1-20 of 29

Search Results for aluminum alloys A380.0

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006575
EISBN: 978-1-62708-210-5
... Abstract The aluminum alloys 380.0, A380.0, and B380.0 are widely used for making general-purpose die castings. This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, fabrication characteristics, and application characteristics...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002184
EISBN: 978-1-62708-188-7
... Abstract This article begins with a discussion on the classification of aluminum alloys and the selection of alloy and temper based on machinability. It provides an overview of cutting force and power, tool design and material, and general machining conditions. In addition, the article...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006625
EISBN: 978-1-62708-210-5
... Abstract This article contains a table that lists the values of nominal compositions and composition limits of aluminum alloy castings. alloy nominal composition aluminum alloy castings The compositions in this table are based on industry handbooks, notably The Aluminum...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003128
EISBN: 978-1-62708-199-3
... 1 3 4 3 … 380.0 2 1 2 5 3 4 … A380.0 2 2 2 4 3 4 … 384.0 2 2 1 3 3 4 … 390.0 2 2 2 2 4 2 … 413.0 1 2 1 2 4 4 … C443.0 2 3 3 2 5 4 … 515.0 4 5 5 1 2 4 … 518.0 5 5 5 1 1 4 … 1, best; 5, worst. Individual alloys...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001062
EISBN: 978-1-62708-162-7
... Abstract This article is a compilation of property data for standard grades of cast aluminum alloys. Data are provided for mechanical, thermal, and electrical properties. The listing for each alloy includes commercial names, chemical compositions, applications, relevant specifications...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001061
EISBN: 978-1-62708-162-7
... Abstract Aluminum casting alloys are the most versatile of all common foundry alloys and generally have the highest castability ratings. This article discusses the designation and classification of aluminum casting alloys based on their composition and the factors influencing alloy selection...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006548
EISBN: 978-1-62708-210-5
... 4 3 1 4 851.0 4 4 4 4 3 1 4 852.0 4 4 4 4 3 1 4 Die casting alloys 360.0 1 1 2 2 3 4 … A360.0 1 1 2 2 3 4 … 364.0 2 2 1 3 4 3 … 380.0 2 1 2 5 3 4 … A380.0 2 2 2 4 3 4 … 384.0 2 2 1 3 3 4 … 390.0 2 2 2 2 4...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003223
EISBN: 978-1-62708-199-3
... Zn Bumper bars, bumper reinforcements, headrest bars (extruded), seat track Casting alloys 319.0 5.5–6.5 Si Manifolds, cylinder heads, blocks, internal engine parts, pistons 356.0 6.5–7.5 Si Cylinder heads, manifolds A356.0 6.5–7.5 Si Wheels A380.0 7.5–9.5 Si Blocks...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006553
EISBN: 978-1-62708-210-5
... Abstract This article summarizes some general alloy groupings by application or major characteristics. The groupings include cast rotor, general-purpose, elevated-temperature, wear-resistant, moderate-strength, high-strength, and high-integrity die casting alloys and cast aluminum alloys...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005331
EISBN: 978-1-62708-187-0
..., and A413.1 ingot is used to produce 360.0 and A360.0, 380.0 and A380.0, 413.0 and A413.0 castings, respectively. (e) 0.15 max Sb, 0.15 max Pb. (f) 0.08–0.15 V. (g) 0.10 max Pb. (h) 0.003–0.007 Be, 0.005 max B. (i) Used for centrifugally cast products. (j) Reactivation date of alloy...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006524
EISBN: 978-1-62708-207-5
... date of alloy designation. (h) If iron exceeds 0.45, manganese content shall not be less than one-half the iron content. (i) 0.04–0.07 Be. (j) 0.002 max Be. (k) 0.10–0.30 Be. (l) A360.1, A380.1, and A413.1 ingot is used to produce 360.0 and A360.0, 380.0 and A380.0, and 413.0...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003127
EISBN: 978-1-62708-199-3
..., gear cases, and cylinder heads for air-cooled engines Alloy A380.0 Streetlamp housings, typewriter frames, and dental equipment Alloy 360.0 Frying skillets, cover plates, instrument cases, and parts requiring corrosion resistance Alloy 413.0 Outboard motor parts such as pistons, connecting...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003123
EISBN: 978-1-62708-199-3
... Abstract More than 450 alloy designations/compositions have been registered by the Aluminum Association (AA) Inc. for aluminum and aluminum alloys. This article contains tables that list the designations and composition limits of wrought unalloyed aluminum and wrought aluminum alloys...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006251
EISBN: 978-1-62708-169-6
... of the alloys can be produced from a wide variety of casting processes, commercial die castings are limited to a relatively small number of compositions, namely, 360.0, A360.0, 380.0, A380.0, 383.0, 384.0, A384.0, B390.0, 413.0, C443.0, and 518.0. Nominal composition of aluminum alloy castings Table 3...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006482
EISBN: 978-1-62708-207-5
..., commercial die castings are limited to a relatively small number of compositions, namely, 360.0, A360.0, 380.0, A380.0, 383.0, 384.0, A384.0, B390.0, 413.0, C443.0, and 518.0. Nominal composition of aluminum alloy castings Table 3 Nominal composition of aluminum alloy castings Alloy Nominal...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006496
EISBN: 978-1-62708-207-5
... Abstract Castability is a complex characteristic that depends on both the intrinsic fluid properties of the molten metal and the manner in which the particular alloy solidifies. This article discusses the practical aspects of solidification important to aluminum foundrymen. The primary focus...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003130
EISBN: 978-1-62708-199-3
... Abstract This article discusses the corrosion resistance of aluminum and aluminum alloys in various environments, such as in natural atmospheres, fresh waters, seawater, and soils, and when exposed to chemicals and their solutions and foods. It describes the forms of corrosion of aluminum...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003121
EISBN: 978-1-62708-199-3
... Abstract Aluminum and its alloys are used in a broad range of applications. This article discusses the primary and secondary production of aluminum and the classification system for cast and wrought products. It describes some of the more common manufactured forms, including commercial wrought...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003192
EISBN: 978-1-62708-199-3
... steels, wrought Cast irons—gray, ductile, and malleable Aluminum alloys, wrought and cast Titanium alloys, wrought Nickel-base, high-temperature alloys, wrought and cast. Turning, free-machining low-carbon steels, wrought Table 1 Turning, free-machining low-carbon steels, wrought...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006507
EISBN: 978-1-62708-207-5
... Abstract The strength of aluminum castings can be improved significantly by heat treatments, which control the size, shape, and distribution of the impurity elements in the casting. This article presents a discussion on the heat treatment of aluminum alloy castings, with a focus...