1-20 of 234

Search Results for beryllium grades

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book Chapter

By A. James Stonehouse, James M. Marder
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001086
EISBN: 978-1-62708-162-7
.... Beginning with an overview of the mining and refining processes of beryllium, this article discusses powder production and consolidation methods, beryllium grades and their designations, and the protective measures that have been enacted to reduce exposure to beryllium. beryllium beryllium...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003165
EISBN: 978-1-62708-199-3
... conductivity. The article describes structural, instrument, and optical grade beryllium and the corresponding compositional ranges. It also discusses processing and product forms as well as factors affecting corrosion resistance. The article concludes with a short note on health and safety considerations when...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006058
EISBN: 978-1-62708-175-7
... and aluminum-beryllium alloys such as extrusion, rolling, welding, joining, and machining are discussed. The article discusses quality control and provides information on the structural, optical, and high-purity grades of beryllium. aluminum-beryllium alloys beryllium alloys beryllium powder cold...
Book Chapter

Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005142
EISBN: 978-1-62708-186-3
... pulverizing a vacuum-cast ingot. The hot pressed block can be warm rolled to the desired sheet thickness. Unalloyed beryllium is available in two grades, I (instrument grade) and S (structural grade). Typical applications for instrument-grade beryllium include gyroscopes, components in inertial guidance...
Image
Published: 30 September 2015
Fig. 2 Near-net shape O-30-grade beryllium mirror blank segment processed by hot isostatic pressing for the James Webb Space Telescope More
Book Chapter

By Douglas V. Gallagher, R.E. Hardesty
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002191
EISBN: 978-1-62708-188-7
... of as-machined, annealed, and etched beryllium Table 2 Transverse tensile properties of as-machined, annealed, and etched beryllium Grade Condition Ultimate tensile strength 0.2% yield strength Yield point, MPa (ksi) Elongation, % MPa ksi MPa ksi S200E Before machining 366 53.1 227...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003827
EISBN: 978-1-62708-183-2
... that contains halide, sulfate, or nitrate ions. The article provides information on the behavior of beryllium under the combined effects of high-purity water environment, stress and chemical environment, and high-temperature environment. The compositions of the structural grades for intentionally controlled...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003770
EISBN: 978-1-62708-177-1
... Abstract The two major types of beryllium-containing alloys are copper-berylliums and nickel-berylliums. The most widely used beryllium-containing alloys are wrought copper-berylliums, which provide good strength while retaining useful levels of electrical and thermal conductivity. This article...
Book Chapter

By Roy I. Batista
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001456
EISBN: 978-1-62708-173-3
... oxide content. It is partially through the control of this oxide that the final properties of the beryllium are achieved. Them are structural, optical, and instrument grades of beryllium to permit design optimization. Other forms of beryllium sheet, plate, or extrusions are fabricated from the block...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003331
EISBN: 978-1-62708-176-4
... Mullite 18 14 Niobium carbide 10 9 Beryllium carbide 9+ … Tantalum carbide 9+ … Beryllia 9 … Alumina 9 … Titanium carbide 9 8 Zirconium carbide 9 8 Zirconia 8 7 Zircon 8 … Steatite 7.5 … Thoria 7 … Magnesia 6 … Porcelain enamel 6 3.5...
Book Chapter

By Bo Hu
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006090
EISBN: 978-1-62708-175-7
..., and so forth, play a great role in the efficiency of oxygen scavenging. Chemically reduced iron powder and electrolytic iron powder are two common types of iron powders used in oxygen scavengers. Because the applications are related to consumer food products, the iron powder should be a food grade...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001071
EISBN: 978-1-62708-162-7
... Abstract Addition of beryllium, up to about 2 wt″, produces dramatic effects in copper, nickel, aluminum, magnesium, gold, zinc, and other base metal alloys. This article provides information on the chemical composition, microstructure, heat treatment, fabrication characteristics, production...
Book Chapter

By Jack A. Hamill, Jr.
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006018
EISBN: 978-1-62708-175-7
..., iron  Filters for fuel, hydraulic fluids, air Bronze, stainless steel, nickel  Hardware Aluminum, beryllium, titanium, iron  Heat shields Beryllium, tungsten  Heat shield coating Aluminum  Jet engine components Superalloys  Magnetic shields Aluminum, nickel, cobalt  Measuring...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003181
EISBN: 978-1-62708-199-3
... Abstract This article provides a detailed account on forming operations (blanking, piercing, press-brake forming, contour rolling, deep drawing, cold forming, and hot forming) of various nonferrous metals, including aluminum alloys, beryllium, copper and its alloys, magnesium alloys, nickel...
Book Chapter

By Chester J. Van Tyne, John Walters
Series: ASM Handbook
Volume: 4C
Publisher: ASM International
Published: 09 June 2014
DOI: 10.31399/asm.hb.v04c.a0005884
EISBN: 978-1-62708-167-2
... deformation is excellent with the exception of the machinable grades. Hot deformation has an effect on the mechanical properties of ductility, impact toughness, and fatigue life of the final component. The change in properties occurs due to the breakup of segregation, closing of pores, and the homogenization...
Book Chapter

Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002185
EISBN: 978-1-62708-188-7
... Alloys that are difficult to machine, including the nonleaded coppers, low-zinc brasses and nickel silvers, the phosphor bronzes and aluminum bronzes, cupro-nickel, and some beryllium copper Machinability Ratings Table 1 lists the nominal compositions and machinability ratings of the most...
Book Chapter

By Sabit Ali
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006281
EISBN: 978-1-62708-169-6
..., nickel-aluminum bronzes, silicon bronzes, and beryllium bronzes. This article briefly discusses the types, hardening mechanisms, heat treatment processes, applications, and mechanical properties of these bronzes and high-copper alloys. beryllium-copper alloys cast aluminum bronze cast beryllium...
Book Chapter

Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005644
EISBN: 978-1-62708-174-0
... with rutile and basic electrodes Vanadium steel … … … … Low-carbon-grade electrodes. Minimum heat input 30 kJ/mm (760 kJ/in.) for 30 mm (1.2 in.) thickness, unless preheating or low-hydrogen electrodes are employed C-Mn steel (0.15–0.025 C) 100–200 (212–390) … … … For thick sections, low...
Book Chapter

By R. Terrence Webster
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001084
EISBN: 978-1-62708-162-7
..., and the role of oxygen. It concludes by providing useful information on the applications of reactor and industrial grades of zirconium alloys. allotropic transformation anisotropy applications of zirconium alloys cold work fabrication hafnium recrystallization zirconium zirconium alloys...
Book Chapter

By M. Ned Rogers
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001438
EISBN: 978-1-62708-173-3
... contain alloying elements to enhance a specific property or characteristic, for example, machinability Many copper alloys have common names, such as oxygen-free copper (99.95% Cu min), beryllium copper (0.2 to 2.0% Be), Muntz metal (Cu-40Zn), Naval brass (Cu-39.25Zn-0.75Sn), and commercial bronze...