1-18 of 18 Search Results for

UNS S15500

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Series: ASM Handbook
Volume: 12
Publisher: ASM International
Published: 01 January 1987
DOI: 10.31399/asm.hb.v12.a0000612
EISBN: 978-1-62708-181-8
...-pressure compressor used in a polyethylene process. The forging was made of Armco 15-5PH (UNS S15500), quenched and tempered to the H1075 condition. The end cap was located between the crosshead and plunger of the compressor, where it was subjected to repeated impacts by the tungsten carbide plunger...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002180
EISBN: 978-1-62708-188-7
... 0.040 0.030 23.00–28.00 2.50–5.00 1.00–2.00 … … S32950 … 0.03 2.00 0.60 0.035 0.010 26.0–29.0 3.50–5.20 1.00–2.50 0.15–0.35 … Precipitation-hardenable alloys S13800 (c) [XM-13] 0.05 0.20 0.10 0.01 0.008 12.25–13.25 7.50–8.50 2.00–2.50 0.01 0.90–1.35 Al S15500...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005961
EISBN: 978-1-62708-168-9
... to 0.0006 in. per 1 in.). Condition A material, when hardened to condition H1150, contracts approximately 0.023 to 0.030 mm per 25 mm (0.0009 to 0.0012 in. per 1 in.). Thermal treatment temperatures for Type 630 are: Alloy 15-5 PH As with 17-4 PH, alloy 15-5 PH (UNS S15500) is supplied...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005673
EISBN: 978-1-62708-198-6
... UNS No. Alloy Composition (a) , % C Mn Si Cr Ni Mo P S Other Martensitic types S13800 PH13-8 Mo 0.05 0.10 0.10 12.25–13.25 7.5–8.5 2.0–2.5 0.01 0.008 0.90–1.35 Al; 0.01 N S15500 15-5PH 0.07 1.00 1.00 14.0–15.5 3.5–5.5 … 0.04 0.03 2.5–4.5 Cu; 0.15–0.45 Nb...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001046
EISBN: 978-1-62708-161-0
... 0.75 Mo 440C S44004 0.95–1.20 1.00 1.00 16.0–18.0 … 0.04 0.03 0.75 Mo Precipitation-hardening types PH 13-8 Mo S13800 0.05 0.20 0.10 12.25–13.25 7.5–8.5 0.01 0.008 2.0–2.5 Mo; 0.90–1.35 Al; 0.01 N 15-5 PH S15500 0.07 1.00 1.00 14.0–15.5 3.5–5.5 0.04 0.03 2.5–4.5...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003115
EISBN: 978-1-62708-199-3
...–1.35 Al; 0.01 N S15500 15-5PH 0.07 1.00 1.00 14.0–15.5 3.5–5.5 … 0.04 0.03 2.5–4.5 Cu; 0.15–0.45 Nb S17400 17-4PH 0.07 1.00 1.00 15.0–17.5 3.0–5.0 … 0.04 0.03 3.0–5.0 Cu; 0.15–0.45 Nb S45000 Custom 450 0.05 1.00 1.00 14.0–16.0 5.0–7.0 0.5–1.0 0.03 0.03 1.25–1.75...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001412
EISBN: 978-1-62708-173-3
...  P, Sh, St H1000 1380 200 1310 190 6–10 (c) … 43 … A 693 15-5PH (UNS S15500)  B, F H900 1310 190 1170 170 10; 6 (b) 35; 15 (b) 40 … A 564, A 705  B, F H925 1170 170 1070 155 10; 7 (b) 38; 20 (b) 38 … A 564, A 705  B, F H1025 1070 155 1000 145 12; 8...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003812
EISBN: 978-1-62708-183-2
...–1.35Al, 0.01N S15500 15-5PH, XM-12 0.07 1.00 0.04 0.03 1.00 14.00–15.50 3.50–5.50 … 2.50–4.50Cu, 0.15–0.45Nb S45000 Custom 450 0.05 1.00 0.03 0.03 1.00 14.00–16.00 5.00–7.00 0.5–1.00 1.25–1.75Cu, Nb: 8×C min S45500 Custom 455 0.05 0.50 0.04 0.03 0.50 11.00–12.50 7.50...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001476
EISBN: 978-1-62708-173-3
... Type UNS designation Covered electrodes Bare welding wire Dissimilar PH stainless steels Martensitic 17-4 PH S17400 AMS 5827B (17-4 PH) or E308 AMS 5826 (17-4 PH) or ER308 E309 or ER309, E309Cb or ER309Cb 15-5 PH S15500 AMS 5827B (17-4 PH) or E308 AMS 5826 (17-4 PH) or ER308...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002403
EISBN: 978-1-62708-193-1
...) ht 431 S43100 0.20 1.00 1.00 15.0–17.0 1.25–2.50 0.04 0.03 … 1030 (149) ht Precipitation hardening types (f) 15-5PH S15500 0.07 1.00 1.00 14.0–15.5 3.5–5.5 0.04 0.03 2.5–4.5Cu, 0.15–0.45 (Nb + Ta) 1000 (145) ht 17-4PH S17400 0.07 1.00 1.00 15.5–17.5 3.0–5.0...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001434
EISBN: 978-1-62708-173-3
... Table 1(a) Compositions of nominally martensitic stainless steels Designation UNS No. ASTM specification Composition, wt% C Mn P (max) S Si (max) Cr Ni Mo N Other XM-32 K64152 A 565 0.08–0.15 0.50–0.90 0.025 0.025 max 0.35 11.00–12.50 2.00–3.00 1.50–2.00 0.01–0.05...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001048
EISBN: 978-1-62708-161-0
... 2.0 … … … … … Lapelloy S42300 0.30 11.5 … 2.75 … … … 0.25 V Precipitation-hardening martensitic stainless steels Custom 450 … 0.05 max 15.5 6.0 0.75 … 8 × C min … 1.5 Cu Custom 455 … 0.03 11.75 8.5 … … 0.30 1.2 2.25 Cu 15-5 PH S15500 0.07 15.0 4.5...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001305
EISBN: 978-1-62708-170-2
... (g) 0.05 0.20 0.10 0.010 0.008 12.25–13.25 7.50–8.50 2.00–2.50 0.01 0.90–1.35 Al S15500 15-5PH (g) 0.07 1.00 1.00 0.040 0.030 14.00–15.50 3.50–5.50 … … 0.15–0.45 Nb; 2.50–4.50 Cu S15700 15-7PH (g) 0.09 1.00 1.00 0.040 0.030 14.00–16.00 6.50–7.25 2.00–3.00...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003767
EISBN: 978-1-62708-177-1
... S13800 0.05 0.20 0.10 12.25–13.25 7.5–8.5 0.01 0.008 2.0–2.5 Mo; 0.90–1.35 Al; 0.01 N 15-5 PH S15500 0.07 1.00 1.00 14.0–15.5 3.5–5.5 0.04 0.03 2.5–4.5 Cu; 0.15–0.45 Nb 17-4 PH S17400 0.07 1.00 1.00 15.5–17.5 3.0–5.0 0.04 0.03 3.0–5.0 Cu; 0.15–0.45 Nb 17-7 PH S17700...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002461
EISBN: 978-1-62708-194-8
... 0.15 1.00 0.040 0.040 1.00 6.00–8.00 … 0.45–0.65 … 504 S50400 0.15 1.00 0.040 0.040 1.00 8.00–10.00 … 0.90–1.10 … S13800 0.05 0.10 0.01 0.008 0.10 12.25–13.25 7.50–8.50 2.00–2.50 Al 0.90–1.35; N 0.010 … S15500 0.07 1.00 0.040 0.030 1.00 14.00–15.50 3.50–5.50...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001039
EISBN: 978-1-62708-161-0
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002183
EISBN: 978-1-62708-188-7
... …  431 S43100 Precipitation-hardening martensitic stainless steels  Custom 450 …  Custom 455 …  15-5 PH S15500  17-4 PH S17400  PH 13-8 Mo S13800 Precipitation-hardening semiaustenitic stainless steels  AM-350 S35000  AM-355 S35500  17-7 PH S17700  PH 15-7 Mo...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004190
EISBN: 978-1-62708-184-9
... resistance, alloy 2205 clad plate has been suggested for some applications. The metallurgy used for refiner backing disks, drive shafts, and casings varies with the manufacturer and specific process conditions. Alloys that have been used include forged 15-5PH (S15500), CA6-NM (J91540), and CB-6 (J91804...