EISBN: 978-1-62708-195-5
... Abstract This article highlights the selected applications of advanced polymer-matrix composites, metal-matrix composites, and ceramic matrix composites. advanced polymer-matrix composites metal-matrix composites ceramic matrix composites APPLICATIONS of advanced composite...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003480
EISBN: 978-1-62708-195-5
... Abstract This article presents an overview of advanced composites, namely, polymer matrix composites, metal-matrix composites, ceramic-matrix composites, and carbon-matrix composites. It also provides information on the properties and applications of the composites in thermal management...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003372
EISBN: 978-1-62708-195-5
... Abstract This article focuses on the process methods and matrix chemistries of ceramic-matrix composites. These methods include pressure-assisted densification, chemical vapor infiltration, melt infiltration, polymer infiltration and pyrolysis, and sol-gel processing. The article discusses...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0009084
EISBN: 978-1-62708-177-1
... matrix. Composite materials having polymeric matrices are susceptible to degradation from heat, sunlight, ozone, atomic oxygen (in space), moisture, solvents (chemicals), fatigue, excessive loading, and combinations of these environmental conditions ( Ref 1 ). The rate and extent of degradation...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006478
EISBN: 978-1-62708-190-0
... Abstract This article introduces the principal methodologies and some advanced technologies that are being applied for nondestructive evaluation (NDE) of fiber-reinforced polymer-matrix composites. These include acoustic emission, ultrasonic, eddy-current, computed tomography, electromagnetic...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003465
EISBN: 978-1-62708-195-5
... provides an overview of the composite failure modes affected by matrix resin and testing approach. differential scanning calorimetry dynamic mechanical analysis mechanical failure modes polymer composite thermomechanical analysis FAILURE OF A COMPOSITE STRUCTURE can be caused by several...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003471
EISBN: 978-1-62708-195-5
..., and thermal processes. Thermoplastic-matrix composites are recycled by regrinding, compounding/blending and reprocessing. The article concludes with discussion on the properties of recycled composite fibers. blending industrial waste disposal polymer-matrix composites recycling regrinding...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003368
EISBN: 978-1-62708-195-5
... Composites bv. (b) Cytec Fiberite Advanced Composites Properties of glass reinforced thermoplastic-matrix composites (unidirectional S2-glass tape reinforcement) Table 4 Properties of glass reinforced thermoplastic-matrix composites (unidirectional S2-glass tape reinforcement) Properties...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003063
EISBN: 978-1-62708-200-6
...-temperature applications CERAMIC-MATRIX COMPOSITES (CMCs), one of the newest segments of the advanced materials family, are being developed for a number of high-temperature and high-performance applications in industrial, aerospace, and energy conservation sectors. Government and corporate laboratories...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003572
EISBN: 978-1-62708-180-1
..., aspect ratio, distribution, orientation, combination with fillers, and the quality of bonding with the matrix), and operating conditions. Fibers are far more wear resistant than the matrix and hence control the wear of composite. Continuous fiber-reinforced composites with a thermoset-polymer matrix...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0009071
EISBN: 978-1-62708-177-1
... rods to high-performance airplane parts, the use of fiber-reinforced composite materials is becoming more popular due to their high strength-to-weight ratio combined with easy manufacturing methods. Fiber-reinforced polymeric-matrix composites consist of reinforcing fibers and a polymer resin...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0009080
EISBN: 978-1-62708-177-1
... applications and designs. While there have been advances in fiber technology, the majority of new composite applications over the past few decades have been due to a redesigned balance of matrix properties with an emphasis on improved damage tolerance. First-generation advanced composites were not toughened...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003374
EISBN: 978-1-62708-195-5
... polymeric matrix composites. Research since 1990 has expanded the concept of the fiber-matrix interface, which exists as a two-dimensional boundary, into that of a fiber- matrix interphase that exists in three dimensions ( Ref 2 ). The complexity of this interphase can best be illustrated with the use...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003031
EISBN: 978-1-62708-200-6
...-reinforced composites matrix resins organic matrices polymer-matrix composites reinforcements A COMPOSITE MATERIAL can be defined as a macroscopic combination of two or more distinct materials, having a recognizable interface between them. However, because composites are usually used...
Series: ASM Handbook
Volume: 11B
Publisher: ASM International
Published: 15 May 2022
DOI: 10.31399/asm.hb.v11B.a0006869
EISBN: 978-1-62708-395-9
... and the thermal failure of the polymeric matrix ( Ref 21 ). In general, when SFRPs undergo the wear process, the higher portion of the load is sustained by the fibers. Therefore, the polymeric matrix in the interfacial region around the fibers experiences higher stress and higher temperature, as shown by Fig. 6...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0009082
EISBN: 978-1-62708-177-1
... are commonly developed from carbon or glass fibers combined with a petroleum-based polymeric matrix. In recent years, composites made from renewable resources have received increasing attention due to environmental concerns. Rising petroleum costs and consumption has increased the demand for renewable...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003451
EISBN: 978-1-62708-195-5
... for repair of polymer matrix composites Table 1 Aerospace Material Specifications for repair of polymer matrix composites SpecificationNo. Title Issued AMS 2980 Carbon Fiber Fabric and Epoxy Resin, Wet Lay-up Repair Material Work in progress AMS 2960 Glass Fabric with Epoxy...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003397
EISBN: 978-1-62708-195-5
... components. The list of advanced materials includes particulate and fiber-reinforced polymer, ceramic-matrix composites (CMCs), and metal- matrix composites (MMCs). Adapting the various RP processes for direct fabrication of ceramic materials has received the most effort because, compared to techniques...
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006373
EISBN: 978-1-62708-192-4
... material. Most of the advances in materials have been achieved in polymer-based composites. Frictional Behavior of Polymer Composites Tribological behavior of polymer composites depends on the chain structure of macromolecules of the polymeric matrix and the effect of fillers. Practically all...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003441
EISBN: 978-1-62708-195-5
... dianiline (bis F). Bismaleimide resins cure by means of addition polymerization with little or no evolution of volatiles. They are prime candidates for matrix resins because of their high-temperature resistance, environmental stability under hot/wet conditions, superior smoke/toxicity properties, and epoxy...