..., nuts C60800 Aluminum bronze, 5% B 111, B 359, B 395 Condenser, evaporator and heat-exchanger tubes; distiller tubes C65100 Silicon bronze B B 315 Heat-exchanger tubes; electrical conduits C65500 Silicon bronze A B 315 Chemical equipment, heat-exchanger tubes; piston rings C68700...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006280
EISBN: 978-1-62708-169-6
... Bronze, low fuming 56.0–60.0 0.05 0.25–1.25 bal 0.75–1.10 Sn; 0.01 Al; 0.01–0.50 Mn; 0.04–0.15 Si C68700 Aluminum brass, arsenical 76.0–79.0 0.07 0.06 bal 1.8–2.5 Al; 0.02–0.06 As C68800 … bal 0.05 0.2 21.3–24.1 3.0–3.8 Al; 0.25–0.55 Co C69050 … 70.0–75.0 … … bal 0.50–1.5...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0006543
EISBN: 978-1-62708-183-2
... Forging brass C37700 8.44 0.305 Architectural bronze C38500 8.47 0.306 Inhibited admiralty C44300 8.53 0.308 Naval brass C46400, C46500 8.41 0.304 Aluminum brass C68700 8.33 0.3001 Leaded naval brass C48500 8.44 0.305 Manganese bronze (A) … 8.36 0.302 Phosphor...
Series: ASM Handbook
Volume: 4E
Publisher: ASM International
Published: 01 June 2016
DOI: 10.31399/asm.hb.v04e.a0006276
EISBN: 978-1-62708-169-6
... at 20 °C (70 °F), at.% Brasses Zinc 37 Phosphor bronzes Tin 9 Aluminum bronzes Aluminum 19 Silicon bronzes Silicon 8 Copper-nickels, nickel silvers Nickel 100 In North America, the Unified Numbering System (UNS) is the accepted designation for copper and copper alloys...
Book Chapter

Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003548
EISBN: 978-1-62708-180-1
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006783
EISBN: 978-1-62708-295-2
Series: ASM Handbook Archive
Volume: 11
Publisher: ASM International
Published: 01 January 2002
DOI: 10.31399/asm.hb.v11.a0003556
EISBN: 978-1-62708-180-1
... that this may be due to the ratio of cathodic to anodic areas, where a single phase, for example, ferrite, is preferentially attacked relative to a large area of less susceptible material. Penetration rates of 17 mm/year (0.7 in./year) in United Numbering System (UNS) 30800 welds have been reported. Perforation...
Series: ASM Handbook
Volume: 13B
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v13b.a0003816
EISBN: 978-1-62708-183-2
... on brass that contains a few percent aluminum in addition to copper and zinc. This markedly increases the resistance to impingement attack in turbulent high-velocity saline water. For example, the arsenical aluminum brass C68700 (76Cu-22Zn-2Al) is frequently used for marine condensers and heat exchangers...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003137
EISBN: 978-1-62708-199-3
... An important constituent of the corrosion film on a brass that contains a few percent aluminum in addition to copper and zinc is aluminum oxide (Al 2 O 3 ), which markedly increases resistance to impingement attack in turbulent high-velocity saline water. For example, the arsenical aluminum brass C68700 (76Cu...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003131
EISBN: 978-1-62708-199-3
... and Temper Designation Systems Alloy Designations In North America, the accepted designation for copper alloys is part of the Unified Numbering System (UNS). Under the UNS system, the identifiers of copper alloys take the form of five-digit codes preceded by the letter “C” (for copper). The five...
Series: ASM Handbook
Volume: 11
Publisher: ASM International
Published: 15 January 2021
DOI: 10.31399/asm.hb.v11.a0006788
EISBN: 978-1-62708-295-2
Series: ASM Handbook
Volume: 9
Publisher: ASM International
Published: 01 December 2004
DOI: 10.31399/asm.hb.v09.a0003772
EISBN: 978-1-62708-177-1
..., 1 Sn, 38.7 Zn, 1.5 Fe, 0.3 Mn C68700 Arsenical aluminum brass 77.5 Cu, 20.3 Zn, 2.2 Al, (0.04 As) Wrought copper-nickel alloys and nickel silvers C70600 Copper-nickel, 10% 88.6 Cu, 10 Ni, 1.4 Fe C71300 Copper-nickel, 25% 75 Cu, 25 Ni C71500 Copper-nickel, 30% 68.5 Cu, 31 Ni...
Series: ASM Handbook
Volume: 14A
Publisher: ASM International
Published: 01 January 2005
DOI: 10.31399/asm.hb.v14a.a0004004
EISBN: 978-1-62708-185-6
... C24000 C31400 C61400 C26000 (cartridge brass) C33000 C63000 C42500 C54400 … C44300 C69700 … C50200 C70600 … C51000 C71000 … C52100 C71500 … C52400 C77000 … C65100 … … C65500 … … C68700 … … C75200 … … C76200 … … Note: OFHC, oxygen-free...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001065
EISBN: 978-1-62708-162-7
... C68700 (aluminum bronze, arsenical) 77.5 Cu, 20.5 Zn, 2.0 Al, 0.1 As T 414 60 186 27 55 30 C68800 73.5 Cu, 22.7 Zn, 3.4 Al, 0.40 Cu F 565–889 82–129 379–786 55–114 36–2 … C69000 73.3 Cu, 3.4 Al, 0.6 Ni, 22.7 Zn F 496–896 72–130 345–807 50–117 40–2 … C69400 (silicon red...
Series: ASM Handbook
Volume: 13C
Publisher: ASM International
Published: 01 January 2006
DOI: 10.31399/asm.hb.v13c.a0004105
EISBN: 978-1-62708-184-9
.../yr 90Cu-10Ni C70600 0.075 3 0.86 34 70Cu-30Ni C71500 0.13 5 0.66 26 2% Al brass C68700 0.075 3 0.56 22 6% Al brass C60800 0.13 5 0.53 21 Arsenical admiralty brass C44300 0.33 13 0.89 35 Phosphorus deoxidized copper C12200 0.36 14 2.7 105 CDA...
Series: ASM Handbook
Volume: 2
Publisher: ASM International
Published: 01 January 1990
DOI: 10.31399/asm.hb.v02.a0001066
EISBN: 978-1-62708-162-7
... Copper tube alloys and typical applications UNS number Alloy type ASTM specifications Typical uses C10200 Oxygen-free copper B 68, B 75, B 88, B 111, B 188, B 280, B 359, B 372, B 395, B 447 Bus tube, conductors, wave guides C12200 Phosphorus deoxidized copper B 68, B 75, B 88, B 111...
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001438
EISBN: 978-1-62708-173-3
... C46400 Naval brass 60 Cu, 39.25 Zn, 0.75 Sn (d) 899 1650 30 F F NR Special brasses C67500 Manganese bronze A 58.5 Cu, 39 Zn, 1.4 Fe, 1 Sn, 0.1 Mn 888 1630 27 F F NR C68700 Aluminum brass, arsenical 77.5 Cu, 20.5 Zn, 2 Al (0.06 As) 971 1780 26 F F NR Nickel silvers...
Book Chapter

Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003206
EISBN: 978-1-62708-199-3
... electrodes (AWS A5.17-89) Electrode Composition (a) (b) , wt% AWS classification UNS No. C Mn Si S P Cu (c) Ti Low-manganese electrodes EL8 K01008 0.10 0.25–0.60 0.07 0.030 0.030 0.35 … EL8K K01009 0.10 0.25–0.60 0.10–0.25 0.030 0.030 0.35 … EL12 K01012...
Series: ASM Desk Editions
Publisher: ASM International
Published: 01 December 1998
DOI: 10.31399/asm.hb.mhde2.a0003204
EISBN: 978-1-62708-199-3
Series: ASM Handbook
Volume: 6
Publisher: ASM International
Published: 01 January 1993
DOI: 10.31399/asm.hb.v06.a0001443
EISBN: 978-1-62708-173-3