1-8 of 8 Search Results for

aluminum alloy 7085

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006739
EISBN: 978-1-62708-210-5
...Specified minimum strength properties (S- or A-basis) of aluminum alloy 7085-T7451 plate Table 2 Specified minimum strength properties (S- or A-basis) of aluminum alloy 7085-T7451 plate Thickness, mm (in.) Direction 7085-T7451 (AMS 4470) F ty (A), MPa (ksi) F tu (A), MPa (ksi...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006594
EISBN: 978-1-62708-210-5
...Alloying (wt%) of traditional and modern aluminum-lithium alloys Table 1 Alloying (wt%) of traditional and modern aluminum-lithium alloys Alloy Cu Mg Li Ag Status, date registered Density, g/cm 3 (lb/in. 3 ) Low Cu, high Mg, high Li alloys 8090 1.0–1.6 0.6–1.3 2.2–2.7...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006726
EISBN: 978-1-62708-210-5
...Fracture toughness values for select 2<italic>xxx</italic> and 7<italic>xxx</italic> aluminum alloys Table 1 Fracture toughness values for select 2 xxx and 7 xxx aluminum alloys Material Product form Thickness range, mm (in.) Fracture toughness ( K Ic ), MPa √m (ksi √in.) L-T T...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003996
EISBN: 978-1-62708-185-6
...- to intermediate-strength aluminum alloys, such as 1100 and 6061, flow stresses are lower than those of carbon steel. For high-strength alloys—particularly 7 xxx series alloys such as 7 x 75, 7010, 7040, 7 x 49, 7050, 7085, and others—flow stresses, and therefore forging pressures, are considerably higher than...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006516
EISBN: 978-1-62708-210-5
...Abstract Abstract The development of aluminum alloys has progressed along two tracks: heat treatable and non-heat treatable. The Aluminum Association alloy composition limits and product temper are defined for major alloying elements. This article summarizes the historical evolution...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006493
EISBN: 978-1-62708-207-5
.... For some low- to intermediate-strength aluminum alloys, such as 1100 and 6061, flow stresses are lower than those of carbon steel. For high-strength alloys—particularly 7 xxx -series alloys such as 7 x 75, 7010, 7040, 7 x 49, 7050, 7085, and others—flow stresses, and therefore forging pressures...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006543
EISBN: 978-1-62708-210-5
...Nominal compositions for wrought aluminum alloys Table 1 Nominal compositions for wrought aluminum alloys Alloy UNS No. Composition (a) , % Al min (b) , % Notes Si Fe Cu Mn Mg Cr Ni Zn Ti 1050 A91050 … … … … … … … … … 99.50 … 1060 A91060...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006624
EISBN: 978-1-62708-210-5
... limits for wrought aluminum alloys Notes to the nominal compositions and composition limits for wrought aluminum alloys Indicator Definition (a) Both nominal compositions and composition limits are shown. Nominal values are midrange of limits for elements for which a composition range...