Fig. 3 Microstructure of quenched and tempered low-alloy UNS G43400 steel showing a mixture of bainite (dark etching constituent) and martensite (lighter gray). 4% picral + 2% nital etch. Original magnification 500× More
Image
Published: 01 December 2004
Fig. 56 Microstructure of quenched and tempered UNS G43400 steel showing a mixed bainite (dark-appearing constituent) and martensite structure. 4% picral + 2% nital. Original magnification 500× More
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003763
EISBN: 978-1-62708-177-1
..., G52986, G43400, and G86200. The letter “G” designates standard carbon and alloy steels. Following the AISI/SAE practice, the first two digits describe the class of steel, and the next two digits describe the nominal carbon content. The UNS 41 xxx -series of low-alloy steels are chromium-molybdenum steels...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003092
EISBN: 978-1-62708-199-3
... ranges, and product analysis tolerances of carbon and alloy steels. The major designation systems discussed include the Society of Automotive Engineers (SAE)-American Iron and Steel Institute (AISI) designations, Unified Numbering System (UNS) designations, American Society for Testing and Materials...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002179
EISBN: 978-1-62708-188-7
... G41500 (b) 187–241 55 G41610 (d) 187–241 50 G43200 (e) 187–229 60 G43400 (d) 187–241 50 G43400 (d) 187–241 50 G44190 (b) 170–212 65 G44220 (c) 170–212 65 G44270 (b) 170–212 65 G46150 (c) 174–223 65 G46170 (c) 174–223 65 G46200 (c) 183–229 65...
Series: ASM Handbook
Volume: 24A
Publisher: ASM International
Published: 30 June 2023
DOI: 10.31399/asm.hb.v24A.a0006993
EISBN: 978-1-62708-439-0
... for Additive Manufacturing—General Principles—Part Classifications for Additive Manufactured Parts Used in Aviation” ASTM F3554 “Standard Specification for Additive Manufacturing—Finished Part Properties—Grade 4340 (UNS G43400) via Laser Beam Powder-Bed Fusion for Transportation Applications” ASTM F3302...
Series: ASM Handbook
Volume: 13A
Publisher: ASM International
Published: 01 January 2003
DOI: 10.31399/asm.hb.v13a.a0003702
EISBN: 978-1-62708-182-5
... about corrosion, sometimes the direct result of poor communication and/or a lack of appreciation of the true service conditions ( Ref 5 ). As an example, a type 316 stainless steel (Unified Numbering System, or UNS, S31600) pipe was considered a suitable choice for admitting steam and subsequently air...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001009
EISBN: 978-1-62708-161-0
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005954
EISBN: 978-1-62708-168-9
... 0.10–0.40 0.025 0.025 0.15–0.35 2.25–3.50 1.00–1.80 0.20–0.60 … 4340 G43400 0.38–0.43 0.60–0.80 0.035 0.040 0.15–0.35 1.65–2.00 0.70–0.90 0.20–0.30 … E4340 G43406 0.38–0.43 0.65–0.85 0.025 0.025 0.15–0.35 1.65–2.00 0.70–0.90 0.20–0.30 … (300M) K44220 0.40–0.46...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001013
EISBN: 978-1-62708-161-0
... 0.41–0.49 0.70–1.00 0.15–0.30 0.80–1.15 … 0.15–0.25 4340 G43400 0.36–0.44 0.55–0.80 0.15–0.30 0.60–0.90 1.65–2.00 0.20–0.30 E4340 (c) G43406 0.37–0.44 0.60–0.85 0.15–0.30 0.65–0.90 1.65–2.00 0.20–0.30 4615 G46150 0.12–0.18 0.40–0.65 0.15–0.30 … 1.65–2.00 0.20–0.30...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003828
EISBN: 978-1-62708-183-2
... the alloy galvanically corroded when coupled to AISI 4340 steel and 7075-T6 aluminum ( Ref 23 ). The same study showed that magnesium alloy ZK60A-T5 (UNS M16600) protected U-0.75Ti, and 4340 (UNS G43400) steel with a zinc chromate conversion coating protected the alloy for a limited time. U-0.75Ti showed...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001015
EISBN: 978-1-62708-161-0
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002461
EISBN: 978-1-62708-194-8
... 0.48–0.53 0.75–1.00 0.035 0.040 0.15–0.35 … 0.80–1.10 0.15–0.25 4161 G41610 0.56–0.64 0.75–1.00 0.035 0.040 0.15–0.35 … 0.70–0.90 0.25–0.35 4320 G43200 0.17–0.22 0.45–0.65 0.035 0.040 0.15–0.35 1.65–2.00 0.40–0.60 0.20–0.30 4340 G43400 0.38–0.43 0.60–0.80 0.035...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004190
EISBN: 978-1-62708-184-9
... digester environments ( Ref 13 , 16 ). Duplex stainless steel has also been used for the replacement of one digester top. Corrosion The most serious corrosion problem with carbon steel continuous digesters has been caustic stress-corrosion cracking (SCC) of un-stress-relieved seam welds...
Series: ASM Handbook
Volume: 19
Publisher: ASM International
Published: 01 January 1996
DOI: 10.31399/asm.hb.v19.a0002397
EISBN: 978-1-62708-193-1
... strength ranges due to tempering) 4130 G41300 0.30 0.50 0.25 1.0 … 0.20 … … … 900–1700 4140 G41400 0.40 0.83 0.25 0.93 … 0.20 … … … 900–1800 4340 G43400 0.40 0.70 0.25 0.80 1.9 0.25 … … … 900–1800 300M K44315 0.42 0.76 1.60 0.76 1.76 0.41 0.10...
Series: ASM Handbook
Volume: 24A
Publisher: ASM International
Published: 30 June 2023
DOI: 10.31399/asm.hb.v24A.9781627084390
EISBN: 978-1-62708-439-0