Published: 01 January 1990
SAE/AISI 4147H UNS H41470. Heat-treating temperatures recommended by SAE Normalize (for forged or rolled specimens only): 870 °C (1600 °F) Austenitize: 845 °C (1550 °F) More
Book Chapter

Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001030
EISBN: 978-1-62708-161-0
... Normalize (for forged or rolled specimens only): 870 °C (1600 °F) Austenitize: 845 °C (1550 °F) SAE/AISI 4147H UNS H41470. Heat-treating temperatures recommended by SAE Normalize (for forged or rolled specimens only): 870 °C (1600 °F) Austenitize: 845 °C (1550 °F) SAE/AISI 4150H UNS H41500...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003092
EISBN: 978-1-62708-199-3
... ranges, and product analysis tolerances of carbon and alloy steels. The major designation systems discussed include the Society of Automotive Engineers (SAE)-American Iron and Steel Institute (AISI) designations, Unified Numbering System (UNS) designations, American Society for Testing and Materials...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001028
EISBN: 978-1-62708-161-0
.../1.20 0.15/0.25 … H41450 4145H 0.42/0.49 0.65/1.10 0.15/0.35 … 0.75/1.20 0.15/0.25 … H41470 4147H 0.44/0.51 0.65/1.10 0.15/0.35 … 0.75/1.20 0.15/0.25 … H41500 4150H 0.47/0.54 0.65/1.10 0.15/0.35 … 0.75/1.20 0.15/0.25 … H41610 4161H 0.55/0.65 0.65/1.10 0.15/0.35...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005954
EISBN: 978-1-62708-168-9
... … 0.75–1.20 0.15–0.25 … H41470 4147H 0.44–0.51 0.65–1.10 0.15–0.35 … 0.75–1.20 0.15–0.25 … H41500 4150H 0.47–0.54 0.65–1.10 0.15–0.35 … 0.75–1.20 0.15–0.25 … H41610 4161H 0.55–0.65 0.65–1.10 0.15–0.35 … 0.65–0.95 0.25–0.35 … H43200 4320H 0.17–0.23 0.40–0.70 0.15...