1-6 of 6

Search Results for airless centrifugal vane-type wheels

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001228
EISBN: 978-1-62708-170-2
... Abstract Mechanical cleaning systems are used to remove contaminants of work surface by propelling abrasive materials through any of these three principal methods: airless centrifugal blast blade- or vane-type wheels; compressed air, direct-pressure dry blast nozzle systems; or compressed-air...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003217
EISBN: 978-1-62708-199-3
... Drying equipment for immersion phosphating systems can be of several types. For small parts, such as washers, a centrifuge can be used to spin off moisture. If parts are hot enough, no additional heated air is required. However, if parts are cold, heated air can be introduced into the centrifuge...
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006519
EISBN: 978-1-62708-207-5
... Cleaning Blast cleaning is also used to remove scale resulting from core removal or heat treatment. Both pneumatic and airless (centrifugal) blasting machines are employed. Metallic abrasives (steel or iron grit or shot) and ceramic abrasives (silica sand, aluminum oxide, garnet, and staurolite...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005255
EISBN: 978-1-62708-187-0
... thermal expansion in the solid state, relatively low solidification shrinkage, and good compatibility with a wide range of materials. Still other waxes that have been used are montan wax (both acid and ester types), fatty acid amides, ceresin, stearone, and hydrogenated castor oil. The waxes listed...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001304
EISBN: 978-1-62708-170-2
.... In the vast majority of cases, the particles are propelled in a matrix of air or water to the work surface. The basic means of propelling the blasting material is with either air pressure or a centrifugal wheel. Equipment for blast cleaning and finishing is described in the article “Mechanical Cleaning...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.9781627081993
EISBN: 978-1-62708-199-3