Published: 01 January 1990
Fig. 66 Time to failure in an aqueous solution (5% NaCl and 0.5% acetic acid deaerated and saturated with hydrogen sulfide) as a function of yield strength for UNS S41000, S15500, S17400, and S13800 stainless steels loaded to 345 MPa (50 ksi) in tension. Tempering temperatures, in degrees More
Series: ASM Handbook
Volume: 18
Publisher: ASM International
Published: 31 December 2017
DOI: 10.31399/asm.hb.v18.a0006372
EISBN: 978-1-62708-192-4
... 55 8 Aged at 566 °C (1050 °F) 38 HRC 17 2.5 Aged at 621 °C (1150 °F) 33 HRC 14 2 S17400 Aged at 480 °C (895 °F) 45 HRC 69 10 Aged at 621 °C (1150 °F) 34 HRC 35 5 S13800 Aged at 538 °C (1000 °F) 46 HRC 21 3 S66286 Aged at 718 °C (1325 °F) 30 HRC 14 2...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005961
EISBN: 978-1-62708-168-9
... hardening wrought stainless steels Table 1 Composition of selected AISI standard precipitation hardening wrought stainless steels Alloy name (type) (b) UNS No. Element, wt% (a) C S P Si Cr Ni Cu Al Mn Nb+Ta Other Martensitic 13-8 PH (XM-13) S13800 0.05 0.008 0.01...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002180
EISBN: 978-1-62708-188-7
... 2.50–5.00 1.00–2.00 … … S32950 … 0.03 2.00 0.60 0.035 0.010 26.0–29.0 3.50–5.20 1.00–2.50 0.15–0.35 … Precipitation-hardenable alloys S13800 (c) [XM-13] 0.05 0.20 0.10 0.01 0.008 12.25–13.25 7.50–8.50 2.00–2.50 0.01 0.90–1.35 Al S15500 (c) [XM-12] 0.07 1.00...
Series: ASM Handbook
Volume: 23
Publisher: ASM International
Published: 01 June 2012
DOI: 10.31399/asm.hb.v23.a0005673
EISBN: 978-1-62708-198-6
... UNS No. Alloy Composition (a) , % C Mn Si Cr Ni Mo P S Other Martensitic types S13800 PH13-8 Mo 0.05 0.10 0.10 12.25–13.25 7.5–8.5 2.0–2.5 0.01 0.008 0.90–1.35 Al; 0.01 N S15500 15-5PH 0.07 1.00 1.00 14.0–15.5 3.5–5.5 … 0.04 0.03 2.5–4.5 Cu; 0.15–0.45 Nb...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001046
EISBN: 978-1-62708-161-0
... 0.75 Mo 440C S44004 0.95–1.20 1.00 1.00 16.0–18.0 … 0.04 0.03 0.75 Mo Precipitation-hardening types PH 13-8 Mo S13800 0.05 0.20 0.10 12.25–13.25 7.5–8.5 0.01 0.008 2.0–2.5 Mo; 0.90–1.35 Al; 0.01 N 15-5 PH S15500 0.07 1.00 1.00 14.0–15.5 3.5–5.5 0.04 0.03 2.5–4.5...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001412
EISBN: 978-1-62708-173-3
... of precipitation-hardening stainless steels per specification noted Alloy and product form (a) Condition Tensile strength Yield strength Elongation, % Reduction in area, % Hardness, HRC ASTM specification MPa ksi MPa ksi min max Martensitic types PH13-8 Mo (UNS S13800)  B, F H950...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003115
EISBN: 978-1-62708-199-3
... of precipitation-hardening stainless steels Table 5 Chemical compositions of precipitation-hardening stainless steels UNS No. Alloy Composition (a) , % C Mn Si Cr Ni Mo P S Other Martensitic types S13800 PH13-8 Mo 0.05 0.10 0.10 12.25–13.25 7.5–8.5 2.0–2.5 0.01 0.008 0.90...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003812
EISBN: 978-1-62708-183-2
... grades S41040 XM-30 0.18 1.00 0.040 0.030 1.00 11.5–13.0 … … 0.05–0.30Nb S41610 XM-6 0.15 1.50–2.50 0.06 0.15 min 1.00 12.0–14.0 … 0.60 … Precipitation-hardenable grades S13800 PH13-8Mo, XM-13 0.05 0.20 0.01 0.008 0.10 12.25–13.25 7.50–8.50 2.00–2.50 0.90...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002403
EISBN: 978-1-62708-193-1
... + Ta) 1000 (145) ht PH13-8Mo S13800 0.05 0.10 0.10 12.25–13.25 7.5–8.5 0.01 0.008 2.0–2.5Mo, 0.90–1.35Al, 0.01N 1310 (190) ht Custom 455 (XM-16) S45500 0.05 0.50 0.50 11.0–12.5 7.5–9.5 0.04 0.03 0.5Mo, 1.5–2.5Cu, 0.8–1.4Ti, 0.1–0.5Nb 1410 (205) ht 17-7PH S17700 0.09...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001434
EISBN: 978-1-62708-173-3
... approximately matching compositions, as classified by the American Welding Society (AWS), are also listed in Table 1(b) , but only for selected base metals. Compositions of nominally martensitic stainless steels Table 1(a) Compositions of nominally martensitic stainless steels Designation UNS...
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003285
EISBN: 978-1-62708-176-4
... 60 (S21800) 205 Type 301 169 345+ 50+ 205 Type 420 472 345+ 50+ 213 S17400 313 345+ 50+ 205 S17400 332 345+ 50+ 205 Nitronic 50 205 345+ 50+ 205 S13800 297 345+ 50+ 205 S13800 437 345+ 50+ 205 AISI 4337 448 345+ 50+ 205 Stellite 6B 415 345...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001048
EISBN: 978-1-62708-161-0
... … … 0.30 … 3.5 Cu 17-4PH S17400 0.04 16.5 4.25 … … 0.25 … 3.6 Cu PH 13-8 Mo S13800 0.05 12.5 8.0 2.25 … … … 1.1 Al Precipitation-hardening semiaustenitic stainless steels AM-350 S35000 0.10 16.5 4.25 2.75 0.10 … … … AM-355 S35500 0.13 15.5 4.25 2.75 0.10...
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001305
EISBN: 978-1-62708-170-2
...–27.0 4.50–6.50 2.00–4.00 0.10–0.25 1.50–2.50 Cu S32900 329 0.20 1.00 0.75 0.040 0.030 23.00–28.00 2.50–5.00 1.00–2.00 … … S32950 7-Mo Plus (e) 0.03 2.00 0.60 0.035 0.010 26.0–29.0 3.50–5.20 1.00–2.50 0.15–0.35 … Precipitation-hardenable alloys S13800 PH13-8 Mo...
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003767
EISBN: 978-1-62708-177-1
... S13800 0.05 0.20 0.10 12.25–13.25 7.5–8.5 0.01 0.008 2.0–2.5 Mo; 0.90–1.35 Al; 0.01 N 15-5 PH S15500 0.07 1.00 1.00 14.0–15.5 3.5–5.5 0.04 0.03 2.5–4.5 Cu; 0.15–0.45 Nb 17-4 PH S17400 0.07 1.00 1.00 15.5–17.5 3.0–5.0 0.04 0.03 3.0–5.0 Cu; 0.15–0.45 Nb 17-7 PH S17700...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002461
EISBN: 978-1-62708-194-8
... 0.15 1.00 0.040 0.040 1.00 6.00–8.00 … 0.45–0.65 … 504 S50400 0.15 1.00 0.040 0.040 1.00 8.00–10.00 … 0.90–1.10 … S13800 0.05 0.10 0.01 0.008 0.10 12.25–13.25 7.50–8.50 2.00–2.50 Al 0.90–1.35; N 0.010 … S15500 0.07 1.00 0.040 0.030 1.00 14.00–15.50 3.50–5.50...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001039
EISBN: 978-1-62708-161-0
Series: ASM Handbook
Volume: 8
Publisher: ASM International
Published: 01 January 2000
DOI: 10.31399/asm.hb.v08.a0003309
EISBN: 978-1-62708-176-4
... is consistently higher than that of weld metal specimens ( Ref 66 ). Another application example of the rising step-load bend technique is the evaluation of potential-step polarization and hydrogen over-potential on crack propagation and crack arrest of T-250 maraging steel and PH-13-8Mo (UNS S13800) steel...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002183
EISBN: 978-1-62708-188-7
... …  431 S43100 Precipitation-hardening martensitic stainless steels  Custom 450 …  Custom 455 …  15-5 PH S15500  17-4 PH S17400  PH 13-8 Mo S13800 Precipitation-hardening semiaustenitic stainless steels  AM-350 S35000  AM-355 S35500  17-7 PH S17700  PH 15-7 Mo...