Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006564
EISBN: 978-1-62708-210-5
..., fabrication characteristics, and application characteristics of these 3xxx series alloys. age-hardenable permanent mold casting alloys aluminum alloy 333.0 aluminum alloy A333.0 fabrication characteristics high-temperature applications mechanical properties physical properties pressure tightness...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003123
EISBN: 978-1-62708-199-3
... Ingot 8.5–10.0 0.6 2.0–4.0 0.10 0.9–1.3 … 0.10 0.10 0.20 … … 0.30 bal 333.0 333 P 8.0–10.0 1.0 3.0–4.0 0.50 0.05–0.50 … 0.50 1.0 0.25 … … 0.50 bal 333.1 333 Ingot 8.0–10.0 0.8 3.0–4.0 0.50 0.10–0.50 … 0.50 1.0 0.25 … … 0.50 bal A333.0 … P 8.0–10.0...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001058
EISBN: 978-1-62708-162-7
... … 0.25 … 0.50 rem 333.1 A03331 … Ingot 8.0–10.0 0.8 3.0–4.0 0.50 0.10–0.50 … 0.50 1.0 … 0.25 … 0.50 rem A333.0 A13330 … P 8.0–10.0 1.0 3.0–4.0 0.50 0.05–0.50 … 0.50 3.0 … 0.25 … 0.50 rem A333.1 A13331 … Ingot 8.0–10.0 0.8 3.0–4.0 0.50 0.10–0.50 … 0.50...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006513
EISBN: 978-1-62708-207-5
... and 333) 322.0 Nickel-free, high-silicon alloy with higher copper used extensively in the manufacture of automotive pistons, but has been replaced by alloy 336 and hypereutectic 390-type alloys. 333.0, A333.0 Have good casting characteristics in permanent molds and develop somewhat better as-cast...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006524
EISBN: 978-1-62708-207-5
... 2.0–4.0 0.50 0.50–1.5 … 0.50 1.0 0.25 … … 0.50 333.0 P 8.0–10.0 1.0 3.0–4.0 0.50 0.05–0.50 … 0.50 1.0 0.25 … … 0.50 A333.0 P 8.0–10.0 1.0 3.0–4.0 0.50 0.05–0.50 … 0.50 3.0 0.25 … … 0.50 336.0 P 11.0–13.0 1.2 0.5–1.5 0.35 0.7–1.3 … 2.0–3.0 0.35 0.25...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005331
EISBN: 978-1-62708-187-0
... 1.0 1.0–2.0 0.20–0.6 0.20–0.6 0.35 0.25 1.5 0.25 … … … 0.50 332.0 P 8.5–10.5 1.2 2.0–4.0 0.50 0.50–1.5 … 0.50 1.0 0.25 … … … 0.50 333.0 P 8.0–10.0 1.0 3.0–4.0 0.50 0.05–0.50 … 0.50 1.0 0.25 … … … 0.50 A333.0 P 8.0–10.0 1.0 3.0–4.0 0.50 0.05–0.50...