1-20 of 54 Search Results for

amorphous simple metal-transition metal-rare earth metal alloys

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003836
EISBN: 978-1-62708-183-2
... the general corrosion behavior and localized corrosion behavior of transition metal-metal binary alloys, transition metal-metalloid alloys, and amorphous simple metal-transition metal-rare earth metal alloys. It concludes with a discussion on the environmentally induced fracture of glassy alloys...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001089
EISBN: 978-1-62708-162-7
... Materials” in this Volume. A fairly recent commercial development is the use of amorphous rare earth-transition metal alloys for information storage as magnetooptic discs. [1] In this application amorphous Tb 25 (Fe 0.9 Co 0.1 ) 75 thin films (500 to 2000 Å thick) are RF or DC sputtered on...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006057
EISBN: 978-1-62708-175-7
... magnetic properties magnetically soft components magnetism metal injection molding neodymium-iron-boron magnets permanent magnets permeability phosphorus iron powder metallurgy pure iron rare earth-cobalt magnets silicon iron COMMERCIAL SOFT MAGNETIC POWDER METALLURGY (PM) ALLOYS are...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006388
EISBN: 978-1-62708-192-4
... behavior of aluminum alloys, aluminum-base composites, and metal-matrix composites. It presents the effect of material-related parameters and external factors on wear behavior and transitions of aluminum-silicon alloys. The article also presents the most important factors affecting the dry sliding wear...
Book Chapter

By W.L. Johnson
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001095
EISBN: 978-1-62708-162-7
... metalloid element (for example, silicon, phosphorus, boron, carbon, and so on). The Giessen group discovered a second class of metallic liquids that form glasses at rapid solidification rates. These are referred to as the metal-metal systems. These alloys contain an early transition metal or rare earth...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006018
EISBN: 978-1-62708-175-7
... Pyrotechnics Aluminum, graphite, iron, magnesium Radio and television  Cores Iron, MolyPermalloy  Getters (television tubes) Barium, nickel  Permanent magnets Iron, nickel, cobalt, aluminum, barium, ferrites, rare earths  Printed circuits Copper, silver  Receiving tubes Tungsten...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006503
EISBN: 978-1-62708-207-5
.... Goyer R.A. , Toxicity of Metals , Properties and Selection: Nonferrous Alloys and Special-Purpose Materials , Vol 2 , Metals Handbook , 10th ed. , ASM International , 1990 , p 1233 – 1269 68. Meng L. and Zheng X.L. , Overview of the Effects of Impurities and Rare Earth...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004168
EISBN: 978-1-62708-184-9
.... Static conditions are rarely observed in reinforced-concrete structures. Most efforts to fit profiles of chloride content versus depth from the concrete surface employ Fick's second law: (Eq 1) ∂ C ∂ t = D ∂ 2 C ∂ x 2 where C is the chloride ion concentration at some...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001117
EISBN: 978-1-62708-162-7
... Tensile strength: 98.8% pure, amorphous, 1.6 to 2.4 GPa; fibers, 2.6 to 3.1 GPa Compressive strength: with B 2 O 3 present, up to 0.5 GPa 99.9% crystalline: 3300 HK (with 100 g load), 9.3 moh Tension: amorphous, 440 GPa Cadmium is a relatively rare metal that is present in the crust...
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005772
EISBN: 978-1-62708-165-8
... ). Metal boride coatings or deposition via chemical vapor deposition (CVD) of TiB 2 , ZrB 2 , rare earth borides, and so forth on steel, refractory metals, and alloys have been made using the following chloride reaction: (Eq 6) MCl 4 ( g ) + 2 BCL 3 ( g ) + 5 H 2 ( g...
Series: ASM Handbook
Volume: 22B
Publisher: ASM International
Published: 01 November 2010
DOI: 10.31399/asm.hb.v22b.9781627081979
EISBN: 978-1-62708-197-9
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005294
EISBN: 978-1-62708-187-0
..., calcium, cerium or other rare earths, magnesium, strontium, titanium, and zirconium. The silicon in the alloys does not cause significant chill reduction unless added to a level that markedly increases the CE. Because ferrosilicon dissolves readily, it helps to distribute the reactive elements uniformly...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006329
EISBN: 978-1-62708-179-5
... steel scrap, cast iron scrap, foundry returns, ferrosilicon, and carbon. Pig iron is rarely used because of cost, although it does offer advantages in terms of purity. The type of scrap employed will depend on economics. The elimination of coke from the charge also reduces the sulfur absorbed by the...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001049
EISBN: 978-1-62708-161-0
... , p 347 – 356 10.7449/1984/Superalloys_1984_347_356 Appendix: P/M Cobalt-Base Wear-Resistant Materials 1. Fritzlen G.A. and Elbaum J.K. , Cobalt-Chromium-Tungsten-Molybdenum Wear-Resistant Alloys , in Vol 1 , 8th ed. , Metals Handbook , American Society for Metals , 1961...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003005
EISBN: 978-1-62708-200-6
... materials, including ferrous alloys, nonferrous alloys, ceramics, cermets and cemented carbides, engineering plastics, polymer-matrix composites, metal-matrix composites, ceramic-matrix and carbon-carbon composites, and reviews their general property characteristics and applications. It describes the...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001304
EISBN: 978-1-62708-170-2
..., hot-dip coating processes, electrogalvanizing, electroplating, metal cladding, organic coatings, zinc-rich coatings, porcelain enameling, thermal spraying, hardfacing, vapor-deposited coatings, surface modification, and surface hardening via heat treatment. alloy steel cadmium plating carbon...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006375
EISBN: 978-1-62708-192-4
... properties as adhesion, friction, and wear—and contaminant layers can greatly reduce adhesion and friction and, accordingly, provide lubrication. Because contaminants are weakly bound to the surface, physically rather than chemically, they can be removed by bombarding them with rare gas ions (e.g., argon...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006521
EISBN: 978-1-62708-207-5
... 0273RE95, National Center for Manufacturing Sciences , 1995 35. Hinton B.R.W. , Ryan N.E. , Arnott D.R. , Trathen P.N. , Wilson L. , and Williams B.E. , The inhibition of aluminium alloy corrosion by rare earth metal cations , Corrosion Australas , 10 , No. 3...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006787
EISBN: 978-1-62708-295-2
...-generation plants (coal, oil, natural gas, and nuclear), pulp and paper mills, waste-incineration sites, numerous industrial chemical processes, diesel engines (power, land vehicle, and maritime), and gas turbine (land-based, marine shipboard, and aircraft). Predicting corrosion of metals and alloys or...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002473
EISBN: 978-1-62708-194-8
... Mar-M-211 73.46 11.60 102.19 −269.76 360.82 2 9.0 5.0 0 2.5 5.0 2.7 2.0 0.1 10.0 … 9.5 Range 5–25.5 0–8 0–9 0–9 0–12 0–5 0–5.5 0–1 … … 6.50–13 (a) Ni = balance. (b) Rare exceptions out of the typical composition range. Source: Ref 18...