... for standard grades of ductile iron Table 2 Compositions and general uses for standard grades of ductile iron Specification No. Grade or class UNS TC (a) Typical composition, % Description General uses Si Mn P S ASTM A 395; ASME SA395 60-40-18 F32800 3.00 min 2.50 max (b...