Skip Nav Destination
Close Modal
By
C.E. Cross, M.L. Kohn
By
John Weritz
By
Wojciech Z. Misiolek, Richard M. Kelly
By
John Weritz, S. Lampman
By
R.J. Bucci, G. Nordmark, E.A. Starke, Jr.
Search Results for
aluminum alloy 5454
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 60
Search Results for aluminum alloy 5454
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Book Chapter
5454 High-Strength Al-Mg-Mn-Cr Alloy
Available to PurchaseSeries: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006702
EISBN: 978-1-62708-210-5
... properties, and fabrication characteristics of this 5xxx series alloy. aluminum alloy 5454 aluminum-magnesium-manganese-chromium solid solution alloys chemical and process industries chemical handling fabrication characteristics mechanical properties physical properties The composition...
Abstract
Alloy 5454 is an Al-Mg-Mn-Cr solid solution alloy with relatively high strength used for handling chemicals at elevated temperatures in the chemical and process industries. This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, and fabrication characteristics of this 5xxx series alloy.
Book Chapter
Aluminum Filler Metal Selection Charts
Available to PurchaseSeries: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006623
EISBN: 978-1-62708-210-5
... Abstract This article provides a comprehensive matrix for selecting an aluminum filler alloy for the gas tungsten arc and gas metal arc welding processes, based on the various requirements or service conditions. A table lists the nominal strengths of aluminum filler metals. aluminum...
Abstract
This article provides a comprehensive matrix for selecting an aluminum filler alloy for the gas tungsten arc and gas metal arc welding processes, based on the various requirements or service conditions. A table lists the nominal strengths of aluminum filler metals.
Book Chapter
4043 Welding Filler Metal
Available to PurchaseSeries: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006691
EISBN: 978-1-62708-210-5
... Abstract The aluminum alloy 4043 is recommended as a filler metal when resistance to salt water corrosion is required, especially when welding such aluminum alloys as 5052, 6061, and 6063. This datasheet provides information on key alloy metallurgy, and processing effects on tensile properties...
Abstract
The aluminum alloy 4043 is recommended as a filler metal when resistance to salt water corrosion is required, especially when welding such aluminum alloys as 5052, 6061, and 6063. This datasheet provides information on key alloy metallurgy, and processing effects on tensile properties of this 4xxx series alloy.
Book Chapter
5754 Al-3.1Mg Alloy
Available to PurchaseSeries: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006706
EISBN: 978-1-62708-210-5
... Abstract This datasheet provides information on key alloy metallurgy and processing effects on physical and mechanical properties of Al-3.1Mg alloy 5754. aluminum-magnesium alloy 5754 mechanical properties physical properties Alloy 5754 ( Table 1 ) is closely related to the alloys...
Abstract
This datasheet provides information on key alloy metallurgy and processing effects on physical and mechanical properties of Al-3.1Mg alloy 5754.
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001436
EISBN: 978-1-62708-173-3
... Aluminum alloys Acceptable filler alloys Wrought Cast 1 xxx series … Base alloy, 1100, 1188, 4043, 4047 2014, 2219 222.0, 295.0, 319.0, 333.0 2319, 4043, 4145 3003, 5005, 5050 … 1100, 4043, 4047 5052, 5454, 6061, 6063, 7005 … 4043, 4047, 5554 … 354.0, 355.0, C355.0 4009...
Abstract
Aluminum and its alloys can be joined by as many or more methods than any other metal. This article discusses the properties of aluminum, namely hydrogen solubility, electrical conductivity, and thermal characteristics. It analyses the primary factors commonly considered when selecting a welding filler alloy. These include ease of welding or freedom from cracking, tensile or shear strength of the weld, weld ductility, service temperature, corrosion resistance, and color match between the weld and base alloy after anodizing. The article provides a detailed description of gas-shielded arc welding processes for welding of aluminum alloys and also reviews other welding processes such as oxyfuel gas welding and laser-beam welding.
Book Chapter
Properties of Wrought Aluminum Alloys
Available to PurchaseSeries: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003126
EISBN: 978-1-62708-199-3
... Abstract This article is a comprehensive collection of property data for wrought aluminum and aluminum alloys. Data are provided for the physical properties and mechanical properties of wrought aluminum and aluminum alloys. The listing also includes values that indicate the effect...
Abstract
This article is a comprehensive collection of property data for wrought aluminum and aluminum alloys. Data are provided for the physical properties and mechanical properties of wrought aluminum and aluminum alloys. The listing also includes values that indicate the effect of temperatures on tensile strength, yield strength, and elongation, and the mechanical properly limits for aluminum alloy die forgings, non-heat-treatable and heat-treatable aluminum alloy sheets and plates, and non-heat-treatable aluminum alloy extruded wires, rods, bars, and shapes.
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001059
EISBN: 978-1-62708-162-7
... treatments are used to control certain properties and characteristics of the worked, or wrought, product or alloy. This article discusses the designation system, classification, product forms, corrosion and fabrication characteristics, and applications of wrought aluminum alloys. Commercial wrought aluminum...
Abstract
Aluminum mill products are those that have been subjected to plastic deformation by hot- and cold-working mill processes such as rolling, extruding, and drawing, either singly or in combination. Microstructural changes associated with the working and with any accompanying thermal treatments are used to control certain properties and characteristics of the worked, or wrought, product or alloy. This article discusses the designation system, classification, product forms, corrosion and fabrication characteristics, and applications of wrought aluminum alloys. Commercial wrought aluminum products are divided into flat-rolled products (sheet, plate, and foil); rod, bar, and wire; tubular products; shapes; and forgings. The article discusses factors affecting the strengthening mechanisms, fracture toughness, and physical properties of aluminum alloys, in addition to the effects of alloying on the physical and mechanical properties. Important alloying elements and impurities are listed alphabetically as a concise review of major effects.
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006510
EISBN: 978-1-62708-207-5
... Abstract Weldability is a function of three major factors: base material quality, welding process, and design. This article focuses on base-metal weldability of aluminum alloys in terms of mechanical property degradation in both the weld region and heat-affected zone, weld porosity...
Abstract
Weldability is a function of three major factors: base material quality, welding process, and design. This article focuses on base-metal weldability of aluminum alloys in terms of mechanical property degradation in both the weld region and heat-affected zone, weld porosity, and susceptibility to solidification cracking and liquation cracking. It provides an overview on welding processes, including gas metal arc welding, gas tungsten arc welding, resistance spot and seam welding, laser beam welding, and various solid-state welding processes. A review on joint design is also included, mainly in the general factors associated with service weldability (fitness). The article also provides a discussion on the selection and weldability of non-heat-treatable aluminum alloys, heat treatable aluminum alloys, aluminum-lithium alloys, and aluminum metal-matrix composites.
Book Chapter
Selection and Weldability of Non-Heat-Treatable Aluminum Alloys
Available to PurchaseSeries: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001418
EISBN: 978-1-62708-173-3
... Abstract Non-heat-treatable aluminum alloys constitute a group of alloys that rely solely upon cold work and solid solution strengthening for their strength properties. This article focuses on the weldability and weld properties of different classes on non-heat-treatable aluminum alloys...
Abstract
Non-heat-treatable aluminum alloys constitute a group of alloys that rely solely upon cold work and solid solution strengthening for their strength properties. This article focuses on the weldability and weld properties of different classes on non-heat-treatable aluminum alloys.
Book Chapter
5254 Higher-Purity Al-Mg-Cr Alloy
Available to PurchaseSeries: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006701
EISBN: 978-1-62708-210-5
.... aluminum alloy 5254 fabrication characteristics heat exchangers higher-purity aluminum-magnesium-chromium alloys mechanical properties physical properties pumps steam-jacketed kettles Alloy 5254, introduced in 1951 for welded chemical tanks and gas cylinders, has a slightly higher purity level...
Abstract
Alloy 5254 is a higher-purity Al-Mg-Cr alloy used in heat exchangers, steam-jacketed kettles, and pumps. This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, and fabrication characteristics of this 5xxx series alloy.
Book Chapter
Machining of Aluminum and Aluminum Alloys
Available to PurchaseBook: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002184
EISBN: 978-1-62708-188-7
... Abstract This article begins with a discussion on the classification of aluminum alloys and the selection of alloy and temper based on machinability. It provides an overview of cutting force and power, tool design and material, and general machining conditions. In addition, the article...
Abstract
This article begins with a discussion on the classification of aluminum alloys and the selection of alloy and temper based on machinability. It provides an overview of cutting force and power, tool design and material, and general machining conditions. In addition, the article discusses distortion and dimensional variation and machining problems during the machining of high-silicon aluminum alloy. It also provides information on tool design and material, speed and feed, and the cutting fluid used for various machining processes, namely, turning, boring, planing and shaping, broaching, reaming, tapping, milling, sawing, grinding, honing, and lapping. The article concludes with a discussion on drilling operations in automatic bar and chucking machines and drill presses.
Book Chapter
Introduction to Mechanical Testing of Components
Available to PurchaseSeries: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003321
EISBN: 978-1-62708-176-4
... 1 ) for selected steels and aluminum alloys, respectively, for monotonic loads. Tables 1 and 2 also list cyclic stress-strain properties, as described later. General properties related to monotonic stress-strain behavior are described briefly here. Monotonic and cyclic stress-strain properties...
Abstract
This article describes the tests for the common types of fabricated components and modeling of metal deformation. It provides an overview of component testing and briefly reviews the relationship of mechanical properties in the process of mechanical design for static loads, cyclic loads, dynamic loads, and high-temperature materials. The article describes the general properties related to monotonic stress-strain behavior of steels. It also discusses materials properties and operating stresses as well as other factors, such as part shape and environmental effects, which play significant roles in the design process of components.
Book Chapter
Aluminum Alloy Nomenclature and Temper Designations
Available to PurchaseSeries: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006251
EISBN: 978-1-62708-169-6
... Abstract The most widely accepted alloy and temper designation system for aluminum and its alloys is maintained by the Aluminum Association and recognized by the American National Standards Institute (ANSI) as the American National Standard Alloy and Temper Designation Systems for Aluminum...
Abstract
The most widely accepted alloy and temper designation system for aluminum and its alloys is maintained by the Aluminum Association and recognized by the American National Standards Institute (ANSI) as the American National Standard Alloy and Temper Designation Systems for Aluminum (ANSI H35.1). This article provides a detailed discussion on the alloy and temper designation system for aluminum and its alloys. The Aluminum Association alloy designations are grouped as wrought and cast alloys. Lengthy tables provide information on alloying elements in wrought aluminum and aluminum alloys; nominal composition of aluminum alloy castings; typical mechanical properties of wrought and cast aluminum alloys in various temper conditions; and cross references to former and current cast aluminum alloy designations.
Book Chapter
Aluminum Alloy Nomenclature and Temper Designations
Available to PurchaseSeries: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006482
EISBN: 978-1-62708-207-5
... Abstract Commercial aluminum alloys are classified based on how they are made and what they contain. This article describes the ANSI H35.1 designation system, which is widely used to classify wrought and cast aluminum alloys. The ANSI standard uses a four-digit numbering system to identify...
Abstract
Commercial aluminum alloys are classified based on how they are made and what they contain. This article describes the ANSI H35.1 designation system, which is widely used to classify wrought and cast aluminum alloys. The ANSI standard uses a four-digit numbering system to identify alloying elements, compositional modifications, purity levels, and product types. It also uses a multicharacter code to convey process-related details on heat treating, hardening, cooling, cold working, and other stabilization treatments. The article includes several large tables that provide extensive information on aluminum alloy and temper designations and how they correspond to critical mechanical properties as well as other designation systems.
Book Chapter
Extrusion of Aluminum Alloys
Available to PurchaseSeries: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004015
EISBN: 978-1-62708-185-6
... Abstract Aluminum and aluminum alloys are very suitable for extrusion and many types of profiles can be produced from easily extrudable alloys. This article lists the basic characteristics of aluminum and its alloys. It tabulates the aluminum extrusion alloys by series and lists the typical...
Abstract
Aluminum and aluminum alloys are very suitable for extrusion and many types of profiles can be produced from easily extrudable alloys. This article lists the basic characteristics of aluminum and its alloys. It tabulates the aluminum extrusion alloys by series and lists the typical applications for 6xxx series aluminum extrusions. The article discusses three broad categories of extrusion profiles: solid profile, hollow profile, and semi hollow profile. It provides information on weldability and machinability, which are often considered in profile design and product performance. The article discusses different aluminum extrusion processes, such as the direct extrusion process and the indirect extrusion process. It schematically illustrates the plotting of flow stress and extrudability for several types of aluminum alloys. The article concludes with information on the heat treatment and precipitation hardening for alloys, such as 2xxx, 6xxx, and 7xxx.
Book Chapter
Wrought Aluminum Processes and Products
Available to PurchaseSeries: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006518
EISBN: 978-1-62708-207-5
... the various product forms in which commonly used wrought aluminum alloys are available. The article also provides design guidelines for aluminum extrusions and discusses various forming methods. aluminum wrought products extrusions forgings forming wrought aluminum alloys ALUMINUM wrought...
Abstract
This article introduces the basic characteristics, processes, and product forms associated with the five major categories of aluminum wrought products, namely, flat-rolled products (sheet, plate, and foil); rod, bar, and wire; tubular products; profiles; and forgings. It summarizes the various product forms in which commonly used wrought aluminum alloys are available. The article also provides design guidelines for aluminum extrusions and discusses various forming methods.
Book Chapter
Aluminum Wrought Products
Available to PurchaseSeries: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003125
EISBN: 978-1-62708-199-3
... Abstract This article discusses the classification, characteristics and temper designations of wrought aluminum alloys. Wrought aluminum products are available as flat-rolled products such as sheets, plates, and foils; rods, bars, and wires; tubular products such as tubes and pipes; extruded...
Abstract
This article discusses the classification, characteristics and temper designations of wrought aluminum alloys. Wrought aluminum products are available as flat-rolled products such as sheets, plates, and foils; rods, bars, and wires; tubular products such as tubes and pipes; extruded shapes; forgings; and impacts. The article provides information on product economics, design and selection, including product dimension and dimension tolerances, and design and use of wrought product capabilities. Finally, it tabulates the specifications and standards for aluminum mill products.
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006486
EISBN: 978-1-62708-210-5
... equipment, for example, a shear or brake press. Nominal strengths of some wrought aluminum products used in structural design Table 2 Nominal strengths of some wrought aluminum products used in structural design Alloy Temper ASTM specification, product Thickness mm Thickness in. Tensile...
Abstract
Aluminum wrought products, castings, welds, and fasteners are used in many structural applications where they are required to safely support a load. It is useful to design aluminum structural components with its structural properties in mind from conceptualization rather than attempting to mimic components of other materials. This article discusses design specifications, design requirements and methods, and material properties used in aluminum structural design. These properties include tensile yield strength and tensile ultimate strength, welding, and ductility. The article describes various factors that affect the strength of two categories of aluminum structural components, namely members and connections. Design requirements for aluminum bolts, rivets, screws, and pins are provided. The article concludes with a discussion on the considerations for serviceability, namely deflections and vibrations.
Book
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.9781627082105
EISBN: 978-1-62708-210-5
Book Chapter
Selecting Aluminum Alloys to Resist Failure by Fracture Mechanisms
Available to PurchaseBook: Fatigue and Fracture
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002406
EISBN: 978-1-62708-193-1
... Abstract This article provides an overview of fatigue and fracture resistance of aluminum alloys. It discusses the characteristics of aluminum alloy classes and the fracture mechanics of aluminum alloys. The article tabulates relative stress-corrosion cracking ratings for high-strength wrought...
Abstract
This article provides an overview of fatigue and fracture resistance of aluminum alloys. It discusses the characteristics of aluminum alloy classes and the fracture mechanics of aluminum alloys. The article tabulates relative stress-corrosion cracking ratings for high-strength wrought aluminum products. It analyzes the selection of various alloys for stress-corrosion cracking resistance, including aluminum-lithium alloys, copper-free 7XXX alloys, and casting alloys. The article presents a list of typical tensile properties and fatigue limit of aluminum alloys. It also describes the effects of composition, microstructure, thermal treatments, and processing in fatigue crack growth of aluminum alloys.