DOI: 10.31399/asm.hb.v13c.a0004186
EISBN: 978-1-62708-184-9
... ) ( Ref 3 ). Fig. 2 Effect of acid concentration on corrosion rate of type 316L stainless steel in phosphoric acid at 163 °C (325 °F) Type 317L (UNS S31703) stainless steel behaves similarly to 316L and can be used interchangeably up to approximately 60% acid. At this point, 316L apparently...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003662
EISBN: 978-1-62708-182-5
... N08926 1.6 5.2 S 53 2 S32760 2.4 7.9 MS OK at 60 0 S39724 2.4 7.9 MS OK at 60 0 UNS, Unified Numbering System. (a) MS, moderately severe; S, severe. (b) Maximum depth (0.57 mm, or 0.022 in.) found on UNS S31703 tube; all others ≤0.22 mm (0.0087 in.). Source: Ref 45...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001410
EISBN: 978-1-62708-173-3
... Mo 316LN S31653 0.03 2.0 1.00 16.0–18.0 10.0–14.0 0.045 0.03 2.0–3.0 Mo; 0.10–0.16 N 316N S31651 0.08 2.0 1.00 16.0–18.0 10.0–14.0 0.045 0.03 2.0–3.0 Mo; 0.10–0.16 N 317 S31700 0.08 2.0 1.00 18.0–20.0 11.0–15.0 0.045 0.03 3.0–4.0 Mo 317L S31703 0.03 2.0 1.00...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004153
EISBN: 978-1-62708-184-9
... chemical compositions of the various alloys considered for use in FGD systems are shown in Table 1 . Included in generally increasing corrosion-resistance order are the austenitic stainless steels, types 316L (UNS S31603) and 317L (S31703), and the 4% molybdenum stainless steels, types 317LM (S31725...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002180
EISBN: 978-1-62708-188-7
... 1.00 0.045 0.030 16.00–18.00 10.00–14.00 2.00–3.00 … … S31620 316F 0.08 2.00 1.00 0.20 0.10 min 17.00–19.00 12.00–14.00 1.75–2.50 … … S31700 317 0.08 2.00 1.00 0.045 0.030 18.00–20.00 11.00–15.00 3.00–4.00 … … S31703 317L 0.030 2.00 1.00 0.045 0.030 18.00...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003664
EISBN: 978-1-62708-182-5
...) 120 0.1 (4) S31603 Type 316L 1 h at 675 °C (1250 °F) Oxalic acid (A 262-A) … (a) Ferric sulfate (A 262-B) 120 0.1 (4) S31700 Type 317 None Oxalic acid (A 262-A) … (a) Ferric sulfate (A 262-B) 120 0.1 (4) S31703 Type 317L 1 h at 675 °C (1250 °F) Oxalic acid (A 262...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003812
EISBN: 978-1-62708-183-2
... 0.10N S31603 316L 0.030 2.00 0.045 0.030 0.75 16.0–18.0 10.0–14.0 2.00–3.00 0.10N S31651 316N 0.08 2.00 0.045 0.030 0.75 16.0–18.0 10.0–14.0 2.00–3.00 0.10–0.16N S31700 317 0.08 2.00 0.045 0.030 0.75 18.0–20.0 11.0–15.0 3.0–4.0 0.10N S31703 317L 0.030 2.00...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001046
EISBN: 978-1-62708-161-0
... 317L S31703 0.03 2.00 1.00 18.0–20.0 11.0–15.0 0.045 0.03 3.0–4.0 Mo 321 S32100 0.08 2.00 1.00 17.0–19.0 9.0–12.0 0.045 0.03 5 × %C min Ti 321H S32109 0.04–0.10 2.00 1.00 17.0–19.0 9.0–12.0 0.045 0.03 5 × %C min Ti 330 N08330 0.08 2.00 0.75–1.5 17.0–20.0 34.0...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003115
EISBN: 978-1-62708-199-3
... 0.045 0.03 3.0–4.0 Mo S31703 317L 0.03 2.0 1.00 18.0–20.0 11.0–15.0 0.045 0.03 3.0–4.0 Mo S32100 321 0.08 2.0 1.00 17.0–19.0 9.0–12.0 0.045 0.03 5 × %C min Ti S32109 321H 0.04–0.10 2.0 1.00 17.0–19.0 9.0–12.0 0.045 0.03 5 × %C min Ti N08330 330 0.08 2.0 0.75...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003821
EISBN: 978-1-62708-183-2
... Table 1 Nominal compositions of nickel alloys resistant to aqueous corrosion Family Common name UNS No. Form Composition, wt% Ni Cu Mo Cr Fe W Mn Si C Al Ti Other Ni 200 N02200 Wrought 99.5 0.1 … … 0.2 … 0.2 0.2 0.08 … … … 201 N02201 Wrought 99.5 0.1...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004130
EISBN: 978-1-62708-184-9
..., S31703, S31803, N08904, N08367, S44660, S20910, S44735, N10276, and R50250. The practical importance of ennoblement is increased probability of localized corrosion as E corr approaches the pitting potential ( E pit ) for stainless steels vulnerable to crevice corrosion, especially types 304 (UNS...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005990
EISBN: 978-1-62708-168-9
... 0.03 2.00 1.00 16.0–18.0 10.0–14.0 0.045 0.03 2.0–3.0 Mo; 0.10–0.16 N 316N S31651 0.08 2.00 1.00 16.0–18.0 10.0–14.0 0.045 0.03 2.0–3.0 Mo; 0.10–0.16 N 317 S31700 0.08 2.00 1.00 18.0–20.0 11.0–15.0 0.045 0.03 3.0–4.0 Mo 317L S31703 0.03 2.00 1.00 18.0–20.0 11.0...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004137
EISBN: 978-1-62708-184-9
... 317L S31703 0.03 max bal 13.0 19.0 3.5 2.0 max 1.00 max Si, 0.045 max P, and 0.03 max S 625 N06625 0.10 max 5.0 max bal 21.5 9.0 0.50 max 0.40 max Al, 0.40 max Ti, 3.65 Nb, 0.015 max P, 0.015 max S, and 0.50 max Si 825 N08825 0.05 max bal 42.0 21.5 3.0 1.0 max 0.8 Ti, 0.5...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003117
EISBN: 978-1-62708-199-3
... 7-Mo PLUS 15 60 S31803 2205 17.5 63.5 S32250 Ferralium 255 22.5 72.5 Austenitic grades S30400 Type 304 <−2.5 <27.5 S31600 Type 316 −2.5 27.5 S31703 Type 317L 0 32 N08020 20Cb-3 0 32 N08366 AL-6N 17.5 63.5 N08367 AL-6XN 32.5 90.5...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003548
EISBN: 978-1-62708-180-1
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003637
EISBN: 978-1-62708-182-5
... and filamentous microorganisms observed on a Unified Numbering System (UNS) S20910 (Nitronic 50) alloy surface immersed in natural seawater for 28 days. Source: Ref 16 Fig. 8 Filamentous and coccoidal microorganisms observed on a UNS S20910 (Nitronic 50) alloy surface immersed in natural seawater...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003203
EISBN: 978-1-62708-199-3
...–1950 N08020 20Cb-3 925–955 1700–1750 Low-carbon grades S30403 304L 1010–1120 1850–2050 S30453 304LN 1010–1120 1850–2050 S31603 316L 1040–1110 1900–2025 S31653 316LN 1040–1110 1900–2025 S31703 317L 1040–1110 1900–2025 High-nitrogen grades S20100 201...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006783
EISBN: 978-1-62708-295-2
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001434
EISBN: 978-1-62708-173-3
... approximately matching compositions, as classified by the American Welding Society (AWS), are also listed in Table 1(b) , but only for selected base metals. Compositions of nominally martensitic stainless steels Table 1(a) Compositions of nominally martensitic stainless steels Designation UNS...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001048
EISBN: 978-1-62708-161-0
... … … … … 317L S31703 0.035 max 19.0 13.0 3.5 … … … … 321 S32100 0.08 max 18.0 10.0 … … … 5 × C min, 0.70 max … 321H S32109 0.04–0.10 18.0 10.0 … … … 4 × C min, 0.60 max … 347 S34700 0.08 max 18.0 11.0 … … 10 × C min (c) … 1.0 (Nb + Ta) max 347H S34709 0.04–0.10...