Published: 01 January 1989
Fig. 9 Titanium nitrides (E) in UNS G10600 steel microalloyed with titanium and vanadium. Unetched. 270× More
Image
Published: 01 December 2004
Fig. 12 Characteristics of heat treated or finished parts. (a) One end of a cross section through a flame-hardened UNS G10600 steel guide bar showing the hardened case. Dark-gray area at outside edges is a fully hardened martensitic structure; black area is the transition zone between More
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002179
EISBN: 978-1-62708-188-7
... into three groups, depending on their carbon content: Low-carbon steel with less than 0.3% C (UNS grades G10050 to G10290) ( Ref 2 ) Medium-carbon steel with 0.3 to 0.6% C (UNS grades G10300 to G10600) High-carbon steel with more than 0.6% C (UNS grades G10640 to G10950) The low-carbon...
Book Chapter

By Samuel M. Purdy
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003750
EISBN: 978-1-62708-177-1
... parts to show the depth of hardening ( Fig. 12a ), decarburization ( Fig. 12b ), grinding burns ( Fig. 12c ), and soft spots from improper quenching. Fig. 12 Characteristics of heat treated or finished parts. (a) One end of a cross section through a flame-hardened UNS G10600 steel guide bar...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003092
EISBN: 978-1-62708-199-3
... 0.46–0.53 0.60–0.90 0.040 0.050 G10500 1050 0.48–0.55 0.60–0.90 0.040 0.050 G10530 1053 0.48–0.55 0.70–1.00 0.040 0.050 G10550 1055 0.50–0.60 0.60–0.90 0.040 0.050 G10590 1059 0.55–0.65 0.50–0.80 0.040 0.050 G10600 1060 0.55–0.65 0.60–0.90 0.040 0.050...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005949
EISBN: 978-1-62708-168-9
... 0.050 G10600 C60 S58C 60 1064 0.60–0.70 0.50–0.80 0.040 0.050 G10640 D63-2 … … 1065 0.60–0.70 0.60–0.80 0.040 0.050 G10650 C68 … 65 1069 0.65–0.75 0.60–0.90 0.040 0.050 … D70-2 … 70 1070 0.65–0.75 0.60–0.90 0.040 0.050 G10700 C67 … 70 1074 0.70–0.80...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001013
EISBN: 978-1-62708-161-0
... 0.60–0.90 0.040 0.050 G10600 1060 0.55–0.66 0.60–0.90 0.040 0.050 G10640 1064 0.59–0.70 0.50–0.80 0.040 0.050 G10650 1065 0.59–0.70 0.60–0.90 0.040 0.050 G10700 1070 0.65–0.76 0.60–0.90 0.040 0.050 G10740 1074 0.69–0.80 0.50–0.80 0.040 0.050 G10750 1075...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001009
EISBN: 978-1-62708-161-0
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001015
EISBN: 978-1-62708-161-0
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002461
EISBN: 978-1-62708-194-8
...–0.55 0.70–1.00 0.040 max 0.050 max 1055 G10550 0.50–0.60 0.60–0.90 0.040 max 0.050 max 1059 (b) G10590 0.55–0.65 0.50–0.80 0.040 max 0.050 max 1060 G10600 0.55–0.65 0.60–0.90 0.040 max 0.050 max 1064 (b) G10640 0.60–0.70 0.50–0.80 0.040 max 0.050 max 1065 (b...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.9781627081689
EISBN: 978-1-62708-168-9
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001304
EISBN: 978-1-62708-170-2
...–0.90 0.040 0.050 G10550 1055 0.52–0.60 0.60–0.90 0.040 0.050 G10600 1060 0.55–0.66 0.60–0.90 0.040 0.050 G10640 1064 0.59–0.70 0.50–0.80 0.040 0.050 G10650 1065 0.59–0.70 0.60–0.90 0.040 0.050 G10700 1070 0.65–0.76 0.60–0.90 0.040 0.050 G10740 1074 0.69...