1-16 of 16 Search Results for

UNS S41600

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001408
EISBN: 978-1-62708-173-3
... … A 276, A 479 W Annealed, cold finished 1030 max 150 max … … … … … A 580 CA6NM (UNS S41500) P, Sh, St Tempered 795 115 620 90 15 … 32 HRC max A 176, A 240 B, F Tempered 795 115 620 90 15 45 … A 276, A 473, A 479 Types 416 (UNS S41600) and 416Se (UNS S41623...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002180
EISBN: 978-1-62708-188-7
... … … … … S41000 410 0.15 1.00 1.00 0.040 0.030 11.50–13.00 … … … … S41400 414 0.15 1.00 1.00 0.040 0.030 11.50–13.50 1.25–2.50 … … … S41600 416 0.15 1.25 1.00 0.060 0.15 min 12.00–14.00 … 0.60 … … S41610 [XM-6] 0.15 1.50–2.50 1.00 0.06 0.15 min 12.00–14.00 … 0.60...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001046
EISBN: 978-1-62708-161-0
... S41600 0.15 1.25 1.00 12.0–14.0 … 0.06 0.15 min 0.6 Mo (b) 416Se S41623 0.15 1.25 1.00 12.0–14.0 … 0.06 0.06 0.15 min Se 420 S42000 0.15 min 1.00 1.00 12.0–14.0 … 0.04 0.03 … 420F S42020 0.15 min 1.25 1.00 12.0–14.0 … 0.06 0.15 min 0.6 Mo (b) 422 S42200...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005673
EISBN: 978-1-62708-198-6
... and dental instruments Table 4 Chemical compositions of martensitic stainless steels commonly used for surgical and dental instruments UNS No. Type/designation Composition (a) , % C Mn Si Cr Ni P S Other S41000 410 0.15 1.00 1.00 11.5–13.5 … 0.04 0.03 … S41600 416...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0006543
EISBN: 978-1-62708-183-2
... Type 416 S41600 7.7 0.28 Type 420 S42000 7.7 0.28 Type 430, 430F S43000, S43020 7.72 0.279 Type 431 S43100 7.7 0.28 Types 440A, 440B, 440C S44002, S44003, S44004 7.7 0.28 Type 446 S44600 7.65 0.276 Type 501 S50100 7.7 0.28 Type 502 S50200 7.82 0.283 19...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003115
EISBN: 978-1-62708-199-3
... S40300 403 0.15 1.00 0.50 11.5–13.0 … 0.04 0.03 … S41000 410 0.15 1.00 1.00 11.5–13.5 … 0.04 0.03 … S41400 414 0.15 1.00 1.00 11.5–13.5 1.25–2.50 0.04 0.03 … S41600 416 0.15 1.25 1.00 12.0–14.0 … 0.06 0.15 min 0.6 Mo (b) S41623 416Se 0.15 1.25 1.00...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003812
EISBN: 978-1-62708-183-2
...–13.0 0.60 … … S41000 410 0.08–0.15 1.00 0.040 0.030 1.00 11.5–13.5 0.75 … … S41400 414 0.15 1.00 0.040 0.030 1.00 11.5–13.5 1.25–2.50 … … S41600 416 0.15 1.25 0.060 0.15 min 1.00 12.0–14.0 … 0.60 … S41623 416Se 0.15 1.25 0.060 0.060 1.00 12.0–14.0...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005985
EISBN: 978-1-62708-168-9
... 0.03 … 410 S41000 0.15 1.00 1.00 11.5–13.5 … 0.04 0.03 … 414 S41400 0.15 1.00 1.00 11.5–13.5 1.25–2.50 0.04 0.03 … 416 S41600 0.15 1.25 1.00 12.0–14.0 … 0.06 0.15 min 0.6 Mo (b) 416Se S41623 0.15 1.25 1.00 12.0–14.0 … 0.06 0.06 0.15 min Se 420...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004149
EISBN: 978-1-62708-184-9
... 90-10 cupronickel C70600 B111 … ∼88 (bal) 1.3 … 10 … 1 max Mn, 1 max Zn Type 304 S30400 A182 19 … ∼70 (bal) … 9 … 2 max Mn, 1 max Si Type 316 S31600 A182 17 … 67 (bal) 2.5 12 … 2 max Mn, 1 max Si Type 416 S41600 A194 13 … ∼85 (bal) 0.6 max … … 1.25 max Mn...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003116
EISBN: 978-1-62708-199-3
... Non-free-machining alloys Related free-machining alloys Selenium-bearing Sulfur-bearing Ferritic S43000 S43023 S43020 S44400 … S18200 (a) S18235 Martensitic S41000 S41623 S41600 S41610 (b) S42000 S42023 S42020 S44004 S44023 S44020 Austenitic...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001434
EISBN: 978-1-62708-173-3
... max 1.00 11.50–13.50 1.25–2.50 … … … 410NiMo S41500 A 240 0.05 max 0.5–1.0 0.030 0.030 max 0.60 11.5–14.0 3.5–5.5 0.5–1.0 … … 416 S41600 A 473 0.15 max 1.25 max 0.06 0.15 min 1.00 12.00–14.00 … 0.60 max … … XM-6 S41610 A 582 0.15 max 1.50–2.50 0.06 0.15 min...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001048
EISBN: 978-1-62708-161-0
... 403 S40300 0.15 max 12.0 … … … … … … 410 S41000 0.15 max 12.5 … … … … … … 410Cb S41040 0.15 max 12.5 … … … 0.12 … … 416 S41600 0.15 max 13.0 … 0.6 (b) … … … 0.15 min S 422 S42200 0.20 12.5 0.75 1.0 … … … 1.0 W, 0.22 V H-46 … 0.12 10.75...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003767
EISBN: 978-1-62708-177-1
... 11.5–13.0 … 0.04 0.03 … 410 S41000 0.15 1.00 1.00 11.5–13.5 … 0.04 0.03 … 414 S41400 0.15 1.00 1.00 11.5–13.5 1.25–2.50 0.04 0.03 … 416 S41600 0.15 1.25 1.00 12.0–14.0 … 0.06 0.15 min 0.6 Mo (b) 416Se S41623 0.15 1.25 1.00 12.0–14.0 … 0.06 0.06 0.15...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001305
EISBN: 978-1-62708-170-2
... … … … … S41400 414 0.15 1.00 1.00 0.040 0.030 11.50–13.50 1.25–2.50 … … … S41600 416 0.15 1.25 1.00 0.060 0.15 (a) 12.00–14.00 … 0.60 … … S41610 416 Plus X (d) 0.15 1.50–2.50 1.00 0.060 0.15 (a) 12.00–14.00 … 0.60 … … S41623 416Se 0.15 1.25 1.00 0.060 0.060...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002461
EISBN: 978-1-62708-194-8
... 1.00 11.50–14.50 … … Al 0.10–0.30 409 S40900 0.08 1.00 0.045 0.045 1.00 10.50–11.75 … … Ti 6 × C min; 0.75 max 410 S41000 0.15 1.00 0.040 0.030 1.00 11.50–13.50 … … … 414 S41400 0.15 1.00 0.040 0.030 1.00 11.50–13.50 1.25–2.50 … … 416 S41600 0.15 1.25...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002183
EISBN: 978-1-62708-188-7
... SR …  18Cr-2Mo …  446 S44600  E-Brite 26-1 S44627  26-1Ti …  29Cr-4Mo … Quenched-and-tempered martensitic stainless steels  403 S40300  410 S41000  416 S41600  422 S42200  H-46 …  Moly Ascoloy …  Greek Ascoloy …  Jethete M-152 …  Almar 363...