1-20 of 28 Search Results for

aluminum alloy B443.0

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006580
EISBN: 978-1-62708-210-5
... characteristics of these alloys. aluminum alloy 443.0 aluminum alloy A443.0 aluminum alloy B443.0 aluminum alloy C443.0 aluminum-silicon hypoeutectic casting alloys fabrication characteristics mechanical properties physical properties The 443 series of aluminum casting alloys have nominal...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002184
EISBN: 978-1-62708-188-7
..., B295.0, 308.0, 319.0, 328.0, A332.0, F332.0, 333.0, 354.0, 355.0, C355.0, 356.0, A356.0, 357.0, 359.0, B443.0, 514.0, A514.0, B514.0, 520.0, 535.0, 705.0, 707.0, A712.0, D712.0, 713.0, 771.0, 850.0, A850.0, B850.0, Hiduminium RR-350 40–100 As-cast 200 (650) 0.004–0.006 (0.00015–0.00025) 0.008–0.013...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006548
EISBN: 978-1-62708-210-5
... 391.0 19.0 … … … 0.58 … … … … bal A391.0 19.0 … … … 0.58 … … … … bal B391.0 19.0 … … … 0.58 … … … … bal 413.0 12.0 … … … … … … … … bal A413.0 12.0 … … … … … … … … bal 443.0 5.2 … … … … … … … … bal B443.0 5.2...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001062
EISBN: 978-1-62708-162-7
... Abstract This article is a compilation of property data for standard grades of cast aluminum alloys. Data are provided for mechanical, thermal, and electrical properties. The listing for each alloy includes commercial names, chemical compositions, applications, relevant specifications...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003127
EISBN: 978-1-62708-199-3
..., A357.0 Timing gears, impellers, compressors, and aircraft and missile components requiring high strength Alloys 356.0, A356.0 Machine tool parts, aircraft wheels, pump parts, marine hardware, valve bodies Alloy B443.0 Carburetor bodies, waffle irons Alloy 513.0 Ornamental hardware...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006625
EISBN: 978-1-62708-210-5
... … 0.25 bal 443.0 Nominal 5.2 … … … … … … … … … … … … Limits 4.5–6.0 0.8 0.6 0.50 0.05 0.25 … 0.50 0.25 … … 0.35 bal B443.0 Nominal 5.2 … … … … … … … … … … … … Limits 4.5–6.0 0.8 0.15 0.35 0.05 … … 0.35 0.25 … 0.05 0.15 bal C443.0...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006251
EISBN: 978-1-62708-169-6
... … … … … … … … … … A413.0 12.0 … … … … … … … … … 443.0 5.2 … … … … … … … … … B443.0 5.2 … … … … … … … … … C443.0 5.2 … … … … … … … … … A444.0 7.0 … … … … … … … … … 512.0 1.8 … … … 4.0 … … … … … 513.0 … … … … 4.0 … … 1.8 … … 514.0...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006482
EISBN: 978-1-62708-207-5
... … A390.0-T7 36 36 <1.0 115 … … … 443.0-F 19 8 8 40 14 8 10.3 B443.0-F 17 6 3 25–55 … … … A444.0-F 21 9 9 30–60 … … … A444.0-T4 23 9 12 43 … … … 511.0-F 21 12 3 50 17 8 … 512.0-F 20 13 2 50 17 9 … 514.0-F 25 12 9 50 20 7...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003128
EISBN: 978-1-62708-199-3
... A357.0 (b) … … … … … 359.0 (b) … … … … … 443.0 F 117 17.0 48 7.0 3.0 B443.0 F 117 17.0 41 6.0 3.0 514.0 F 152 22.0 62 9.0 6.0 520.0 T4 290 42.0 152 22.0 12.0 535.0 F or T5 241 35.0 124 18.0 9.0 705.0 F or T5 207 30.0 117 17.0 5.0...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003123
EISBN: 978-1-62708-199-3
... … … 0.10 0.20 … 0.05 0.15 bal A443.0 43(0.30 max Cu) S 4.5–6.0 0.8 0.30 0.50 0.05 0.25 … 0.50 0.25 … … 0.35 bal A443.1 43(0.30 max Cu) Ingot 4.5–6.0 0.6 0.30 0.50 0.05 0.25 … 0.50 0.25 … … 0.35 bal B443.0 43(0.15 max Cu) S, P 4.5–6.0 0.8 0.15 0.35 0.05...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003130
EISBN: 978-1-62708-199-3
... 332.0 T5 C B 336.0 T551, T65 C B 354.0 T61, T62 C A 355.0 All C A C355.0 T61 C A 356.0 All B A A356.0 T61 B A F356.0 All B A A357.0 T61 B A 358.0 T6 B A 359.0 All B A B443.0 F B A A444.0 T4 B A 513.0 F A A 705.0 T5 B...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006496
EISBN: 978-1-62708-207-5
... 1015–1095 380 540–595 1000–1100 A380.0 540–595 1000–1100 383 515–580 960–1080 384 515–580 960–1080 390 … … B390.0 510–650 950–1200 392 550–670 1020–1240 413 575–580 1065–1080 A413.0 575–580 1065–1080 443 575–630 1065–1170 B443.0 575–630 1065–1170...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003175
EISBN: 978-1-62708-199-3
... … 0.35 0.35 max 7.0 … A357.0 S, P … 0.60 0.03 max 7.0 0.15Ti, 0.04Be 360.0 D … 0.50 0.35 max 9.5 … 380.0 D 3.5 … 0.50 max 8.5 … 390.0 D 4.5 0.60 0.10 max 17.0 … 413.0 D … … 0.35 max 12.0 … B443.0 S, P … … 0.50 max 5.2 … (a) S, sand casting...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001061
EISBN: 978-1-62708-162-7
... 322 4210 C355.0 C355 … C355 … SC51B 355 C355 (c) 356.0 356 356 356 SG70A SG70A 323 (d) A356.0 A356 … A356 … SG70B 336 A356 (c) 357.0 357 … 357 … … … 4241 A357.0 A357 … … … … … A357 (c) 359.0 359 … … … … … 359 (c) B443.0 43 43 43...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006507
EISBN: 978-1-62708-207-5
... … … … 0.58 … … … … … B391.0 S 19.0 … … … 0.58 … … … … … 413.0 D 12.0 … … … … … … … … … A413.0 D 12.0 … … … … … … … … … 443.0 S, P 5.2 … … … … … … … … … B443.0 S, P 5.2 … … … … … … … … … C443.0 D 5.2...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006264
EISBN: 978-1-62708-169-6
... 12.0 … … … … … … … … … A413.0 D 12.0 … … … … … … … … … 443.0 S, P 5.2 … … … … … … … … … B443.0 S, P 5.2 … … … … … … … … … C443.0 D 5.2 … … … … … … … … … A444.0 P 7.0 … … … … … … … … … 512.0 S 1.8 … … … 4.0...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006545
EISBN: 978-1-62708-210-5
... 319.0 F C B T6 C C 332.0 T5 C B 336.0 T551, T65 C B 354.0 T61, T62 C A 355.0 All C A C355.0 T61 C A 356.0 All B A A356.0 T61 B A F356.0 All B A A357.0 T61 B A 358.0 T6 B A 359.0 All B A B443.0 F B A A444.0 T4 B...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001058
EISBN: 978-1-62708-162-7
... Abstract A four-digit numerical designation system is used to identify wrought aluminum and aluminum alloys. In addition to providing a detailed account of the temper designation system for aluminum and aluminum alloys, this article describes wrought and cast aluminum and aluminum alloy...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006510
EISBN: 978-1-62708-207-5
... Abstract Weldability is a function of three major factors: base material quality, welding process, and design. This article focuses on base-metal weldability of aluminum alloys in terms of mechanical property degradation in both the weld region and heat-affected zone, weld porosity...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006513
EISBN: 978-1-62708-207-5
...-temperature strength. 443.0, B443.0 Used where high ductility and/or corrosion resistance are required, but not high strength, such as waffle irons and carburetor bodies. 513.0 Al-Mg alloy with about 2% Zn, which makes it more adaptable to permanent mold casting. It can be used for simple casting...