Book Chapter

Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006713
EISBN: 978-1-62708-210-5
... Abstract This datasheet provides information on composition limits, heat treatment, processing effects on physical and mechanical properties, and applications of free-machining aluminum alloys 6033, 6040 and 6041. aluminum alloy 6033 aluminum alloy 6040 aluminum alloy 6041 chemical...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006516
EISBN: 978-1-62708-210-5
... Abstract The development of aluminum alloys has progressed along two tracks: heat treatable and non-heat treatable. The Aluminum Association alloy composition limits and product temper are defined for major alloying elements. This article summarizes the historical evolution of the different...
Book Chapter

By Michael E. Finn
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006494
EISBN: 978-1-62708-207-5
... bodies, end caps, valves, and fittings), transmission valves, flashlight casings, fishing reels, braked pistons, and rifle scopes. Alloy AA 6033 was introduced by Kaiser Aluminum in 2002 as a nonleaded free-machining aluminum alloy with significantly higher strength compared to AA 6061 and AA 6262...
Series: ASM Handbook
Volume: 24A
Publisher: ASM International
Published: 30 June 2023
DOI: 10.31399/asm.hb.v24A.a0006983
EISBN: 978-1-62708-439-0
... the optimized material for an application but because they were available in the supply chain ( Ref 1 ). The list of materials available greatly expanded afterward and now includes a variety of materials from all the major alloy families: Nickel-base superalloys Aluminum-base alloys Copper-base...
Series: ASM Handbook
Volume: 24A
Publisher: ASM International
Published: 30 June 2023
DOI: 10.31399/asm.hb.v24A.9781627084390
EISBN: 978-1-62708-439-0