1-10 of 10 Search Results for

UNS G10300

Sort by
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002179
EISBN: 978-1-62708-188-7
... into three groups, depending on their carbon content: Low-carbon steel with less than 0.3% C (UNS grades G10050 to G10290) ( Ref 2 ) Medium-carbon steel with 0.3 to 0.6% C (UNS grades G10300 to G10600) High-carbon steel with more than 0.6% C (UNS grades G10640 to G10950) The low-carbon...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003092
EISBN: 978-1-62708-199-3
... 0.040 0.050 G10300 1030 0.28–0.34 0.60–0.90 0.040 0.050 G10350 1035 0.32–0.38 0.60–0.90 0.040 0.050 G10370 1037 0.32–0.38 0.70–1.00 0.040 0.050 G10380 1038 0.35–0.42 0.60–0.90 0.040 0.050 G10390 1039 0.37–0.44 0.70–1.00 0.040 0.050 G10400 1040 0.37–0.44...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005949
EISBN: 978-1-62708-168-9
... C25 S25C 25 1026 0.22–0.28 0.60–0.90 0.040 0.050 G10260 CK25 … 25Mn 1029 0.25–0.31 0.60–0.90 0.040 0.050 G10290 28Mn4 S28C … 1030 0.28–0.34 0.60–0.90 0.040 0.050 G10300 C30 S30C 30 1034 0.32–0.38 0.50–0.80 0.040 0.050 G10340 … … … 1035 0.32–0.38 0.60...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001013
EISBN: 978-1-62708-161-0
... G10220 1022 0.17–0.23 0.70–1.00 0.040 0.050 G10230 1023 0.19–0.25 0.30–0.60 0.040 0.050 G10250 1025 0.22–0.28 0.30–0.60 0.040 0.050 G10260 1026 0.22–0.28 0.60–0.90 0.040 0.050 G10300 1030 0.27–0.34 0.60–0.90 0.040 0.050 G10330 1033 0.29–0.36 0.70–1.00 0.040...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001009
EISBN: 978-1-62708-161-0
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001015
EISBN: 978-1-62708-161-0
Series: ASM Handbook
Volume: 4A
Publisher: ASM International
Published: 01 August 2013
DOI: 10.31399/asm.hb.v04a.a0005817
EISBN: 978-1-62708-165-8
... Si Mn P S Cr Mo Ni V Carbon and low-alloy steels 1030 G10300 C30 0.27–0.34 ≤0.4 0.50–0.80 ≤0.045 ≤0.045 ≤0.40 ≤0.10 ≤0.40 … 1045 G10450 C45 0.42–0.50 0.17–0.37 0.50–0.80 ≤0.040 ≤0.040 ≤0.050 ≤0.10 ≤0.30 … … … 30CrMoV9 0.26–0.34 ≤0.4 0.40–0.70 ≤0.035...
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002461
EISBN: 978-1-62708-194-8
...–0.31 0.60–0.90 0.040 max 0.050 max 1030 G10300 0.28–0.34 0.60–0.90 0.040 max 0.050 max 1034 G10340 0.32–0.38 0.50–0.80 0.040 max 0.050 max 1035 G10350 0.32–0.38 0.60–0.90 0.040 max 0.050 max 1037 G10370 0.32–0.38 0.70–1.00 0.040 max 0.050 max 1038 G10380 0.35...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.9781627081689
EISBN: 978-1-62708-168-9
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001304
EISBN: 978-1-62708-170-2
... 1021 0.17–0.23 0.60–0.90 0.040 0.050 G10220 1022 0.17–0.23 0.70–1.00 0.040 0.050 G10230 1023 0.19–0.25 0.30–0.60 0.040 0.050 G10250 1025 0.22–0.28 0.30–0.60 0.040 0.050 G10260 1026 0.22–0.28 0.60–0.90 0.040 0.050 G10300 1030 0.27–0.34 0.60–0.90 0.040 0.050...