1-16 of 16 Search Results for

bimetal sliding bearings

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003167
EISBN: 978-1-62708-199-3
... with bearing material properties. Sliding bearings are commonly classified by terms that describe their application; they also are classified according to material construction, as single-metal, bimetal, or trimetal sliding bearings. The article further provides detailed tabular data on the designation...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006412
EISBN: 978-1-62708-192-4
..., bimetal systems, and trimetal systems. The article describes the designations, nominal compositions, mechanical properties, and applications of various sliding bearing alloys: tin-base alloys, lead-base alloys, copper-base alloys, aluminum-base alloys, silver-base alloys, zinc-base alloys, additional...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006551
EISBN: 978-1-62708-210-5
... to their relatively low hardness, which favors large plastic deformation under sliding conditions. This article discusses the classes and mechanisms of wear in aluminum-silicon alloys, aluminum-tin bearing alloys, and aluminum-matrix composites; describes the effect of material-related parameters on wear behavior...
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006806
EISBN: 978-1-62708-329-4
... Abstract A mechanical part, which supports the moving part, is termed a mechanical bearing and can be classified into rolling (ball or roller) bearings and sliding bearings. This article discusses the failures of sliding bearings. It first describes the geometry of sliding bearings, next...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001809
EISBN: 978-1-62708-180-1
... Abstract This article discusses the classification of sliding bearings and describes the major groups of soft metal bearing materials: babbitts, copper-lead bearing alloys, bronze, and aluminum alloys. It provides a discussion on the methods for fluid-film lubrication in bearings. The article...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003326
EISBN: 978-1-62708-176-4
... Abstract This article provides an overview of two major classes of bearings: rolling bearings and sliding, or plain, bearings. It reviews the experimental data resulted from testing of rolling and sliding bearing materials with illustration. The article presents a table that summarizes rolling...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006398
EISBN: 978-1-62708-192-4
..., respectively. Sliding bearings are also frequently classified according to material construction as single-metal (solid), bimetal (two-layer), or trimetal (three-layer) bearings. These terms refer to the number of principal functional layers that are used. Each one of these types of construction...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001273
EISBN: 978-1-62708-170-2
..., or bronze. The base metal may be in the form of mild steel strip unwound from a coil, a half-round mild steel pressing or bushing, or a bronze or iron casting. The bonded bimetal material is shaped and machined to make plain, fluid film lubricated bearings for a wide variety of automotive, industrial...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.9781627081924
EISBN: 978-1-62708-192-4
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001383
EISBN: 978-1-62708-173-3
... at that time: Shaft reclamation ( Ref 3 ) Hardfacing of agricultural parts ( Ref 4 ) Reconditioning bushings of sliding friction bearings and roll trunnions ( Ref 5 , 6 , 7 , 8 , 9 ) Hardfacing ( Ref 10 ) and improving wear resistance in gas and oil equipment ( Ref 11 ) Process...
Book Chapter

Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005560
EISBN: 978-1-62708-174-0
... at that time: Shaft reclamation ( Ref 3 ) Hardfacing of agricultural parts ( Ref 4 ) Reconditioning bushings of sliding friction bearings and roll trunnions ( Ref 5 , 11 , 12 , 13 , 14 ) Hardfacing ( Ref 11 ) and improving wear resistance in gas and oil equipment ( Ref 12 ) Currently...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001097
EISBN: 978-1-62708-162-7
... conductivity, mechanical properties, chemical properties, fabrication properties, and thermal properties. The article presents a brief note on brush contact materials and their interdependence factors for sliding contacts. It also describes the type of commercial contact materials for electrical contacts...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005625
EISBN: 978-1-62708-174-0
...: the Peltier effect and the Thomson effect. To combine all three effects, two different situations are examined: one typical of an industrial sheet-metal-type weld and one typical of an electrical interconnection. Peltier Effect The Peltier effect occurs when the flow of current through a bimetallic...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003137
EISBN: 978-1-62708-199-3
... of fluid flow Design for streamlined flow; keep velocity low; remove gases from liquid phase; use erosion-resistant alloy Fretting Chafing or galling, often occurring during shipment Lubricate contacting surfaces; interleave sheets of paper between sheets of metal; decrease load on bearing surfaces...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003816
EISBN: 978-1-62708-183-2
..., lead frames, and connectors Industrial products such as molds and bearings Copper and its alloys are unique among the corrosion-resistant alloys in that they do not form a truly passive corrosion product film. In aqueous environments at ambient temperatures, the corrosion product predominantly...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001096
EISBN: 978-1-62708-162-7
..., but temperature changes are relatively unimportant. Copper-Manganese-Nickel Resistance Alloys Copper-manganese-nickel resistance alloys, generally referred to as manganins, have been adopted almost universally for precision resistors, slide wires and other resistive components with values of 1 nΩ or less...