Skip Nav Destination
Close Modal
By
C.H. Hager, Jr., W.M. Hannon, V.M. Bedekar
By
Arthur Reardon
By
Alan J. Chidester, Craig V. Darragh, Robert C. Hoff, John R. Imundo, James L. Maloney, III ...
Search Results for
bearing
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 1974
Search Results for bearing
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001024
EISBN: 978-1-62708-161-0
... Abstract Bearing steels, which include high-carbon and low-carbon types, can be divided into service-based classes, such as normal service, high-temperature service, and service under corrosive conditions. This article discusses the importance of matching the hardenability and quenching...
Abstract
Bearing steels, which include high-carbon and low-carbon types, can be divided into service-based classes, such as normal service, high-temperature service, and service under corrosive conditions. This article discusses the importance of matching the hardenability and quenching of a bearing steel. It also discusses the typical microstructure of a high-carbon through-hardened bearing, and shows typical case and core microstructures in carburized bearing materials. Apart from a satisfactory microstructure, which is obtained through the proper combination of steel grade and heat treatment, the single most important factor in achieving high levels of rolling-contact fatigue life in bearings is the cleanliness, or freedom from harmful nonmetallic inclusions, of the steel. Alloy conservation and a more consistent heat-treating response are benefits of using specially designed bearing steels. The selection of a carburizing steel for a specific bearing section is based on the heat-treating practice of the producer, either direct quenching from carburizing or reheating for quenching, and on the characteristics of the quenching equipment.
Book Chapter
Tribology and Wear of Bearing Steels
Available to PurchaseSeries: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006393
EISBN: 978-1-62708-192-4
... Abstract This article discusses the composition, properties and applications of bearing steels. It focuses on the typical wear modes that rolling-element bearings experience: contact fatigue wear, abrasive wear, adhesive wear, and corrosive wear. The article provides information on reliability...
Abstract
This article discusses the composition, properties and applications of bearing steels. It focuses on the typical wear modes that rolling-element bearings experience: contact fatigue wear, abrasive wear, adhesive wear, and corrosive wear. The article provides information on reliability factor and ABMA and ISO environmental factors.
Book Chapter
Friction and Wear of Sliding Bearing Materials
Available to PurchaseSeries: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006412
EISBN: 978-1-62708-192-4
... Abstract A sliding bearing (plain bearing) is a machine element designed to transmit loads or reaction forces to a shaft that rotates relative to the bearing. This article discusses the properties of bearing materials. It provides information on bearing material systems: single-metal systems...
Abstract
A sliding bearing (plain bearing) is a machine element designed to transmit loads or reaction forces to a shaft that rotates relative to the bearing. This article discusses the properties of bearing materials. It provides information on bearing material systems: single-metal systems, bimetal systems, and trimetal systems. The article describes the designations, nominal compositions, mechanical properties, and applications of various sliding bearing alloys: tin-base alloys, lead-base alloys, copper-base alloys, aluminum-base alloys, silver-base alloys, zinc-base alloys, additional metallic materials, nonmetallic materials. It describes casting processes, powder metallurgy processes, and electroplating processes. The article also discusses the selection criteria for bearing materials.
Book Chapter
Bearing Steels
Available to PurchaseSeries: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003099
EISBN: 978-1-62708-199-3
... Abstract Rolling-element bearings, whether ball bearings or roller bearings with spherical, straight, or tapered rollers, are fabricated from a wide variety of steels. This article discusses the production process, characteristics, nominal compositions, and types of bearing steels...
Abstract
Rolling-element bearings, whether ball bearings or roller bearings with spherical, straight, or tapered rollers, are fabricated from a wide variety of steels. This article discusses the production process, characteristics, nominal compositions, and types of bearing steels. These include standard bearing steels, such as high-carbon bearing steels and carburizing bearing steels; and special-purpose bearing steels, such as high-temperature service bearing steels and corrosion-resistant bearing steels.
Book Chapter
850.0, 851.0, 852.0, and 853.0 Bearing Alloys
Available to PurchaseSeries: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006590
EISBN: 978-1-62708-210-5
... Abstract The aluminum-tin alloys 850.0, 851.0, 852.0, and 853.0 are specialized compositions displaying excellent bearing characteristics under moderate loads and with effective lubrication. This datasheet provides information on key alloy metallurgy, fabrication characteristics, processing...
Abstract
The aluminum-tin alloys 850.0, 851.0, 852.0, and 853.0 are specialized compositions displaying excellent bearing characteristics under moderate loads and with effective lubrication. This datasheet provides information on key alloy metallurgy, fabrication characteristics, processing effects on physical and mechanical properties, and application characteristics of these alloys. Permanent-mold aluminum casting rotating-beam fatigue curves for 850.0-T101, 850.0-T5, and 852.0-T5 alloys are also presented.
Book Chapter
Fracture and Fractography of Tool Steels and Bearing Steels
Available to PurchaseBook: Fractography
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 June 2024
DOI: 10.31399/asm.hb.v12.a0007029
EISBN: 978-1-62708-387-4
... Abstract This article describes some of the underlying factors of tool steel and bearing steel fractures and appearances. It also briefly introduces the general types of cold work and hot work tool steels and their typical performance requirements. This includes the importance...
Abstract
This article describes some of the underlying factors of tool steel and bearing steel fractures and appearances. It also briefly introduces the general types of cold work and hot work tool steels and their typical performance requirements. This includes the importance of microstructural conditions achieved with powder metallurgy (PM) tool steels and the need for steel “cleanliness,” especially in preventing contact fatigue in bearings or bending fatigue in gears.
Book: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001273
EISBN: 978-1-62708-170-2
... to casting, the workpiece must be scrupulously prepared by various cleaning, fluxing, and tinning steps. Babbitting of bearing shells can be accomplished by three methods, namely, static babbitting, centrifugal casting, and metal spray babbitting. babbitting bearing shells bond quality centrifugal...
Abstract
Babbitting is a process by which relatively soft metals are bonded chemically or mechanically to a stronger shell or stiffener which supports the weight and torsion of a rotating, oscillating, or sliding shaft. This article focuses on workpiece preparation and babbitting methods. Prior to casting, the workpiece must be scrupulously prepared by various cleaning, fluxing, and tinning steps. Babbitting of bearing shells can be accomplished by three methods, namely, static babbitting, centrifugal casting, and metal spray babbitting.
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003326
EISBN: 978-1-62708-176-4
... Abstract This article provides an overview of two major classes of bearings: rolling bearings and sliding, or plain, bearings. It reviews the experimental data resulted from testing of rolling and sliding bearing materials with illustration. The article presents a table that summarizes rolling...
Abstract
This article provides an overview of two major classes of bearings: rolling bearings and sliding, or plain, bearings. It reviews the experimental data resulted from testing of rolling and sliding bearing materials with illustration. The article presents a table that summarizes rolling contact fatigue test methods that ASTM published in STP 771. It also describes the role of lubrication in the bearings.
Image
Softening characteristics of cadmium-bearing copper and silver-bearing toug...
Available to Purchase
in Introduction to Copper and Copper Alloys
> Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Published: 01 January 1990
Fig. 2 Softening characteristics of cadmium-bearing copper and silver-bearing tough pitch copper. (a) Softening curves for material cold reduced 21% in area, from 0.1 to 0.075 mm (0.0038 to 0.0030 in.) in thickness. (b) Softening curves for material cold reduced 90% in area, from 0.75 to 0.075
More
Image
Variation in bearing pathway diameter of a needle bearing cup drawn using h...
Available to PurchasePublished: 01 January 2006
Fig. 33 Variation in bearing pathway diameter of a needle bearing cup drawn using high-speed tool steel and carbide dies
More
Image
Published: 01 January 1989
Image
Foil bearing designs. (a) Tension-dominated foil bearing. (b) Multilayer fo...
Available to PurchasePublished: 31 December 2017
Fig. 25 Foil bearing designs. (a) Tension-dominated foil bearing. (b) Multilayer foil bearing. (c) Bump foil bearing
More
Book Chapter
Heat Treatment of Bearings
Available to PurchaseSeries: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005978
EISBN: 978-1-62708-168-9
... Abstract The choice of heat treatment depends on the service requirements of a given bearing and how the bearing will be made. This article describes the design parameters, material characteristics required to sustain performance characteristics, metallurgical properties, and dimensional...
Abstract
The choice of heat treatment depends on the service requirements of a given bearing and how the bearing will be made. This article describes the design parameters, material characteristics required to sustain performance characteristics, metallurgical properties, and dimensional stability. It also provides a description of various extensively-used heat treatment processes, namely, carburizing, carbonitriding, induction surface hardening, and nitriding associated with various bearings. In addition, the article explores the factors to be considered in selecting a process and explains why it is optimum for a specific application.
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001809
EISBN: 978-1-62708-180-1
... Abstract This article discusses the classification of sliding bearings and describes the major groups of soft metal bearing materials: babbitts, copper-lead bearing alloys, bronze, and aluminum alloys. It provides a discussion on the methods for fluid-film lubrication in bearings. The article...
Abstract
This article discusses the classification of sliding bearings and describes the major groups of soft metal bearing materials: babbitts, copper-lead bearing alloys, bronze, and aluminum alloys. It provides a discussion on the methods for fluid-film lubrication in bearings. The article presents the variables of interest for a rotating shaft and the load-carrying capacity and surface roughness of bearings. Grooves and depressions are often provided in bearing surfaces to supply or feed lubricant to the load-carrying regions. The article explains the effect of contaminants in bearings and presents the steps for failure analysis of sliding bearings. It also reviews the factors responsible for bearing failure with examples.
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006362
EISBN: 978-1-62708-192-4
... Abstract This article describes the characteristics of three types of gas bearings, such as aerostatic bearing, precision aerodynamic bearing (PAB), and compliant aerodynamic bearing (CAB). It discusses the applications for aerostatic bearings and advantages in lubricating a bearing...
Abstract
This article describes the characteristics of three types of gas bearings, such as aerostatic bearing, precision aerodynamic bearing (PAB), and compliant aerodynamic bearing (CAB). It discusses the applications for aerostatic bearings and advantages in lubricating a bearing with a compressible gas. The article also describes the different types of aerostatic bearings, such as annular thrust bearings and orifice-compensated journal bearings. It presents a discussion on load capacity and stiffness, friction and power loss, and stability and damping of the aerostatic bearings. The article provides a discussion on the types of PAB and CAB. The types include spiral groove annular thrust bearings, cylindrical journal bearings, three-sector journal bearings, tilting-pad journal bearings, and helical-grooved journal bearings. The types of CAB include foil bearings and pressurized-membrane bearings. The article concludes with a description of factors that influence materials selection for gas-lubricated bearings.
Book Chapter
Materials for Sliding Bearings
Available to PurchaseSeries: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003167
EISBN: 978-1-62708-199-3
... Abstract A sliding bearing (plain bearing) is a machine element designed to transmit loads or reaction forces to a shaft that rotates relative to the bearing. This article explains the role of wear damage mechanisms in the design and selection of bearing materials, and its relationship...
Abstract
A sliding bearing (plain bearing) is a machine element designed to transmit loads or reaction forces to a shaft that rotates relative to the bearing. This article explains the role of wear damage mechanisms in the design and selection of bearing materials, and its relationship with bearing material properties. Sliding bearings are commonly classified by terms that describe their application; they also are classified according to material construction, as single-metal, bimetal, or trimetal sliding bearings. The article further provides detailed tabular data on the designation and composition of the following types of bearing materials: tin-base alloys, lead-base alloys, copper-base alloys, and aluminum-base alloys. It also briefly discusses the following types of bearing materials: zinc-base alloys, silver-base alloys, gray cast irons, cemented carbides, and nonmetallic bearing materials.
Series: ASM Handbook
Volume: 11A
Publisher: ASM International
Published: 30 August 2021
DOI: 10.31399/asm.hb.v11A.a0006806
EISBN: 978-1-62708-329-4
... Abstract A mechanical part, which supports the moving part, is termed a mechanical bearing and can be classified into rolling (ball or roller) bearings and sliding bearings. This article discusses the failures of sliding bearings. It first describes the geometry of sliding bearings, next...
Abstract
A mechanical part, which supports the moving part, is termed a mechanical bearing and can be classified into rolling (ball or roller) bearings and sliding bearings. This article discusses the failures of sliding bearings. It first describes the geometry of sliding bearings, next provides an overview of bearing materials, and then presents the various lubrication mechanisms: hydrostatic, hydrodynamic, boundary lubrication, elastohydrodynamic, and squeeze-film lubrication. The article describes the effect of debris and contaminant particles in bearings. The steps involved in failure analysis of sliding bearings are also covered. Finally, the article discusses wear-damage mechanisms from the standpoint of bearing design.
Book: Fatigue and Fracture
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002376
EISBN: 978-1-62708-193-1
... Abstract This article provides information on the nominal compositions of high-carbon bearing steels and carburizing bearing steels. It discusses the bearing fundamentals with emphasis on surface contact, stresses, and fatigue life of bearings. The article describes bearing life prediction...
Abstract
This article provides information on the nominal compositions of high-carbon bearing steels and carburizing bearing steels. It discusses the bearing fundamentals with emphasis on surface contact, stresses, and fatigue life of bearings. The article describes bearing life prediction using three factors, namely, reliability, material, and application. It analyzes the bearing damage modes and concludes with information on fatigue failure considerations.
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0001810
EISBN: 978-1-62708-180-1
... Abstract Rolling-element bearings use rolling elements interposed between two raceways, and relative motion is permitted by the rotation of these elements. This article presents an overview of bearing materials, bearing-load ratings, and an examination of failed bearings. Rolling-element...
Abstract
Rolling-element bearings use rolling elements interposed between two raceways, and relative motion is permitted by the rotation of these elements. This article presents an overview of bearing materials, bearing-load ratings, and an examination of failed bearings. Rolling-element bearings are designed on the principle of rolling contact rather than sliding contact; frictional effects, although low, are not negligible, and lubrication is essential. The article lists the typical characteristics and causes of several types of failures. It describes failure by wear, failure by fretting, failure by corrosion, failure by plastic flow, failure by rolling-contact fatigue, and failure by damage. The article discusses the effects of fabrication practices, heat treatment and hardness of bearing components, and lubrication of rolling-element bearings with a few examples.
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006398
EISBN: 978-1-62708-192-4
... Abstract Bearings are usually provided where a specific spatial relationship (alignment) must be maintained between the parts or where a force is to be transmitted from one part to the other. This article introduces the general types and configuration of sliding bearings, bearing materials...
Abstract
Bearings are usually provided where a specific spatial relationship (alignment) must be maintained between the parts or where a force is to be transmitted from one part to the other. This article introduces the general types and configuration of sliding bearings, bearing materials, and the practical aspects and solutions in the friction, lubrication, and wear mitigation of sliding bearings. The lubrication of bearings includes thick-film lubrication, thin-film lubrication, and boundary lubrication. The article concludes with a discussion on the effects of material elasticity on the lubrication of bearings.