1-20 of 49 Search Results for

aluminum alloy C355.0

Sort by
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006567
EISBN: 978-1-62708-210-5
..., and application characteristics of these 3xxx series alloys. aluminum alloy 355.0 aluminum alloy C355.0 fabrication characteristics heat treatment high-strength alloys mechanical properties physical properties Used in sand and permanent mold (PM) casting, alloys 355.0 and C355.0 ( Table 1...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006691
EISBN: 978-1-62708-210-5
... A357.0 7.0 … … 0.58 … 0.12 bal 0.55 Be 557–613 1035–1135 (a) Includes AWS designation for brazing fillers, as applicable. (b) Wrought alloy with composition identical to cast alloy C355.0. (c) Wrought alloy with composition identical to cast alloy A356.0. (d) Wrought alloy...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003128
EISBN: 978-1-62708-199-3
... and elevated-temperature aluminum casting alloys. It provides a list of the creep-rupture properties and fatigue strengths of separately sand cast test bars of alloy 201.0, alloy C355.0-T61, alloy A356.0-T61, and alloy 354.0-T61. alloy 201.0 alloy 354.0-T61 alloy A356.0-T61 alloy C355.0-T61 aluminum...
Image
Published: 01 January 1990
Fig. 13 Comparison of (a) notch yield ratio and (b) unit propagation energy versus yield strength for various aluminum alloy premium-quality castings and wrought aluminum alloy plate. 1, XA201.0-T7; 2, 249.0-T7; 3, 224.0-T7; 4, C355.0-T6; 5, 354.0-T6; 6, A356.0-T6; 7, 356.0-T6; 8, A357.0-T6 More
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006553
EISBN: 978-1-62708-210-5
... A356.0 trailer suspension saddle Aluminum-silicon-copper-magnesium alloys such as 328.0. 333.0, 354.0, 355.0, and C355.0 offer excellent strength and hardness with some sacrifice in ductility and corrosion resistance. Casting characteristics are good but inferior to those displayed by copper-free...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006548
EISBN: 978-1-62708-210-5
... by copper-free aluminum-silicon alloys. Properties in the as-cast condition can be acceptable for some applications, but these alloys are typically heat treated for optimum properties. Alloy C355.0 with low iron is a higher-strength version of 355.0. Alloys of this type are routinely cast in sand...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003127
EISBN: 978-1-62708-199-3
... castings are very high because of the fine microstructure and the capability for heat treatment. Some common aluminum permanent mold casting alloys, and typical products cast from them, are presented in the following table: Alloy 336.0 Automotive pistons Alloys 355.0, C355.0, A357.0 Timing...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006623
EISBN: 978-1-62708-210-5
... 319.0, 333.0, 354.0, 355.0, C355.0, 380.0 with alloy 2 as: 1060, 1350 4043 B A A A A A 4145 A A B A A A 1100 4043 B A A A A A 4145 A A B A A A 2014, 2036 2319 B A A A A A 4043 C C B C A A 4145 A B C B A A 2219 2319 B...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001061
EISBN: 978-1-62708-162-7
... Abstract Aluminum casting alloys are the most versatile of all common foundry alloys and generally have the highest castability ratings. This article discusses the designation and classification of aluminum casting alloys based on their composition and the factors influencing alloy selection...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006251
EISBN: 978-1-62708-169-6
... Abstract The most widely accepted alloy and temper designation system for aluminum and its alloys is maintained by the Aluminum Association and recognized by the American National Standards Institute (ANSI) as the American National Standard Alloy and Temper Designation Systems for Aluminum...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006482
EISBN: 978-1-62708-207-5
... Abstract Commercial aluminum alloys are classified based on how they are made and what they contain. This article describes the ANSI H35.1 designation system, which is widely used to classify wrought and cast aluminum alloys. The ANSI standard uses a four-digit numbering system to identify...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002184
EISBN: 978-1-62708-188-7
... Abstract This article begins with a discussion on the classification of aluminum alloys and the selection of alloy and temper based on machinability. It provides an overview of cutting force and power, tool design and material, and general machining conditions. In addition, the article...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001436
EISBN: 978-1-62708-173-3
... Aluminum alloys Acceptable filler alloys Wrought Cast 1 xxx series … Base alloy, 1100, 1188, 4043, 4047 2014, 2219 222.0, 295.0, 319.0, 333.0 2319, 4043, 4145 3003, 5005, 5050 … 1100, 4043, 4047 5052, 5454, 6061, 6063, 7005 … 4043, 4047, 5554 … 354.0, 355.0, C355.0 4009...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006566
EISBN: 978-1-62708-210-5
... process, the alloy has less surface shrinkage than C355.0. Heat Treatment Solution treatment : Soak at 525 °C (980 °F) for 10–12 h; quench in hot water. Temperature of water has been specified at 60–80 °C (140–175 °F) ( Ref 2 ) or at 65–100 °C (150–212 °F) ( Ref 3 ). T6 Aging : from...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001417
EISBN: 978-1-62708-173-3
... … … … 3.5 0.25 0.10 … C355.0 5.0 1.25 … 0.5 … … … A356.0 7.0 … … 0.4 … … … 357.0 7.0 … … 0.5 … … … A357.0 7.0 … … 0.6 … 0.12 … Source: Ref 42 Filler alloys recommended for welding selected aluminum-base alloys to minimize sensitivity to weld cracking...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006625
EISBN: 978-1-62708-210-5
... Abstract This article contains a table that lists the values of nominal compositions and composition limits of aluminum alloy castings. alloy nominal composition aluminum alloy castings The compositions in this table are based on industry handbooks, notably The Aluminum...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006510
EISBN: 978-1-62708-207-5
... … … 0.35 … … bal … 557–613 1035–1135 A357.0 7.0 … … 0.58 … 0.12 bal 0.55 Be 557–613 1035–1135 (a) Wrought alloy with composition identical to cast alloy C355.0. (b) Wrought alloy with composition identical to cast alloy A356.0. (c) Wrought alloy with composition identical...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006569
EISBN: 978-1-62708-210-5
... premium casting of A210.0, A206.0, 224.0, 249.0, 354.0, C355.0, A356.0, D357.0, 358.0, and 359.0. Fabrication Characteristics Fabrication characteristics are similar to alloy 356.0. Like alloy 356.0, it is possible to produce a variety of strength levels by adjustment of magnesium and heat...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003130
EISBN: 978-1-62708-199-3
... Abstract This article discusses the corrosion resistance of aluminum and aluminum alloys in various environments, such as in natural atmospheres, fresh waters, seawater, and soils, and when exposed to chemicals and their solutions and foods. It describes the forms of corrosion of aluminum...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006555
EISBN: 978-1-62708-210-5
... Abstract The 206.0, A206.0, and B206.0 alloys (aluminum alloys 2xxx) are structural castings in the heat-treated temper for automotive and aerospace applications where high tensile and yield strengths with moderate elongations are needed. This datasheet provides information on key alloy...