1-18 of 18 Search Results for

UNS S30200

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003834
EISBN: 978-1-62708-183-2
.... For example, in stainless steel clad aluminum truck bumpers ( Fig. 4 ), type 301 (UNS S30100) or 302 (UNS S30200) stainless steel cladding provides a bright corrosion-resistant surface that also resists the mechanical damage (stone impingement) encountered in service. The aluminum provides a substrate...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001410
EISBN: 978-1-62708-173-3
... 0.03 0.25 N 202 S20200 0.15 7.5–10.0 1.00 17.0–19.0 4.0–6.0 0.06 0.03 0.25 N 205 S20500 0.12–0.25 14.0–15.5 1.00 16.5–18.0 1.0–1.75 0.06 0.03 0.32–0.40 N 301 S30100 0.15 2.0 1.00 16.0–18.0 6.0–8.0 0.045 0.03 … 302 S30200 0.15 2.0 1.00 17.0–19.0 8.0–10.0...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002180
EISBN: 978-1-62708-188-7
... between yield and ultimate tensile strengths, and work-hardening rate for S30100 austenitic stainless steel, S43000 ferritic stainless steel, and G10080 carbon steel Fig. 2 Comparison of thermal conductivities for carbon steel, S30200 austenitic stainless steel, and S43000 ferritic stainless...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001046
EISBN: 978-1-62708-161-0
... 0.25 N 202 S20200 0.15 7.5–10.0 1.00 17.0–19.0 4.0–6.0 0.06 0.03 0.25 N 205 S20500 0.12–0.25 14.0–15.5 1.00 16.5–18.0 1.0–1.75 0.06 0.03 0.32–0.40 N 301 S30100 0.15 2.00 1.00 16.0–18.0 6.0–8.0 0.045 0.03 … 302 S30200 0.15 2.00 1.00 17.0–19.0 8.0–10.0 0.045...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005673
EISBN: 978-1-62708-198-6
... 0.15 2.0 1.00 16.0–18.0 6.0–8.0 0.045 0.03 … S30200 302 0.15 2.0 1.00 17.0–19.0 8.0–10.0 0.045 0.03 … S30300 303 0.15 2.0 1.00 17.0–19.0 8.0–10.0 0.20 0.15 min 0.6 Mo (b) S30400 304 0.08 2.0 1.00 18.0–20.0 8.0–10.5 0.045 0.03 … S30500 305 0.12 2.0 1.00...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003115
EISBN: 978-1-62708-199-3
... 0.15 5.5–7.5 1.00 16.0–18.0 3.5–5.5 0.06 0.03 0.25 N S20200 202 0.15 7.5–10.0 1.00 17.0–19.0 4.0–6.0 0.06 0.03 0.25 N S20500 205 0.12–0.25 14.0–15.5 1.00 16.5–18.0 1.0–1.75 0.06 0.03 0.32–0.40 N S30100 301 0.15 2.0 1.00 16.0–18.0 6.0–8.0 0.045 0.03 … S30200...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0006543
EISBN: 978-1-62708-183-2
... 0.279 HN J94213 7.83 0.283 HT N08605 7.92 0.286 HU … 8.04 0.290 HW … 8.14 0.294 HX … 8.14 0.294 Wrought stainless and heat-resistant steels Type 201 S20100 7.94 0.287 Type 202 S20200 7.94 0.287 Type 301 S30100 7.94 0.287 Type 302 S30200 7.94...
Series: ASM Handbook
Volume: 23A
Publisher: ASM International
Published: 12 September 2022
DOI: 10.31399/asm.hb.v23A.a0006888
EISBN: 978-1-62708-392-8
... UNS No. Chemical composition, wt% C Mn Si Cr Ni N P S Cu Mo Other S30100 0.15 2.0 1.00 16.0–18.0 6.0–8.0 … 0.045 0.03 … … … S30200 0.15 2.0 1.00 17.0–19.0 8.0–10.0 … 0.045 0.03 … … … S30300 0.15 2.0 1.00 17.0–19.0 8.0–10.0...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003812
EISBN: 978-1-62708-183-2
... Austenitic grades S20100 201 0.15 5.5–7.5 0.060 0.030 1.00 16.0–18.0 3.5–5.5 … 0.25N S20200 202 0.15 7.5–10.0 0.060 0.030 1.00 17.0–19.0 4.0–6.0 … 0.25N S30100 301 0.15 2.00 0.045 0.030 1.00 16.0–18.0 6.0–8.0 … 0.10N S30200 302 0.15 2.00 0.045 0.030 0.75 17.0...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005990
EISBN: 978-1-62708-168-9
... in Table 3 . Recommended annealing temperatures for wrought austenitic stainless steels Table 2 Recommended annealing temperatures for wrought austenitic stainless steels UNS No. Designation Temperature (a) °C °F Conventional grades S30100 301 1040 1900 S30200 302 1040...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0003999
EISBN: 978-1-62708-185-6
... stainless steel S30200 192 27.8 168 24.3 148 21.4 124 18 (a) Pressure developed in the roll gap at 20% reduction in hot rolling The flow stress of nickel-base alloys is influenced by alloy content, working temperature, working strain rate, working strain, and the grain size...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001434
EISBN: 978-1-62708-173-3
... approximately matching compositions, as classified by the American Welding Society (AWS), are also listed in Table 1(b) , but only for selected base metals. Compositions of nominally martensitic stainless steels Table 1(a) Compositions of nominally martensitic stainless steels Designation UNS...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003203
EISBN: 978-1-62708-199-3
... S30200 302 1010–1120 1850–2050 S30215 302B 1010–1120 1850–2050 S30300 303 1010–1120 1850–2050 S30323 303Se 1010–1120 1850–2050 S30400 304 1010–1120 1850–2050 S30500 305 1010–1120 1850–2050 S30800 308 1010–1120 1850–2050 S30900 309 1040–1120 1900–2050 S30908...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003116
EISBN: 978-1-62708-199-3
... … … S20300 S30200/S30400 S30323 S30300 S30310 (b) S30345 (c) S30360 (d) S30430 … S30330 S30431 (e) S31600 … S31620 S34700 S34723 S34720 (a) Does not contain titanium. (b) Contains high manganese. (c) Contains aluminum. (d) Contains lead. (e) Contains...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001305
EISBN: 978-1-62708-170-2
... … … 15.00–17.00 1.50–3.00 … 0.15–0.30 1.00 Cu S30100 301 0.15 2.00 1.00 0.045 0.030 16.00–18.00 6.00–8.00 … … … S30200 302 0.15 2.00 1.00 0.045 0.030 17.00–19.00 8.00–10.00 … … … S30300 303 0.15 2.00 1.00 0.20 0.15 (a) 17.00–19.00 8.00–10.00 0.60 … … S30310...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003206
EISBN: 978-1-62708-199-3
... electrodes (AWS A5.17-89) Electrode Composition (a) (b) , wt% AWS classification UNS No. C Mn Si S P Cu (c) Ti Low-manganese electrodes EL8 K01008 0.10 0.25–0.60 0.07 0.030 0.030 0.35 … EL8K K01009 0.10 0.25–0.60 0.10–0.25 0.030 0.030 0.35 … EL12 K01012...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003767
EISBN: 978-1-62708-177-1
... 16.5–18.0 1.0–1.75 0.06 0.03 0.32–0.40 N 301 S30100 0.15 2.00 1.00 16.0–18.0 6.0–8.0 0.045 0.03 … 302 S30200 0.15 2.00 1.00 17.0–19.0 8.0–10.0 0.045 0.03 … 302B S30215 0.15 2.00 2.0–3.0 17.0–19.0 8.0–10.0 0.045 0.03 … 303 S30300 0.15 2.00 1.00 17.0–19.0...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002461
EISBN: 978-1-62708-194-8
... … … 302 S30200 0.15 2.00 0.045 0.030 1.00 17.00–19.00 8.00–10.00 … … 302B S30215 0.15 2.00 0.045 0.030 2.00–3.00 17.00–19.00 8.00–10.00 … … 303 S30300 0.15 2.00 0.20 0.15 min 1.00 17.00–19.00 8.00–10.00 0.60 (a) … 303Se S30323 0.15 2.00 0.20 0.060 1.00 17.00...