EISBN: 978-1-62708-210-5
... aging characteristics for aluminum alloy 296.0-T6, permanent mold. Source: Ref 4 Abstract Abstract Alloy 296.0 is an aluminum permanent-mold casting alloy with higher silicon than 295.0, which reduces shrinkage and improves fluidity. This datasheet provides information on key alloy metallurgy...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006513
EISBN: 978-1-62708-207-5
...Abstract Abstract Aluminum casting in steel and iron permanent molds is used widely throughout industry, and the vast majority of permanent mold castings are made of aluminum and its alloys. There are several methods used to cast aluminum in permanent molds. This article focuses on permanent...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003128
EISBN: 978-1-62708-199-3
... mechanical properties of aluminum permanent mold casting alloys based on tests of separately cast specimens Table 4 Typical mechanical properties of aluminum permanent mold casting alloys based on tests of separately cast specimens Aluminum Association No. Temper Tensile strength Tensile yield...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0009021
EISBN: 978-1-62708-187-0
... of casting were blended smoothly. No defects occurred at this spot. Permanent mold casting of aluminum alloy 355 Fig. 23 This aluminum casting is representative of the maximum capabilities of the permanent mold process for the wall thickness indicated. Fig. 21 In this aluminum permanent...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003127
EISBN: 978-1-62708-199-3
...Cross-reference chart of frequently used specifications for aluminum alloy sand and permanent mold (PM) castings Table 1 Cross-reference chart of frequently used specifications for aluminum alloy sand and permanent mold (PM) castings Alloy Federal ASTM (a) SAE (b) AMS or MIL-21180c...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006524
EISBN: 978-1-62708-207-5
...Relative characteristics of aluminum alloys used in sand, permanent mold, and die casting Table 2 Relative characteristics of aluminum alloys used in sand, permanent mold, and die casting Rating scheme: 1, best; 5, worst. Individual alloys may have different ratings for other casting...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001061
EISBN: 978-1-62708-162-7
...Factors affecting selection of casting process for aluminum alloys Table 7 Factors affecting selection of casting process for aluminum alloys Factor Casting process Sand casting Permanent mold casting Die casting Cost of equipment Lowest cost if only a few items required Less...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0009023
EISBN: 978-1-62708-187-0
... a beneficial freezing pattern in this sand cast steel lever. Fig. 10 Padding this aluminum permanent mold casting facilitated efficient foundry production. Fig. 11 Uniform walls of this permanent mold cast aluminum piston (a) resulted in simultaneous freezing, which caused porosity...
Book Chapter

Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005287
EISBN: 978-1-62708-187-0
..., 2008 Comparison of sand casting, die casting, and permanent mold casting processes for aluminum alloys Table 4 Comparison of sand casting, die casting, and permanent mold casting processes for aluminum alloys Factor Casting process Sand casting Permanent mold casting Die casting...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006488
EISBN: 978-1-62708-207-5
... in a mold by various casting methods. Virtually every casting method that can be used with unreinforced aluminum has been used with DRA composites. These include the sand, gravity die (permanent mold), investment, squeeze, and lost foam casting processes as well as high-pressure die casting. A semisolid...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006548
EISBN: 978-1-62708-210-5
...Abstract Abstract This article aims to comprehensively review and summarize the material properties and engineering data for aluminum alloy castings and their many applications. The discussion focuses on conventional sand, permanent mold, and die castings as well as the premium engineered...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003175
EISBN: 978-1-62708-199-3
...; P, permanent mold casting; D, die casting. (b) All compositions contain balance of aluminum. Fig. 7 Schematics showing (a) the directional solidification process and (b) the single-crystal solidification process for casting of superalloys Fig. 1 Solubility of hydrogen...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005260
EISBN: 978-1-62708-187-0
...Recommended permanent mold materials for aluminum Table 1 Recommended permanent mold materials for aluminum Casting size Number of pours 1,000 10,000 100,000 Small castings 25 mm (1 in.) max dimension Gray iron (a) Gray iron (a) Gray iron with H 14 inserts, H 11, H 13...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005332
EISBN: 978-1-62708-187-0
..., and cavitation. Aluminum bronzes are used in permanent mold casting in addition to sand casting, because aluminum improves the fluidity of the liquid and enables complex shapes to be produced. Zinc has a relatively wide range of solubility in copper in the solid state, whereby compositions containing up...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0009014
EISBN: 978-1-62708-187-0
...Abstract Abstract This article discusses issues that impact a good casting design. The focus is on the casting design in general, and on sand and permanent mold aluminum casting in particular. The article examines the casting design process from a variety of design and processing perspectives...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006590
EISBN: 978-1-62708-210-5
... aluminum casting rotating-beam fatigue curve. Comparison of smooth specimens from two lots, T5 and T101 temper Fig. 2 852.0-T5, permanent-mold aluminum casting rotating-beam fatigue curve. Smooth and notched specimens from two lots Abstract Abstract The aluminum-tin alloys 850.0, 851.0...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006587
EISBN: 978-1-62708-210-5
... ksi MPa ksi 79 175 235 34 210 30.5 3 120 250 205 29.5 175 25 2 175 350 135 19.5 115 17 6 Fig. 1 C712.0-F, permanent mold aluminum casting rotating-beam fatigue curve. Smooth and notched specimens from one lot. Source: Ref 1 Abstract Abstract...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006588
EISBN: 978-1-62708-210-5
..., no notch 16.3 J (12 ft · lbf) 27 J (20 ft · lbf) Abstract Abstract Alloy 713.0 is an aluminum-based casting alloy that ages at room temperature to provide high-strength sand and permanent-mold castings. This datasheet provides information on key alloy metallurgy, processing effects on physical...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005261
EISBN: 978-1-62708-187-0
... Structural Components , SAE 2001-01-0411 8. Arnold T.F. , “Vacuum Permanent Mold Casting,” Aluminum Company of America, Permanent Mold Castings Division 9. VRC/PRC Offers Squeeze Casting Properties at Permanent Mold Costs (Case History: Vacuum Riserless Casting and Pressure Riserless...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006580
EISBN: 978-1-62708-210-5
... to corrosion; increasing iron and magnesium tends to lower ductility. For sand and permanent-mold cast alloys, high copper, iron, or nickel decreasing ductility and resistance to corrosion. Increasing magnesium reduces ductility. Alloy 443.0 typical physical properties Table 2 Alloy 443.0 typical...