1-16 of 16 Search Results for

UNS S40300

Sort by
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001408
EISBN: 978-1-62708-173-3
... compositions for standard and nonstandard grades, respectively. Chemical compositions of standard wrought martensitic stainless steels Table 1 Chemical compositions of standard wrought martensitic stainless steels Type UNS No. Composition, % (a) C Mn Si Cr Ni P S Other 403 S40300...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002180
EISBN: 978-1-62708-188-7
... … … 0.25 … S18200 [XM-34] 0.08 1.25–2.50 1.00 0.04 0.15 min 17.50–19.50 … 1.50–2.50 … … S18235 … 0.025 0.50 1.00 0.030 0.15–0.35 17.50–18.50 1.00 2.00–2.50 0.025 0.30–1.00 Ti, 0.035 C + N Martensitic alloys S40300 403 0.15 1.00 0.50 0.040 0.030 11.50–13.00...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001046
EISBN: 978-1-62708-161-0
... S32900 0.20 1.00 0.75 23.0–28.0 2.50–5.00 0.040 0.030 1.00–2.00 Mo Martensitic types 403 S40300 0.15 1.00 0.50 11.5–13.0 … 0.04 0.03 … 410 S41000 0.15 1.00 1.00 11.5–13.5 … 0.04 0.03 … 414 S41400 0.15 1.00 1.00 11.5–13.5 1.25–2.50 0.04 0.03 … 416...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003115
EISBN: 978-1-62708-199-3
... S40300 403 0.15 1.00 0.50 11.5–13.0 … 0.04 0.03 … S41000 410 0.15 1.00 1.00 11.5–13.5 … 0.04 0.03 … S41400 414 0.15 1.00 1.00 11.5–13.5 1.25–2.50 0.04 0.03 … S41600 416 0.15 1.25 1.00 12.0–14.0 … 0.06 0.15 min 0.6 Mo (b) S41623 416Se 0.15 1.25 1.00...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0006543
EISBN: 978-1-62708-183-2
... Type 316, 316L S31600, S31603 7.98 0.288 Type 317 S31700 7.98 0.288 Type 321 S32100 7.94 0.287 Type 329 S32900 7.98 0.288 Type 330 N08330 7.98 0.288 Type 347 S34700 8.03 0.290 Type 403 S40300 7.7 0.28 Type 405 S40500 7.7 0.28 Type 410 S41000 7.70 0.278...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003812
EISBN: 978-1-62708-183-2
... 1.00 0.040 0.040 1.00 18.0–23.0 0.60 … … S44400 444 0.025 1.00 0.040 0.030 1.00 17.5–19.5 1.00 1.75–2.50 4(C+N)+0.20 ≤Ti+Nb≤0.80 S44600 446 0.20 1.50 0.040 0.030 1.00 23.0–27.0 0.75 … 0.25N Martensitic grades S40300 403 0.15 1.00 0.040 0.030 0.50 11.5...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005985
EISBN: 978-1-62708-168-9
... to other stainless steels. Compositions of standard wrought martensitic stainless steels Table 1 Compositions of standard wrought martensitic stainless steels Type UNS designation Composition (a) , % C Mn Si Cr Ni P S Other 403 S40300 0.15 1.00 0.50 11.5–13.0 … 0.04...
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003556
EISBN: 978-1-62708-180-1
... that this may be due to the ratio of cathodic to anodic areas, where a single phase, for example, ferrite, is preferentially attacked relative to a large area of less susceptible material. Penetration rates of 17 mm/year (0.7 in./year) in United Numbering System (UNS) 30800 welds have been reported. Perforation...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006788
EISBN: 978-1-62708-295-2
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002403
EISBN: 978-1-62708-193-1
... 1.0 16–18 … 0.04 0.03 0.75–1.25Mo 365 (53) ann 442 S44200 0.20 1.0 1.0 18–23 … 0.04 0.03 … 275 (40) ann 446 S44600 0.20 1.5 1.0 23–27 … 0.04 0.03 0.25N 275 (40) ann Martensitic types 403 S40300 0.15 1.00 0.50 11.5–13.0 … 0.04 0.03 … 550 (80) ht 410...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001434
EISBN: 978-1-62708-173-3
... stainless steels Designation UNS No. ASTM specification Tensile strength Yield strength Elongation, % Matching filler metals MPa ksi MPa ksi A5.4 A5.9 (a) A5.22 XM-32 K64152 A 565 1000 145 790 115 15 … … … 403 S40300 A 479 480 70 275 40 20 E410-XX ER410 E410T...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001048
EISBN: 978-1-62708-161-0
... 403 S40300 0.15 max 12.0 … … … … … … 410 S41000 0.15 max 12.5 … … … … … … 410Cb S41040 0.15 max 12.5 … … … 0.12 … … 416 S41600 0.15 max 13.0 … 0.6 (b) … … … 0.15 min S 422 S42200 0.20 12.5 0.75 1.0 … … … 1.0 W, 0.22 V H-46 … 0.12 10.75...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001305
EISBN: 978-1-62708-170-2
... 1.00 0.040 0.030 23.00–27.00 … … 0.25 … S18200 18-2FM (c) 0.08 1.25–2.50 1.00 0.040 0.15 (a) 17.50–19.50 … 1.50–2.50 … … Martensitic alloys S40300 403 0.15 1.00 0.50 0.040 0.030 11.50–13.00 … … … … S41000 410 0.15 1.00 1.00 0.040 0.030 11.50–13.00...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003767
EISBN: 978-1-62708-177-1
...–2.50 Mo; 0.025 N; 0.2 + 4 (%C + %N) min–0.8 max (Ti + Nb) 446 S44600 0.20 1.50 1.00 23.0–27.0 … 0.04 0.03 0.25 N Duplex (ferritic-austenitic) type 329 S32900 0.20 1.00 0.75 23.0–28.0 2.50–5.00 0.040 0.030 1.00–2.00 Mo Martensitic types 403 S40300 0.15 1.00 0.50...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002461
EISBN: 978-1-62708-194-8
... S34800 0.08 2.00 0.045 0.030 1.00 17.00–19.00 9.00–13.00 … Nb + Ta 10 × C min; Ta 0.10 max; Co 0.20 max 384 S38400 0.08 2.00 0.045 0.030 1.00 15.00–17.00 17.00–19.00 … … 403 S40300 0.15 1.00 0.040 0.030 0.50 11.50–13.00 … … … 405 S40500 0.08 1.00 0.040 0.030...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002183
EISBN: 978-1-62708-188-7
... SR …  18Cr-2Mo …  446 S44600  E-Brite 26-1 S44627  26-1Ti …  29Cr-4Mo … Quenched-and-tempered martensitic stainless steels  403 S40300  410 S41000  416 S41600  422 S42200  H-46 …  Moly Ascoloy …  Greek Ascoloy …  Jethete M-152 …  Almar 363...