Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001408
EISBN: 978-1-62708-173-3
... 795 115 … … … … … A 493 Type 440A (UNS S44002) B Annealed 725 (c) 105 (c) 415 (c) 60 (c) 20 (c) … 95 HRB (c) … B Tempered at 135 °C (600 °F) 1790 (c) 260 (c) 1650 (c) 240 (c) 5 (c) 20 (c) 51 HRC (c) … W Annealed, cold finished 965 max 140 max...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002180
EISBN: 978-1-62708-188-7
... 12.00–14.00 … 0.60 … … S42023 (420FSe) 0.30–0.40 1.25 1.00 0.06 0.06 12.00–14.00 … 0.60 … 0.15 min Se; 0.60 Zr or Cu S43100 431 0.20 1.00 1.00 0.040 0.030 15.00–17.00 1.25–2.50 … … … S44002 440A 0.60–0.75 1.00 1.00 0.040 0.030 16.00–18.00 … 0.75...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005673
EISBN: 978-1-62708-198-6
...) S43100 431 0.20 1.00 1.00 15.0–17.0 1.25–2.50 0.04 0.03 … S44002 440A 0.60–0.75 1.00 1.00 16.0–18.0 … 0.04 0.03 0.75 Mo (a) Single values are maximum values unless otherwise indicated. (b) Optional Martensite is created when the austenite becomes so unstable...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001046
EISBN: 978-1-62708-161-0
... 0.20–0.25 1.00 0.75 11.5–13.5 0.5–1.0 0.04 0.03 0.75–1.25 Mo; 0.75–1.25 W; 0.15–0.3 V 431 S43100 0.20 1.00 1.00 15.0–17.0 1.25–2.50 0.04 0.03 … 440A S44002 0.60–0.75 1.00 1.00 16.0–18.0 … 0.04 0.03 0.75 Mo 440B S44003 0.75–0.95 1.00 1.00 16.0–18.0 … 0.04 0.03...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003115
EISBN: 978-1-62708-199-3
... 431 0.20 1.00 1.00 15.0–17.0 1.25–2.50 0.04 0.03 … S44002 40A 0.60–0.75 1.00 1.00 16.0–18.0 … 0.04 0.03 0.75 Mo S44003 440B 0.75–0.95 1.00 1.00 16.0–18.0 … 0.04 0.03 0.75 Mo S44004 440C 0.95–1.20 1.00 1.00 16.0–18.0 … 0.04 0.03 0.75 Mo Nonstandard grades...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0006543
EISBN: 978-1-62708-183-2
... Type 416 S41600 7.7 0.28 Type 420 S42000 7.7 0.28 Type 430, 430F S43000, S43020 7.72 0.279 Type 431 S43100 7.7 0.28 Types 440A, 440B, 440C S44002, S44003, S44004 7.7 0.28 Type 446 S44600 7.65 0.276 Type 501 S50100 7.7 0.28 Type 502 S50200 7.82 0.283 19...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003812
EISBN: 978-1-62708-183-2
... 1.00 0.040 0.030 1.00 15.0–17.0 1.25–2.50 … … S44002 440A 0.60–0.75 1.00 0.040 0.030 1.00 16.0–18.0 … 0.75 … S44003 440B 0.75–0.95 1.00 0.040 0.030 1.00 16.0–18.0 … 0.75 … S44004 440C 0.95–1.20 1.00 0.040 0.030 1.00 16.0–18.0 … 0.75 … Precipitation...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005985
EISBN: 978-1-62708-168-9
... 0.04 0.03 … 440A S44002 0.60–0.75 1.00 1.00 16.0–18.0 … 0.04 0.03 0.75 Mo 440B S44003 0.75–0.95 1.00 1.00 16.0–18.0 … 0.04 0.03 0.75 Mo 440C S44004 0.95–1.20 1.00 1.00 16.0–18.0 … 0.04 0.03 0.75 Mo (a) Single values are maximum values unless otherwise...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002403
EISBN: 978-1-62708-193-1
... and carbon contents are increased in alloys S42000, S44002, S44003, and S44004. The first of these contains 14% Cr and 0.3% C and has a hardness capability of 50 HRC. The other three alloys contain 16% Cr and from 0.6 to 1.1% C. These alloys are capable of 60 HRC and a tensile yield strength of 1900 MPa (280...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001434
EISBN: 978-1-62708-173-3
... 2.50–3.00 … V, 0.20–0.30 431 S43100 A 479 0.20 max 1.00 max 0.040 0.030 max 1.00 15.00–17.00 1.25–2.50 … … … 440A S44002 A 276 0.60–0.75 1.00 max 0.040 0.030 max 1.00 16.00–18.00 … 0.75 … … 440B S44003 A 276 0.75–0.95 1.00 max 0.040 0.030 max 1.00 16.00–18.00...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005953
EISBN: 978-1-62708-168-9
... 431 S43100 0.20 1.00 1.00 0.04 0.03 15.0–17.0 1.25–2.50 … 440A S44002 0.60–0.75 1.00 1.00 0.04 0.03 16.0–18.0 … 0.75 Mo 440B S44003 0.75–0.95 1.00 1.00 0.04 0.03 16.0–18.0 … 0.75 Mo 440C S44004 0.95–1.20 1.00 1.00 0.04 0.03 16.0–18.0 … 0.75 Mo TrimRite...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001305
EISBN: 978-1-62708-170-2
... … … S42023 420FSe (b) 0.30–0.40 1.25 1.00 0.060 0.060 12.00–14.00 … 0.60 … 0.15 min Se; 0.60 Zr or Cu S43100 431 0.20 1.00 1.00 0.040 0.030 15.00–17.00 1.25–2.50 … … … S44002 440A 0.60–0.75 1.00 1.00 0.040 0.030 16.00–18.00 … 0.75 … … S44003 440B 0.75–0.95 1.00...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003767
EISBN: 978-1-62708-177-1
...–17.0 1.25–2.50 0.04 0.03 … 440A S44002 0.60–0.75 1.00 1.00 16.0–18.0 … 0.04 0.03 0.75 Mo 440B S44003 0.75–0.95 1.00 1.00 16.0–18.0 … 0.04 0.03 0.75 Mo 440C S44004 0.95–1.20 1.00 1.00 16.0–18.0 … 0.04 0.03 0.75 Mo Precipitation-hardening types PH 13-8 Mo...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002461
EISBN: 978-1-62708-194-8
... 1.00 16.00–18.00 … 0.75–1.25 Nb + Ta 5 × C min, 0.70 max 440A S44002 0.60–0.75 1.00 0.040 0.030 1.00 16.00–18.00 … 0.75 … 440B S44003 0.75–0.95 1.00 0.040 0.030 1.00 16.00–18.00 … 0.75 … 440C S44004 0.95–1.20 1.00 0.040 0.030 1.00 16.00–18.00 … 0.75 … 442...