EISBN: 978-1-62708-210-5
... and critical applications requiring premium-quality castings. Toughness and strength are not as good as alloy 206.0 ( Fig. 2 ), but the alloys provide high strength with fairly good ductility ( Tables 7 and 8 ). Aluminum 357.0 exhibits good general corrosion resistance under ordinary atmospheric, marine...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006568
EISBN: 978-1-62708-210-5
... type test Tensile properties of representative squeeze-cast aluminum alloy castings Table 4 Tensile properties of representative squeeze-cast aluminum alloy castings Alloy Temper Casting process Tensile strength Yield strength, 0.2 % offset Elongation in 50 mm (2 in.) or 4D...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006251
EISBN: 978-1-62708-169-6
...Typical mechanical properties (in customary units) of wrought aluminum alloys in various temper conditions Table 4 Typical mechanical properties (in customary units) of wrought aluminum alloys in various temper conditions Alloy and temper (a) Tension Hardness, Brinell No., 500 kg load...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006482
EISBN: 978-1-62708-207-5
...Abstract Abstract Commercial aluminum alloys are classified based on how they are made and what they contain. This article describes the ANSI H35.1 designation system, which is widely used to classify wrought and cast aluminum alloys. The ANSI standard uses a four-digit numbering system...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003128
EISBN: 978-1-62708-199-3
...Typical physical properties of aluminum casting alloys Table 1 Typical physical properties of aluminum casting alloys Aluminum Association No. Temper (a) Specific gravity (b) Density (b) Approximate melting range Electrical conductivity, %IACS Thermal conductivity at 25 °C...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002184
EISBN: 978-1-62708-188-7
...Abstract Abstract This article begins with a discussion on the classification of aluminum alloys and the selection of alloy and temper based on machinability. It provides an overview of cutting force and power, tool design and material, and general machining conditions. In addition, the article...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006570
EISBN: 978-1-62708-210-5
... References 1. Lemon R.C. , Howle C.R. , Premium Strength Aluminum Casting Alloys 354 and 359 , Transactions AFS , Vol 70 , 1963 , p 465 – 470 2. Caceres C.H. , Svensson I.L. , and Taylor J.A , Strength-Ductility Behavior of Al-Si-Cu-Mg Casting Alloys in T6 Temper...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006553
EISBN: 978-1-62708-210-5
...Abstract Abstract This article summarizes some general alloy groupings by application or major characteristics. The groupings include cast rotor, general-purpose, elevated-temperature, wear-resistant, moderate-strength, high-strength, and high-integrity die casting alloys and cast aluminum...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001061
EISBN: 978-1-62708-162-7
...Factors affecting selection of casting process for aluminum alloys Table 7 Factors affecting selection of casting process for aluminum alloys Factor Casting process Sand casting Permanent mold casting Die casting Cost of equipment Lowest cost if only a few items required Less...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006548
EISBN: 978-1-62708-210-5
... ) and AMS ( Ref 5 ) specifications are: A201.0-T6 A206.0-T6 224.0-T6 249.0-T6 354.0A through D-T6 356.0A through D-T6 357.0-T6 358.0-T6 359.0-T6 Representative applications of premium engineered aluminum casting alloys include: Aerospace and missile structural...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003127
EISBN: 978-1-62708-199-3
...Cross-reference chart of frequently used specifications for aluminum alloy sand and permanent mold (PM) castings Table 1 Cross-reference chart of frequently used specifications for aluminum alloy sand and permanent mold (PM) castings Alloy Federal ASTM (a) SAE (b) AMS or MIL-21180c...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006625
EISBN: 978-1-62708-210-5
...) Ingot; 1.5 min Fe/Si ratio. (f) Also contains 0.40–1.0% Ag (0.7% nominal). (g) Also contains 0.20–0.30% Sb (0.25% nominal), 0.20–0.30% Co (0.25% nominal), and 0.10–0.30% Zr. Ti + Zr contents = 0.50% max. (h) Alloy has been designated “Inactive” by The Aluminum Association but still occurs...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005331
EISBN: 978-1-62708-187-0
...Abstract Abstract This article begins with a discussion on the effects of alloying and impurity elements on the properties of aluminum cast alloys and their chemical compositions. It describes the various means of structural control, namely, chemistry control, control of element ratios based...
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006573
EISBN: 978-1-62708-210-5
.... With copper limits, the alloys have excellent resistance to corrosion and stress corrosion cracking. Like alloys 356.0 and 357.0, these Al-Si-Mg alloys also are flexible with respect to property variations with adjustments in magnesium alloying and heat treatment. For example, there are five variations...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001417
EISBN: 978-1-62708-173-3
... Casting alloys 242.0 … 4.0 … 1.5 … … 2.0 Ni 319.0 6.0 3.5 … … … … … 355.0 5.0 1.2 … 0.5 … … … 356.0 7.0 … … 0.4 … … … 357.0 7.0 … … 0.6 … … … Source: Ref 3 , 4 , 5 Numerical designations for the heat-treated tempers of aluminum alloys...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006524
EISBN: 978-1-62708-207-5
...Relative characteristics of aluminum alloys used in sand, permanent mold, and die casting Table 2 Relative characteristics of aluminum alloys used in sand, permanent mold, and die casting Rating scheme: 1, best; 5, worst. Individual alloys may have different ratings for other casting...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006529
EISBN: 978-1-62708-207-5
... limiting their brazeability. Not all aluminum alloys can be readily brazed ( Table 1 ). The high-strength, high-magnesium 5 xxx series wrought aluminum alloys, such as 5052, and certain casting alloys (such as Cast 357.0 and 359.0) contain large amounts of alloying elements. These additions, in most...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006507
EISBN: 978-1-62708-207-5
...Abstract Abstract The strength of aluminum castings can be improved significantly by heat treatments, which control the size, shape, and distribution of the impurity elements in the casting. This article presents a discussion on the heat treatment of aluminum alloy castings, with a focus...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006264
EISBN: 978-1-62708-169-6
...Typical heat treatments for aluminum alloy sand and permanent mold castings Table 1 Typical heat treatments for aluminum alloy sand and permanent mold castings Alloy Temper Type of casting (a) Solution heat treatment (b) Aging treatment Temperature (c) Time, h Temperature (c...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002455
EISBN: 978-1-62708-194-8
... consideration of the alternative manufacturing processes. As an example, a hydraulic accumulator piston for an automotive transmission was made from a thermoplastic polymer instead of the more conventional aluminum alloy ( Ref 1 ). Use of the glass-filled linear polyphenylene sulfide (PPS) plastic resulted...