1-20 of 348 Search Results for

accuracy

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005239
EISBN: 978-1-62708-187-0
... boundary conditions, physical properties, enmeshing, and evaluation of simulation results. The article provides some insights into the application of models to real world problem for foundry process engineers. accuracy casting physical properties modeling enmeshing simulation code COMPUTER...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005260
EISBN: 978-1-62708-187-0
... of short-term and long-term variables on the dimensional accuracy of permanent mold castings. It concludes with information on the factors of the surface finish on permanent mold castings. mold coatings dimensional accuracy gravity casting methods permanent mold casting mold design mold...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005252
EISBN: 978-1-62708-187-0
... shell molding and green sand molding. casting dimensional accuracy green sand molding shell molding tensile strength mold cracking soft molds peelback mold shift shell coremaking sand reclamation resin-sand properties mold defects mold patterns THE SHELL PROCESS was first...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003971
EISBN: 978-1-62708-185-6
... surface-rolling machines. The article outlines the significant characteristics of pressing-type machines: load and energy characteristics, time-related characteristics, and accuracy characteristics. It summarizes different specialized processes such as advanced roll-forming methods, equal-channel angular...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004035
EISBN: 978-1-62708-185-6
... with tooling-point centers on the exposed faces. Figure 2(c) shows the forged part in place within the inspection fixture. Datum planes and tooling points are chosen early in part layout, before dimensioning. For accuracy, all tooling points are placed on the drawing so that they fall in one die half...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004004
EISBN: 978-1-62708-185-6
... variations obtained in production runs of specific cold-headed products. It concludes with a discussion on the applications of warm heading. bolt makers cold heading cold heading machine cutting to length defects descaling dies dimensional accuracy headers heat treating lubricating machining...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003015
EISBN: 978-1-62708-200-6
... extrusion, chill-roll film extrusion, pipe or tube extrusion, wire and cable coverings, extrusion coating, and profile extrusion, and provides some discussion on multiple-screw extruders. The article describes the dimensional accuracy of extrusion products, and lists common defects that occur frequently in...
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.a0006680
EISBN: 978-1-62708-213-6
... quantifying phase mixtures in powder samples. It provides information on typical sensitivity and experimental limits on precision of XRPD analysis and other systematic sources of errors that affect accuracy. Some of the factors pertinent to the estimation of crystallite size and defects are also presented...
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.a0006638
EISBN: 978-1-62708-213-6
... significance of the raw analytical total. Sections on accuracy of the standards-based k-ratio/matrix corrections protocol with EDS and processes of analysis when severe peak overlap occurs are also included. The article provides information on low-atomic-number elements, iterative qualitative-quantitative...
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.a0006658
EISBN: 978-1-62708-213-6
... information on the factors applicable to the accuracy and precision of AFM measurements. It ends by discussing the applications for AFMs in the fields of science, technology, and engineering. precision atomic force microscopy There are three general types of...
Series: ASM Handbook
Volume: 10
Publisher: ASM International
Published: 15 December 2019
DOI: 10.31399/asm.hb.v10.a0006639
EISBN: 978-1-62708-213-6
... calibration of materials for accurate measurements using XPS are provided, along with some aspects of the accuracy in quantitative analysis by XPS. In addition, the article presents examples of how XPS data can be used to solve problems with surface interactions. chemical composition X-ray...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003974
EISBN: 978-1-62708-185-6
... energy, time-related characteristics, and characteristics for accuracy. Velocity under pressure, V p , is the velocity of the slide under load. This is an important variable because it determines the contact time under...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004027
EISBN: 978-1-62708-185-6
... Abstract The systematic study of microstructural evolution during deformation under hot working conditions is important in controlling processing variables to achieve dimensional accuracy. This article explains the microstructural features that need to be modeled and provides an outline of the...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003986
EISBN: 978-1-62708-185-6
... Abstract Precision forging is defined as a closed-die forging process in which the accuracy of the shape, dimensional tolerances, and surface finish exceed normal expectations to the extent that some of the postforge operations can be eliminated. This article provides an overview of the key...
Series: ASM Handbook
Volume: 4B
Publisher: ASM International
Published: 30 September 2014
DOI: 10.31399/asm.hb.v04b.a0005925
EISBN: 978-1-62708-166-5
... thermometers fall under the noncontact type. The article describes two types of instrumentation used in heat treating: field test instruments for temperature-uniformity surveys and system-accuracy tests; and controlling, monitoring, and recording instruments for digital instrumentation. electrical...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003158
EISBN: 978-1-62708-199-3
... Abstract Thermocouple devices are the most widely used devices for measurement of temperature in the metals industry. Favorable characteristics of these devices include good accuracy, suitability over a wide temperature range, fast thermal response, ruggedness, high reliability, low cost, and...
Series: ASM Handbook
Volume: 17
Publisher: ASM International
Published: 01 August 2018
DOI: 10.31399/asm.hb.v17.a0006447
EISBN: 978-1-62708-190-0
... Abstract Visual inspection (VI) is the oldest inspection technique man has used as a quality-control tool to evaluate products, assess their final form in terms of fabrication accuracy and external features based on experience, and decide on their acceptance or rejection. This article discusses...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005249
EISBN: 978-1-62708-187-0
... Abstract This article discusses slurry molding that encompasses two distinct processes: plaster molding and ceramic molding. Plaster mold casting is a specialized casting process used to produce nonferrous castings that have greater dimensional accuracy, smoother surfaces, and more finely...
Series: ASM Handbook
Volume: 22A
Publisher: ASM International
Published: 01 December 2009
DOI: 10.31399/asm.hb.v22a.a0005438
EISBN: 978-1-62708-196-2
... predict variation in manufacturing for a fixed product must exhibit high accuracy to small changes in process and material input parameters but does not need the ability to extrapolate accurately over large variations of composition or process variables. A model used to design a new alloy for a range of...
Book: Casting
Series: ASM Handbook
Volume: 15
Publisher: ASM International
Published: 01 December 2008
DOI: 10.31399/asm.hb.v15.a0005233
EISBN: 978-1-62708-187-0
... to the governing PDEs. Other examples include turbulence models, combustion models, and multiphase flow models. All models necessarily introduce imprecision, and an ongoing goal of research is to improve the accuracy of these models. Other issues for three-dimensional engineering CFD include geometry...