1-20 of 46 Search Results for

abrasive waterjet machining

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002158
EISBN: 978-1-62708-188-7
... Abstract This article discusses the functions of the major components of a waterjet machining system. These include hydraulic unit, intensifier, accumulator, filters, water transmission lines, on/off valve, waterjet nozzles, abrasive waterjet nozzle, waterjet catchers, and fluid additives...
Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005107
EISBN: 978-1-62708-186-3
... Abstract This article provides a detailed account of the process development, cutting principle, and components of the abrasive waterjet cutting process. The advantages of abrasive waterjet machining are summarized. The article also discusses the factors affecting the cut quality...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002180
EISBN: 978-1-62708-188-7
.... The article describes turning, drilling, tapping, milling, broaching, reaming, and grinding operations on stainless steel. It concludes with information on some of the nontraditional machining techniques, including abrasive jet machining, abrasive waterjet machining electrochemical machining, electron beam...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 November 1995
DOI: 10.31399/asm.hb.emde.a0003055
EISBN: 978-1-62708-200-6
..., honing, and polishing as well as abrasive waterjet, electrical discharge, laser, and ultrasonic machining. References References 1. Ota M. and Miyahara K. , The Influence of Grinding on the Flexural Strength of Ceramics , Proceedings of the Fourth International Grinding Conference...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002155
EISBN: 978-1-62708-188-7
... Thermal Chemical Abrasive jet machining (AJM) Abrasive flow machining (AFM) Waterjet machining (WJM) Abrasive waterjet machining (AWJM) Ultrasonic machining (USM) Electrochemical machining (ECM) Electrochemical grinding (ECG) Electrochemical discharge grinding (ECDG) Electrostream drilling (ES...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003186
EISBN: 978-1-62708-199-3
... Material removal categories of nontraditional machining processes Mechanical Abrasive jet machining (AJM) Abrasive flow machining (AFM) Waterjet machining (WJM) Abrasive waterjet machining (AWJM) Ultrasonic machining (USM) Electrical Electrochemical machining (ECM...
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.9781627081887
EISBN: 978-1-62708-188-7
Series: ASM Handbook
Volume: 2A
Publisher: ASM International
Published: 30 November 2018
DOI: 10.31399/asm.hb.v02a.a0006494
EISBN: 978-1-62708-207-5
... of aluminum alloys. The article lists the inherent disadvantages of machining processes that involve compression/shear chip formation. It discusses the machining of aluminum metal-matrix composites and nontraditional machining of aluminum, such as abrasive jet, waterjet, electrodischarge, plasma arc...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002194
EISBN: 978-1-62708-188-7
.... Waterjet, abrasive waterjet, and laser cutting are among the nontraditional machining methods used. In the waterjet process, a hydraulically driven intensifier pumps a fluid (typically filtered and conditioned water) at pressures up to 410 MPa (60 ksi). The fluid is expelled through an orifice to form...
Book Chapter

By K. Subramanian
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002152
EISBN: 978-1-62708-188-7
..., slurry, and high-pressure waterjet dressing. It concludes with information on the conditioning process of the CBN wheel. abrasive stick abrasive-jet cubic boron nitride abrasives diamond diamond abrasives grinding hard ceramics superabrasives SUPERABRASIVES collectively refer...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002179
EISBN: 978-1-62708-188-7
... traditional machining operations, such as turning, drilling, milling, shaping, thread cutting, and grinding, to the microstructure of standard steel grades. It also explains the technologies in non-traditional machining processes, such as abrasive waterjet cutting, electrical chemical grinding, and laser...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003424
EISBN: 978-1-62708-195-5
... machined surface of carbon/epoxy composite Fig. 4 Typical abrasive waterjet head configuration Fig. 5 Waterjet cutting Fig. 2 Solid carbide end mill with thin film diamond coating Abstract Abstract This article describes the machining operations of carbon fiber...
Series: ASM Handbook
Volume: 5B
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v05b.a0006024
EISBN: 978-1-62708-172-6
... on surface preparation methods that range from simple solvent cleaning to hand and power tool cleaning, dry and wet abrasive blast cleaning, centrifugal wheel blast cleaning, chemical stripping, and waterjetting for the application of the coating system. In addition, the article provides a description...
Series: ASM Handbook
Volume: 1A
Publisher: ASM International
Published: 31 August 2017
DOI: 10.31399/asm.hb.v01a.a0006335
EISBN: 978-1-62708-179-5
... of the enamel. In some cleaning applications, a shot and grit mixture may be used. Although most often used as a cutting or machining process, the abrasive waterjet process has been tested for its use in degating and defining castings, as well as burn-in removal from castings. High-pressure waterjets...
Book Chapter

Series: ASM Handbook
Volume: 14B
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v14b.a0005174
EISBN: 978-1-62708-186-3
... with machining equipment such as band saws or abrasive waterjet cutting. Nonmechanical methods of cutting include material removal by chemical and/or thermal processes. These methods include gas cutting, electric arc cutting, and laser cutting. This article provides a general overview on these mechanical...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001303
EISBN: 978-1-62708-170-2
... Cutting , Forming and Forging , 9th ed. , Vol 14 , Metals Handbook , ASM International , 1988 , p 743 – 755 4. Johnston C.E. , Waterjet/Abrasive Waterjet Machining , Machining , 9th ed. , Vol 16 , Metals Handbook , ASM International , 1989 , p 520 – 527 5. Pulice F.R...
Book Chapter

By Ted A. Slezak
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002146
EISBN: 978-1-62708-188-7
... Abstract Sawing is the process of cutting a workpiece with power band saws, hacksaws, and circular saws. This article discusses the process capabilities and limitations of band sawing. It provides information on band sawing machines, their fixtures and attachments, band construction...
Series: ASM Handbook
Volume: 21
Publisher: ASM International
Published: 01 January 2001
DOI: 10.31399/asm.hb.v21.a0003423
EISBN: 978-1-62708-195-5
... either traditional solid tools or with newer technologies, such as abrasive waterjet trimming. Even if traditional methods are used, special tools and parameters are required due to the abrasive nature of carbon fibers and the danger of overheating or delaminating the workpiece. Therefore, the tool...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003694
EISBN: 978-1-62708-182-5
... Prepared by Waterjetting.” (d) SSPC-VIS 5/NACE VIS 9, “Guide and Reference Photographs for Steel Surfaces Prepared by Wet Abrasive Blast Cleaning” Abstract This article provides information on the factors influencing the selection of the proper corrosion-resistant coating system. It focuses...
Series: ASM Handbook
Volume: 7
Publisher: ASM International
Published: 30 September 2015
DOI: 10.31399/asm.hb.v07.a0006058
EISBN: 978-1-62708-175-7
... sections compared with wire EDM. Waterjet uses a high-pressure stream of water carrying an abrasive grit such as silicon carbide that abrades a beryllium or aluminum-beryllium blank, leaving a stress-free part without machining damage. Wire sawing beryllium, aluminum-beryllium alloy, E-material, and BeO...