... material for marine cargo applications, having been installed in 14 cargo ships since 1987 ( Ref 5 ). Figure 3 compares the corrosion resistance of 316, 317, and cast alloy 20 (UNS N08007) in 105% super-phosphoric acid (76% P 2 O 5 ) ( Ref 6 ). Note that all of the alloys show less than 0.25 mm/yr...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004219
EISBN: 978-1-62708-184-9
... and the nature of the particulates and fluid. Erosion-corrosion of a UNS N08007 (ACI CN-7M) stainless steel cast impeller after exposure to hot concentrated H 2 SO 4 with solids present is shown in Fig. 7 . Erosion-corrosion is also evident in Fig. 8 , which shows that the erosion-corrosion damage increased...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003662
EISBN: 978-1-62708-182-5
... N30002 3 2.83 0.111 N26022 1 0.98 0.039 Alloy 59 cast 0 0.00 0.000 Note: Except for cast alloy 59, all other materials were thin-section investment castings and tested in as-cast condition. UNS, Unified Numbering System. (a) UNS N08007 and J93254 were tested with smooth surfaces...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004179
EISBN: 978-1-62708-184-9
... (J92800) are more available and are used for pumps and valves in HNO 3 service. The cast version of alloy 20, ACI CN-7M (N08007), is also commonly used in pumps and valves in HNO 3 service at elevated temperatures up to 70% concentration. Cast low-carbon, high-silicon stainless steels have been...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004182
EISBN: 978-1-62708-184-9
...-rich and nickel-base alloys. Source: Ref 3 Group Alloys A N02200, N06030, N06600, N06985, N08007, N08020, N08825 B N06022, N06059, N06200, N06686, N10276, N10665, N10675, N26455, N26022, N30007, N30107 C Carbon steel (a) D C70600, C71500, N04400, N24135, P00020, P04995...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0006543
EISBN: 978-1-62708-183-2
... 0.280 CN-7M N08007 8.00 0.289 Heat-resistant alloy castings HA … 7.72 0.279 HC J92605 7.53 0.272 HD J93005 7.58 0.274 HE J93403 7.67 0.277 HF J92603 7.75 0.280 HH J93503 7.72 0.279 HI J94003 7.72 0.279 HK J94224 7.75 0.280 HL N08604 7.72...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004178
EISBN: 978-1-62708-184-9
... Alloys The 20-type alloys are usually the first considered when an H 2 SO 4 environment is too corrosive for the use of steel, 300 series stainless steels, or cast iron. This group contains both wrought alloy 20Cb-3 (N08020) and cast alloy ACI CN-7M (N08007) that are roughly equivalent...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005990
EISBN: 978-1-62708-168-9
... … … A743 Austenite 0.03 2.00 1.00 20.0–22.0 23.0–27.0 4.5–5.5 Mo CN-7M N08007 … A351, A743, A744 Austenite 0.07 1.50 1.50 19.0–22.0 27.5–30.5 2.0–3.0Mo; 3.0–4.0 Cu CN-7MS J94650 … A743, A744 Austenite 0.07 1.50 3.50 (f) 18.0–20.0 22.0–25.0 2.5–3.0Mo; 1.5–2.0 Cu CT-15C...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003813
EISBN: 978-1-62708-183-2
... 0.04 0.04 18.0–21.0 9.0–13.0 3.0–4.0Mo CH-20 J93402 309 0.20 1.50 2.00 0.04 0.04 22.0–26.0 12.0–15.0 … CK-20 J94202 310 0.20 2.00 2.00 0.04 0.04 23.0–27.0 19.0–22.0 … CN-7M N08007 … 0.07 1.50 1.50 0.04 0.04 19.0–22.0 27.5–30.5 2.0–3.0Mo, 3.0–4.0Cu CN-7MS...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004190
EISBN: 978-1-62708-184-9
... digester environments ( Ref 13 , 16 ). Duplex stainless steel has also been used for the replacement of one digester top. Corrosion The most serious corrosion problem with carbon steel continuous digesters has been caustic stress-corrosion cracking (SCC) of un-stress-relieved seam welds...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004184
EISBN: 978-1-62708-184-9
... Source: Ref 50 For pumps and valves, a cast version of the “20” type alloy CN 7M (20Cr, 29Ni, 3Mo; N08007) is quite often employed ( Ref 51 , 52 ). Corrosion rates are below 0.13 mm/yr (5 mils/yr) for the complete range of NaOH concentration at temperatures up to the atmospheric boiling point...