Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005247
EISBN: 978-1-62708-187-0
... Abstract Primary silicon in hypereutectic aluminum-silicon alloys is very hard, not only imparting improved wear resistance but also decreasing tool life during machining. This article discusses the importance of primary silicon refinement and the process of accomplishing primary silicon...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005301
EISBN: 978-1-62708-187-0
... Abstract This article focuses on aspects that are important for the commercial production of castings. It discusses the modification process in hypoeutectic and eutectic alloys that differ only in the relative volume fraction of primary aluminum and aluminum-silicon eutectic. The article...
Image
Published: 27 April 2016
Fig. 6 Properties of aluminum-silicon alloys. Source: Ref 3 as published in Ref 2 More
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005212
EISBN: 978-1-62708-187-0
..., at higher cooling rates, the system behaves as though the eutectic point is shifted to higher silicon contents, and the eutectic temperature is depressed. Figure 2 illustrates the effect of this apparent shift in the eutectic point on the microstructure of a typical aluminum-silicon alloy. Figure 2...
Image
Published: 31 December 2017
Fig. 15 Influence of silicon content on wear resistance of aluminum-silicon alloy. Source: Ref 135 More
Image
Published: 15 June 2019
Fig. 7 Influence of silicon content on wear resistance of aluminum-silicon alloy. Source: Ref 24 More
Image
Published: 01 January 2002
Fig. 52 Torsion fracture in an aluminum-silicon alloy (alloy 319-T5). Classic brittle torsion fracture on a plane at 45° to the axis of the cylinder. Hardness, 38 HRB; tensile strength, 179 MPa (26 ksi); total elongation, 0.5%. Source: Ref 42 More
Image
Published: 01 January 2002
Fig. 53 Macroscale brittle torsion fracture in an aluminum-silicon alloy (alloy A356 sand casting). Hardness, 38 HRB; tensile strength, 214 MPa (31 ksi); total elongation, 4%. Source: Ref 42 More
Image
Published: 15 January 2021
Fig. 52 Torsion fracture in an aluminum-silicon alloy (alloy 319-T5). Classic brittle torsion fracture on a plane at 45° to the axis of the cylinder. Hardness, 38 HRB; tensile strength, 179 MPa (26 ksi); total elongation, 0.5%. Source: Ref 43 More
Image
Published: 15 January 2021
Fig. 53 Macroscale brittle torsion fracture in an aluminum-silicon alloy (alloy A356 sand casting). Hardness, 38 HRB; tensile strength, 214 MPa (31 ksi); total elongation, 4%. Source: Ref 43 More
Image
Published: 01 January 2002
Fig. 17 Microvoid coalescence in an aluminum-silicon alloy (A380) loaded in tension. (a) Fracture surfaces consist of cleaved particles (i.e., silicon) and ridged fracture of the aluminum. 200×. (b) Higher-magnification (1440×) view of boxed region. (c) A fractured aluminum ligament surrounded More
Image
Published: 01 December 2008
Fig. 6 Microstructure of an aluminum-silicon alloy modified with strontium. (a) At low magnification. (b) At higher magnification and deeply etched. Source: Ref 20 More
Image
Published: 01 December 2008
Fig. 9 Microstructure of an aluminum-silicon alloy. (a) Unmodified. (b) Modified with strontium. Source: Ref 33 More
Image
Published: 01 December 2004
Fig. 3 Cast aluminum-silicon alloy. Etchant: 60% HCl, 30% HNO 3 , 5%HF, 5%H 2 O More
Image
Published: 01 December 2004
Fig. 26 Microstructure of a cast aluminum-silicon alloy depicting well-developed dendritic structure. The dendrite arm spacing (DAS) is the mean center-to-center distance between the dendrite arms. More
Image
Published: 01 December 2004
Fig. 10 As-cast morphologies in a eutectic aluminum-silicon alloy. (a) Unmodified alloy with coarse silicon precipitates formed during solidification. (b) Modified alloy with solidification of finer silicon precipitates. Both etched with 0.5% HF (5m in Table 4 ) and magnified by 750× More
Image
Published: 01 December 2004
Fig. 44 Micrographs of porosity in a cast aluminum-silicon alloy. (a) Gaseous porosity. 100×. (b) Dispersed shrinkage porosity. 50×. (c) Cluster of shrinkage pores. 50×. Source: Ref 38 More
Image
Published: 31 December 2017
Fig. 6 Microstructure of hypereutectic aluminum-silicon alloy with eutectic and primary silicon particles More
Image
Published: 15 January 2021
Fig. 17 Microvoid coalescence in an aluminum-silicon alloy (A380) loaded in tension. (a) Fracture surfaces consist of cleaved particles (i.e., silicon) and ridged fracture of the aluminum. Original magnification: 200×. (b) Higher-magnification (1440×) view of boxed region. (c) Fractured More
Image
Published: 01 June 2016
Fig. 49 Magnesium effects on heat treated aluminum-silicon alloy (Al-10Si with magnesium) More