diagrams.” “Cd-Th (Cadmium - Thorium)” in the article “Cd (Cadmium) Binary Phase Diagrams.” “Co-Th (Cobalt - Thorium)” in the article “Co...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006216
EISBN: 978-1-62708-163-4
....” “B-V (Boron - Vanadium)” in the article “B (Boron) Binary Phase Diagrams.” “C-V (Carbon - Vanadium)” in the article “C (Carbon) Binary Phase Diagrams.” “Co-V (Cobalt - Vanadium)” in the article “Co (Cobalt) Binary Phase Diagrams.” “Cr-V (Chromium - Vanadium)” in the article “Cr...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006215
EISBN: 978-1-62708-163-4
....” “Bi-U (Bismuth - Uranium)” in the article “Bi (Bismuth) Binary Alloy Phase Diagrams.” “C-U (Carbon - Uranium)” in the article “C (Carbon) Binary Alloy Phase Diagrams.” “Cr-U (Chromium - Uranium)” in the article “Cr (Chromium) Binary Alloy Phase Diagrams.” “Fe-U (Iron - Uranium...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006213
EISBN: 978-1-62708-163-4
... (Carbon - Titanium) ” in the article “C (Carbon) Binary Alloy Phase Diagrams.” “ Be-Ti (Cerium - Titanium) ” in the article “Ce (Cerium) Binary Alloy Phase Diagrams.” “Co-Ti (Cobalt - Titanium) ” in the article “Co (Cobalt) Binary Alloy Phase Diagrams.” “Cr-Ti (Chromium - Titanium...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006173
EISBN: 978-1-62708-163-4
... Diagrams.” “Au-La (Gold - Lanthanum)” in the article “Au (Gold) Binary Phase Diagrams.” “Bi-La (Bismuth - Lanthanum)” in the article “Bi (Bismuth) Binary Phase Diagrams.” “C-La (Carbon - Lanthanum)” in the article “C (Carbon) Binary Phase Diagrams.” “Cd-La (Cadmium - Lanthanum...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006190
EISBN: 978-1-62708-163-4
....” “Cr-O (Chromium - Oxygen)” in the article “Cr (Chromium) Binary Alloy Phase Diagrams.” “Cs-O (Cesium - Oxygen)” in the article “Cs (Cesium) Binary Alloy Phase Diagrams.” “Cu-O (Copper - Oxygen)” in the article “Cu (Copper) Binary Alloy Phase Diagrams.” “Fe-O (Iron - Oxygen...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006205
EISBN: 978-1-62708-163-4
...)” in the article “Ba (Barium) Binary Alloy Phase Diagrams.” “Be-Si (Beryllium - Silicon)” in the article “Be (Beryllium) Binary Alloy Phase Diagrams.” “C-Si (Carbon - Silicon)” in the article “C (Carbon) Binary Alloy Phase Diagrams.” “Ca-Si (Calcium - Silicon)” in the article “Ca (Calcium...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006207
EISBN: 978-1-62708-163-4
....” “Cs-Sn (Cesium - Tin)” in the article “Cs (Cesium) Binary Alloy Phase Diagrams.” “Cu-Sn (Copper - Tin)” in the article “Cu (Copper) Binary Alloy Phase Diagrams.” “Dy-Sn (Dysprosium - Tin)” in the article “Dy (Dysprosium) Binary Alloy Phase Diagrams.” “Fe-Sn (Iron - Tin...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006151
EISBN: 978-1-62708-163-4
... Abstract This article is a compilation of binary alloy phase diagrams for which carbon (C) is the first named element in the binary pair. The diagrams are presented with element compositions in weight percent. The atomic percent compositions are given in a secondary scale. For each binary...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006178
EISBN: 978-1-62708-163-4
... Phase Diagrams” “C-Mo (Carbon - Molybdenum)” in the article “C (Carbon) Binary Alloy Phase Diagrams” “Co-Mo (Cobalt - Molybdenum)” in the article “Co (Cobalt) Binary Alloy Phase Diagrams” “Cr-Mo (Chromium - Molybdenum)” in the article “Cr (Chromium) Binary Alloy Phase Diagrams...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006177
EISBN: 978-1-62708-163-4
....” “C-Mn (Carbon - Manganese)” in the article “C (Carbon) Binary Alloy Phase Diagrams.” “Ce-Mn (Cerium - Manganese)” in the article “Ce (Cerium) Binary Alloy Phase Diagrams.” “Co-Mn (Cobalt - Manganese)” in the article “Co (Cobalt) Binary Alloy Phase Diagrams.” “Cr-Mn (Chromium...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006179
EISBN: 978-1-62708-163-4
... element in the binary pair. Additional binary systems that include nitrogen are provided in the following locations in this Volume: “Fe-N (Iron - Nitrogen)” in the article “Fe (Iron) Binary Alloy Phase Diagrams.” “Hf-N (Hafnium - Nitrogen)” in the article “Hf (Hafnium) Binary Alloy Phase...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006166
EISBN: 978-1-62708-163-4
... Phase Diagrams.” “Cu-H (Copper - Hydrogen)” in the article “Cu (Copper) Binary Alloy Phase Diagrams.” “Fe-H (Iron - Hydrogen)” in the article “Fe (Iron) Binary Alloy Phase Diagrams.” H-La (Hydrogen-Lanthanum) H-La crystallographic data H-Li (Hydrogen-Lithium...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006187
EISBN: 978-1-62708-163-4
... - Niobium)” in the article “Cr (Chromium) Binary Alloy Phase Diagrams.” “Cu-Nb (Copper - Niobium)” in the article “Cu (Copper) Binary Alloy Phase Diagrams.” “Fe-Nb (Iron - Niobium)” in the article “Fe (Iron) Binary Alloy Phase Diagrams.” “Ga-Nb (Gallium - Niobium)” in the article “Ga...
Series: ASM Handbook
Volume: 3
Publisher: ASM International
Published: 27 April 2016
DOI: 10.31399/asm.hb.v03.a0006167
EISBN: 978-1-62708-163-4
... in the binary pair. Additional binary systems that include hafnium are provided in the following locations in this Volume: “Be-Hf (Beryllium - Hafnium)” in the article “Be (Beryllium) Binary Alloy Phase Diagrams.” “C-Hf (Carbon - Hafnium)” in the article “C (Carbon) Binary Alloy Phase Diagrams...