1-20 of 36 Search Results for

aluminum alloy 6013

Sort by
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006711
EISBN: 978-1-62708-210-5
.... aluminum alloy 6013 extruded automotive bumpers fabrication characteristics fracture properties high-strength aluminum-magnesium-silicon-copper alloys physical properties static properties tensile properties Alloy 6013 ( Table 1 ) is a high-strength Al-Mg-Si-Cu alloy, initially developed...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006490
EISBN: 978-1-62708-207-5
... in conjunction with motion used for the welding path. Shown in Table 1 are parameters that were established for conventional LBW and LSW for producing butt, lap, fillet, and lap-fillet joints on 3.0 mm (0.12 in.) thick alloy 6013-T4. A neodymium: yttrium-aluminum-garnet (Nd:YAG) laser at a power of 4.5 kW...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006715
EISBN: 978-1-62708-210-5
... of this 6xxx series alloy. It provides a material performance comparison of aluminum alloys 6056-T6511 with 2024-T3511 and 6056-T8511 with 2024-T3511. aluminum alloy 6056 aluminum extrusion alloys aluminum sheet alloys chemical composition corrosion resistance mechanical properties tensile...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006516
EISBN: 978-1-62708-210-5
... Abstract The development of aluminum alloys has progressed along two tracks: heat treatable and non-heat treatable. The Aluminum Association alloy composition limits and product temper are defined for major alloying elements. This article summarizes the historical evolution of the different...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006718
EISBN: 978-1-62708-210-5
... properties. The alloy contains somewhat higher Mg and higher Cr compared with alloy 6013, and it contains an intentional 0.10% V addition. Alloy 6069 is produced as rod and bar with the goal of producing an unrecrystallized microstructure to boost strength. Composition limits of aluminum alloy 6069...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006708
EISBN: 978-1-62708-210-5
... Abstract The 6xxx series aluminum alloys are used across end applications including all forms of transportation, electronics, and building and construction. This article contains tables that list standard specifications for 6xxx series aluminum alloys and select specialty mill products...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003618
EISBN: 978-1-62708-182-5
..., Japan), Japan Institute of Light Metals , 1998 , p 1657 14. Burleigh T.D. , Microscopic Investigation of the Intergranular Corrosion of Alloy 6013- T6 , The Third International Conf. on Aluminum Alloys (Trondheim, Norway), Arnberg L. et al. , Ed., 1992 , p 435 15...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001417
EISBN: 978-1-62708-173-3
... Abstract Aluminum alloys, particularly the heat-treatable alloys, are sensitive to weld cracking. Anticipation of these characteristics and general knowledge of these materials assist in selection of suitable method for welding heat-treatable aluminum alloys. This article provides a general...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006520
EISBN: 978-1-62708-207-5
... Abstract This article summarizes a typical solution and aging heat treatments of 2xxx (Al-Cu), 6xxx (Al-Mg-Si), and 7xxx (Al-Zn-Mg) wrought alloys. It discusses the general aging characteristics and the effects of reheating of aluminum alloys. Typical examples of hardness and conductivity...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006287
EISBN: 978-1-62708-169-6
... found in commercial aluminum alloys are shown in Table 4 . Typical dispersoids in aluminum alloys Table 4 Typical dispersoids in aluminum alloys Alloy Dispersoid 2 x 24 Al 20 Cu 2 Mn 3 5083 Al 11 Cr 2 , Al 6 (Fe,Mn) 6013 Al 12 Mn 3 Si 7046 Al 3 Zr 7 x 75 Al 12 Mg 2...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006500
EISBN: 978-1-62708-207-5
... and the practical aspects of heat generation. The article provides information on the effect of welding on material properties and typical alloys in FSW applications. The alloys include 6061 aluminum, 5083 aluminum, 2xxx aluminum, and 7xxx aluminum alloys. The article concludes with a discussion on FSW equipment...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003163
EISBN: 978-1-62708-199-3
... has focused on aluminum as the matrix metal. The combination of light weight, environmental resistance, and useful mechanical properties has made aluminum alloys very popular; these properties also make aluminum well suited for use as a matrix metal. The melting point of aluminum is high enough...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006288
EISBN: 978-1-62708-169-6
... Abstract This article focuses on the aging characteristics of solution and precipitation heat treated aluminum alloy systems and their corresponding types. It includes information on aluminum-copper systems, aluminum-copper-magnesium systems, aluminum-magnesium-silicon systems, aluminum-zinc...
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005808
EISBN: 978-1-62708-165-8
... destruction causes a low mechanical quality, cracks, porosity, and a very short life of the component. Laser cladding can provide a permanent structural repair and refurbishment on many alloys (e.g., aluminum alloys) that are generally considered unweldable by conventional methods. The success of laser...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006510
EISBN: 978-1-62708-207-5
... Abstract Weldability is a function of three major factors: base material quality, welding process, and design. This article focuses on base-metal weldability of aluminum alloys in terms of mechanical property degradation in both the weld region and heat-affected zone, weld porosity...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003485
EISBN: 978-1-62708-195-5
.../17.5p. The 6092 aluminum matrix alloy is a modified 6 xxx age-hardenable aluminum alloy that was optimized to be used as a matrix alloy for DRA. This alloy has been approved by the Aluminum Association and is the DRA matrix analog to 6013. Design trade studies and material and process development were...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003123
EISBN: 978-1-62708-199-3
... Abstract More than 450 alloy designations/compositions have been registered by the Aluminum Association (AA) Inc. for aluminum and aluminum alloys. This article contains tables that list the designations and composition limits of wrought unalloyed aluminum and wrought aluminum alloys...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001436
EISBN: 978-1-62708-173-3
... Abstract Aluminum and its alloys can be joined by as many or more methods than any other metal. This article discusses the properties of aluminum, namely hydrogen solubility, electrical conductivity, and thermal characteristics. It analyses the primary factors commonly considered when selecting...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003681
EISBN: 978-1-62708-182-5
...-20Cr alloy developed a complete, protective Cr 2 O 3 scale more rapidly when implanted with cerium, yttrium, calcium, or aluminum, but implanted zirconium or chromium had no effect. Scale adherence was increased by ion implantation with cerium, yttrium, calcium, or zirconium. For yttrium- implanted Ni...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006626
EISBN: 978-1-62708-210-5
... Abstract This article contains tables that list typical room-temperature physical properties of wrought aluminum alloys in engineering units and metric units. engineering units metric units physical properties wrought aluminum alloys PHYSICAL PROPERTIES in engineering units...