1-11 of 11 Search Results for

UNS G10150

Sort by
Image
Published: 01 December 2004
Fig. 2 Microstructure of plain carbon UNS G10150 steel showing equiaxed ferrite grains with pearlite islands. 4% picral + 2% nital etch. Original magnification 200× More
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003763
EISBN: 978-1-62708-177-1
... of this microstructure is the ferrite formed on the original or prior-austenite grain boundaries during cooling from austenite. Ferrite in this form is called proeutectoid ferrite and is described later in this article. Figure 2 shows the microstructure of an as-rolled UNS G10150 steel plate. The microstructure also...
Book: Machining
Series: ASM Handbook
Volume: 16
Publisher: ASM International
Published: 01 January 1989
DOI: 10.31399/asm.hb.v16.a0002179
EISBN: 978-1-62708-188-7
..., HB Machinability rating, % G10050 … 45 G10060 95 50 G10080 95 55 G10100 105 55 G10110 … 53 G10120 105 55 G10130 … 53 G10150 111 60 G10160 121 70 G10170 116 65 G10180 126 70 G10190 131 70 G10200 121 65 G10210 131 70 G10220...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003092
EISBN: 978-1-62708-199-3
... G10150 1015 0.13–0.18 0.30–0.60 0.040 0.050 G10160 1016 0.13–0.18 0.60–0.90 0.040 0.050 G10170 1017 0.15–0.20 0.30–0.60 0.040 0.050 G10180 1018 0.15–0.20 0.60–0.90 0.040 0.050 G10190 1019 0.15–0.20 0.70–1.00 0.040 0.050 G10200 1020 0.18–0.23 0.30–0.60 0.040...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.a0005949
EISBN: 978-1-62708-168-9
...) Steel designation AISI or SAE UNS No. Chemical composition, % C Mn P, max S, max 1008 G10080 0.10 max 0.30–0.50 0.040 0.050 1012 G10120 0.10–0.15 0.30–0.60 0.040 0.050 1015 G10150 0.13–0.18 0.30–0.60 0.040 0.050 1018 G10180 0.15–0.20 0.60–0.90 0.040 0.050...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001013
EISBN: 978-1-62708-161-0
... (a) 0.45 (a) 0.040 0.050 G10080 1008 0.10 (a) 0.50 (a) 0.040 0.050 G10090 1009 0.15 (a) 0.60 (a) 0.040 0.050 G10100 1010 0.08–0.13 0.30–0.60 0.040 0.050 G10120 1012 0.10–0.15 0.30–0.60 0.040 0.050 G10150 1015 0.12–0.18 0.30–0.60 0.040 0.050 G10160 1016...
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001009
EISBN: 978-1-62708-161-0
Series: ASM Handbook
Volume: 1
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v01.a0001015
EISBN: 978-1-62708-161-0
Series: ASM Handbook
Volume: 20
Publisher: ASM International
Published: 01 January 1997
DOI: 10.31399/asm.hb.v20.a0002461
EISBN: 978-1-62708-194-8
... 0.08 max 0.25–0.40 0.040 max 0.050 max 1008 G10080 0.10 max 0.30–0.50 0.040 max 0.050 max 1010 G10100 0.08–0.13 0.30–0.60 0.040 max 0.050 max 1012 G10120 0.10–0.15 0.30–0.60 0.040 max 0.050 max 1015 G10150 0.13–0.18 0.30–0.60 0.040 max 0.050 max 1016 G10160 0.13...
Series: ASM Handbook
Volume: 4D
Publisher: ASM International
Published: 01 October 2014
DOI: 10.31399/asm.hb.v04d.9781627081689
EISBN: 978-1-62708-168-9
Series: ASM Handbook
Volume: 5
Publisher: ASM International
Published: 01 January 1994
DOI: 10.31399/asm.hb.v05.a0001304
EISBN: 978-1-62708-170-2
..., % (a) C Mn P max S max G10060 1006 0.08 max 0.45 max 0.040 0.050 G10080 1008 0.10 max 0.50 max 0.040 0.050 G10090 1009 0.15 max 0.60 max 0.040 0.050 G10100 1010 0.08–0.13 0.30–0.60 0.040 0.050 G10120 1012 0.10–0.15 0.30–0.60 0.040 0.050 G10150 1015 0.12...