1-20 of 202 Search Results for

arc cladding

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005632
EISBN: 978-1-62708-174-0
... a discussion on the material combinations, characteristics of laser cladding, and the comparison with arc cladding. It reviews the characteristics and applications of near-net shape processing and explains the process involved in powder bed methods and direct powder methods. arc cladding direct powder...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006391
EISBN: 978-1-62708-192-4
... materials, namely, iron-base overlays, chromium carbide-based overlays, nickel- and cobalt-base alloys, and tungsten carbide-based metal-matrix composite overlays. It discusses the types of hardfacing processes, such as arc welding processes, and laser cladded, oxyacetylene brazing and vacuum brazing...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001442
EISBN: 978-1-62708-173-3
... steel weld cladding and the factors influencing joint integrity in dissimilar metal joining. It concludes with a discussion on joining carbon and low-alloy steels to various dissimilar materials (both ferrous and nonferrous) by arc welding. arc welding buildup alloys carbon steel dissimilar...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006364
EISBN: 978-1-62708-192-4
... strong abrasive wear 6 Fe-Cr-C Ni-Hard 4 MMA, GMAW, GTMW, SAW Wear liners 8 Fe-Cr-V-C/Fe-Cr-V-C + WC Hot isostatic pressed cladding Crushing tools for minerals and rollers for hot briquetting, extrusion tools 10 Fe-Cr-C-Nb Deposition welding, open arc welding Rollers...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.a0005589
EISBN: 978-1-62708-174-0
.... , DuPont J.N. , and Marder A.R. , The Role of Aluminum on the Weldability and Sulfidation Behavior of Iron-Aluminum Claddings , Weld. J. , Vol 78 , 1999 , p 23s – 30s 8. DuPont J.N. and Marder A.R. , Thermal Efficiency of Arc Welding Processes , Weld. J. , Vol 74 , Dec...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003157
EISBN: 978-1-62708-199-3
... contact applications. Where aluminum is used in contacting joints, it should be plated or clad with copper, silver, or tin. Aluminum should never be used for power applications where arcing is present. For instance, if aluminum contacts were substituted for silver in a motor starter, an explosion due...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005712
EISBN: 978-1-62708-171-9
... processes for oil sand coatings and overlays are plasma-transferred arc welding, gas metal arc welding, submerged arc welding, flux-cored arc welding, high-velocity oxyfuel, oxyacetylene, spray and fuse, shielded metal arc welding (stick), and laser cladding. Under abrasive wear conditions...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001414
EISBN: 978-1-62708-173-3
... described in Fig. 3 because of the cost of removing a larger portion of the cladding and depositing more stainless steel filler metal. Because there is no danger of alloy contamination from the cladding layer, method A in Fig. 4 permits the use of faster welding processes, such as submerged arc welding...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001084
EISBN: 978-1-62708-162-7
... excellent resistance to many corrosive media, including superheated water, and it is transparent to thermal energy neutrons. These properties prompted the U.S. Navy to use zirconium in water-cooled nuclear reactors as cladding for uranium fuel. In 1958, zirconium became available for industrial use...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003151
EISBN: 978-1-62708-199-3
... Al 2 O 3 + glass slurry Nickel-chromium coating Oxidation-resistant alloy Ni-Cr Flame spray, detonation gun, plasma arc Chromium carbide coating Carbide Cr-C Plasma spray Noble metal coatings Clad Pt, Rh Roll bonding and hermetic sealing Barrier-layer-clad Pt, Rh...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006708
EISBN: 978-1-62708-210-5
... and arc-welded round tube 6061 AMS 4025, 4026, 4027 Sheet and plate 6061-O AMS 4021 Sheet and plate 6061-O Alclad AMS 4079, 4080, 4081, 4082, 4083 Drawn tube (seamless) 6061-O, 6081-T4, 6061-T6 AMS 4113 Extruded shapes 6061-T6 AMS 4115, 4116, 4117 Cold finished bars, rod, wire...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005204
EISBN: 978-1-62708-187-0
... and implants; corrosion-resistant claddings Refractory metals, EB melting and PM Tungsten Heating elements, punches and dies, and nonconsummable electrodes for arc melting and gas tungsten arc welding for metal processing equipment; targets for x-ray equipment and high-sputtering-rate devices...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002168
EISBN: 978-1-62708-188-7
... distribution when heat treating. A galvo-optic device is a common method of directing and focusing the laser beam for metal marking to produce the specified characters. Inert-gas chambers are used in many cladding and surfacing applications, while arc lamps are used to preheat crack-sensitive alloys to reduce...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006736
EISBN: 978-1-62708-210-5
... Abstract This datasheet provides information on composition limits, ASTM product specifications, processing effects on physical and mechanical properties, and applications of cladding fin stock 7072. alloy composition aluminum alloy 7072 cladding fin stock mechanical properties...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001097
EISBN: 978-1-62708-162-7
... Abstract Electrical contacts are metal devices that make and break electrical circuits. This article provides information on materials selection criteria and failure modes of make-break contacts. It describes the property requirements for make-break arcing contacts, namely, electrical...
Series: ASM Handbook
Volume: 5A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v05a.a0005732
EISBN: 978-1-62708-171-9
... 2006 through 2012 “Corrosion Control for Marine- and Land-Based Infrastructure Applications” “Wear-Resistant Coatings” “Corrosion and Wear Control for Industrial Applications” Type of surface modification process, such as thermal spray, laser cladding plasma-transferred arc (PTA...
Series: ASM Handbook
Volume: 6A
Publisher: ASM International
Published: 31 October 2011
DOI: 10.31399/asm.hb.v06a.9781627081740
EISBN: 978-1-62708-174-0
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006686
EISBN: 978-1-62708-210-5
... plus 3 g H 2 O 2 per liter −0.83 V for 3003 and core of Alclad 3003 −0.96 V for 7072 cladding Table 3 Mechanical properties of alloy 3003 Directional characteristics, tensile strength and elongation of sheet in any of the H tempers, are slightly lower in transverse direction Temper...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006079
EISBN: 978-1-62708-175-7
... …  Other … 0.5 Cu 7.5 Co  Iron bal bal … Physical  Particle size, mesh 60∼230 60∼325 140∼325 Source: Ref 2 Table 5 Functions and composition ranges of coating constituents on low-carbon steel arc welding electrodes Coating constituent Function of constituent...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001429
EISBN: 978-1-62708-173-3
... to about 0.05% C by the arc melting practices of the time. The nickel-chromium-molybdenum alloys proved to be extremely important in the chemical processing industry, because they provided corrosion resistance over a wide range of reducing and oxidizing environments. However, grain boundary...