Skip Nav Destination
Close Modal
Search Results for
aerospace plate alloys
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Book Series
Date
Availability
1-20 of 688 Search Results for
aerospace plate alloys
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Book Chapter
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006607
EISBN: 978-1-62708-210-5
... Abstract Alloy 2124, aerospace plate alloy, is a high-purity version of 2024. This datasheet provides information on key alloy metallurgy, fabrication characteristics, processing effects on physical and mechanical properties, and applications of this series alloy. aerospace plate alloys...
Book Chapter
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006600
EISBN: 978-1-62708-210-5
... information on key alloy metallurgy and processing effects on mechanical properties of plate and extrusions of this 2xxx series alloy. aerospace plate alloys aluminum alloy 2027 aluminum-copper-magnesium-manganese-zirconium alloys damage tolerance alloy plates extrusion alloys mechanical properties...
Abstract
Alloy 2027 is an Al-Cu-Mg-Mn-Zr alloy providing improved mechanical properties compared with those of alloy 2024. Alloy 2027-T3511 extrusions are typically used for stringers to stiffen wing skin panels machined from damage tolerant 2xxx alloy plates. This datasheet provides information on key alloy metallurgy and processing effects on mechanical properties of plate and extrusions of this 2xxx series alloy.
Book Chapter
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006746
EISBN: 978-1-62708-210-5
... on Worldwide Metals and Alloys , Data Sheet Al-402, ASM International , Nov 2006 2. Alcan 7449 T7651: Aluminum Aerospace Plate , Alloy Digest: Data on Worldwide Metals and Alloys , Data Sheet Al-406, ASM International , Dec 2007 3. Alcan 7449 T7951: Aluminum Aerospace Plate , Alloy Digest...
Book Chapter
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006734
EISBN: 978-1-62708-210-5
... Abstract Alloy 7055 is widely used in the aerospace industry in applications as plate and extrusions. This datasheet provides information on key alloy metallurgy and processing effects on fracture, mechanical, tensile, and compressive properties of this 7xxx series alloy. aerospace...
Book Chapter
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006606
EISBN: 978-1-62708-210-5
.... aluminum alloy 2099 aluminum-copper-lithium alloys elastic modulus extrusions fatigue crack growth resistance high-strength alloys mechanical strength plates Alloy 2099 ( Table 1 ) is a third-generation Al-Cu–Li alloy introduced in 2003 to provide an improved combination of strength, elastic...
Book Chapter
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006598
EISBN: 978-1-62708-210-5
... for 2024 sheet, plate, and round product forms. Figures illustrate the effect of stretching and aging on toughness of the 2024 sheet and the effect of temperature on tensile properties of 1.0 mm thick Alclad 2024-T3 sheet. aging Alclad 2024 aluminum alloy 2024 high-strength aerospace alloys...
Abstract
This datasheet provides information on key alloy metallurgy, mill product specifications, processing effects on physical and mechanical properties, and applications of high-strength aerospace alloys 2024 and Alclad 2024. It contains tables that list values of tensile property limits for 2024 sheet, plate, and round product forms. Figures illustrate the effect of stretching and aging on toughness of the 2024 sheet and the effect of temperature on tensile properties of 1.0 mm thick Alclad 2024-T3 sheet.
Book Chapter
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006739
EISBN: 978-1-62708-210-5
... Abstract This datasheet provides information on composition limits, fabrication characteristics, processing effects on physical and mechanical properties, and application performance of thick plate and forging alloy 7085. It presents the specified minimum strength and fracture properties...
Abstract
This datasheet provides information on composition limits, fabrication characteristics, processing effects on physical and mechanical properties, and application performance of thick plate and forging alloy 7085. It presents the specified minimum strength and fracture properties for plate, die, and hand forgings. The datasheet provides a comparison of the strength, fracture toughness, and fatigue crack growth resistance of alloy 7085 plate with those of the legacy plate alloy 7050. It shows tensile yield and ultimate strength at elevated temperature for various temperatures and exposure times for 7085-T7452 die forgings.
Book: Surface Engineering
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001323
EISBN: 978-1-62708-170-2
...” in this Volume.) Chromate conversion coating is a nonelectrolytic process in which the conversion coating is applied to light metals (aluminum, magnesium, cadmium plate) and alloys for corrosion resistance and/or as a paint base. (See the article “Chromate Conversion Coatings” in this Volume.) To a lesser...
Abstract
This article focuses on alternatives to chromium in both hard chromium plating and chromate conversion coating. These include electroless nickel plating, nickel-tungsten composite electroplating, spray coating applications, and cobalt/molybdenum-base conversion coating. The article discusses the material and process substitutions that can be used to eliminate the use or emissions of chromium in industrial processes. It describes the physical characteristics of each coating, economics, environmental impacts, advantages, and disadvantages of alternative processes.
Book Chapter
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006742
EISBN: 978-1-62708-210-5
... an excellent combination of high strength and corrosion resistance compared with other 7 xxx series aerospace alloys of similar strength. Minimum properties are given in Tables 4 and 5 . Stiffened upper wing panels and lower horizontal-stabilizer panels of alloy 7150-T7751 plate and 7150-T77511...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001063
EISBN: 978-1-62708-162-7
... design requirements The groupings do not imply that aluminum-lithium alloys can be directly substituted for aluminum alloys. See text for discussion. Primary design criteria Aluminum aerospace alloys Aluminum-lithium aerospace alloys Sheet Plate Forgings Extrusions Sheet Plate Forgings...
Abstract
Aluminum-lithium alloys have been developed primarily to reduce the weight of aircraft and aerospace structures. This article commences with a discussion on the physical metallurgy and development of aluminum-lithium alloys. It focuses on major commercial aluminum-lithium alloys, including alloy 2090, alloy 2091, alloy 8090, alloy CP276, and Weldalite 049. The article also lists the chemical compositions, physical properties, fabrication characteristics, corrosion performance, and general applications of these alloys. A comparison of alloy properties is represented graphically.
Book Chapter
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006744
EISBN: 978-1-62708-210-5
... Abstract This datasheet provides information on composition limits for aluminum alloy 7255, with emphasis on the minimum static properties of aluminum alloy 7255 plate and fracture toughness of aluminum alloy 7255-T7751. Fatigue crack growth resistance of alloy 7255 plate is compared with those...
Abstract
This datasheet provides information on composition limits for aluminum alloy 7255, with emphasis on the minimum static properties of aluminum alloy 7255 plate and fracture toughness of aluminum alloy 7255-T7751. Fatigue crack growth resistance of alloy 7255 plate is compared with those of legacy alloy 7055 plate.
Book Chapter
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006594
EISBN: 978-1-62708-210-5
... procedures. Groupings of select aerospace alloys and temper conditions according to primary design requirements Table 2 Groupings of select aerospace alloys and temper conditions according to primary design requirements Primary design criteria Sheet Plate Forgings Extrusions High...
Book Chapter
Series: ASM Handbook
Volume: 2B
Publisher: ASM International
Published: 15 June 2019
DOI: 10.31399/asm.hb.v02b.a0006740
EISBN: 978-1-62708-210-5
... effects on mechanical properties of alloy 7097-T7651 plate. aluminum alloy 7097 aluminum alloy plates aluminum-magnesium-zinc-copper-zirconium alloys corrosion resistance fracture toughness mechanical strength thick structural applications Alloy 7097 ( Table 1 ) from Kaiser Aluminum...
Abstract
Alloy 7097 is a quench insensitive Al-Mg-Zn-Cu-Zr alloy engineered for the most advantageous combination of strength, corrosion resistance, and fracture toughness in thick structural applications. This datasheet provides information on